Austenitizing temperatures for water-hardening tool steels normally vary from 760 to 845 °C (1400 to 1550 °F), as indicated in Table 2. Higher temperatures are sometimes used for special purposes (Fig. 2). Hardenability increases as austenitizing temperature increases. The optimum time at austenitizing temperature is from 10 to 30 min. Preheating is unusual except for […]
Wallwork doubles aerospace HIP capacity with second Quintus hot isostatic press
Wallwork Group, Manchester, England, installed a second Quintus Technologies hot isostatic press (HIP) at its UK operations, doubling the company’s HIP capacity for aerospace customers and strengthening process continuity across the UK and European supply chain. The investment will be a centerpiece of the company’s presence at Farnborough International Airshow 2026 (Hall 1, Stand 1000, […]
Bodycote opens new heat treatment facility in Monterrey, Mexico
Bodycote, Macclesfield, England, plans to open a new heat treatment facility in Apodaca, in the Monterrey metropolitan area of Mexico. The new site will expand Bodycote’s North American footprint and provide additional regional capacity to support customers across Mexico and the southern United States, helping reduce logistics complexity and strengthen supply-chain resilience for OEMs and […]
Constellium signs multi-year aluminum extrusions agreement with Airbus
Constellium, Issoire, France, announced a multi-year agreement with Airbus for the supply of aluminum alloy extrusions, reinforcing the company’s role as a long-term supplier of advanced aluminum solutions to the European airframer’s commercial and defense programs. Under the agreement, Constellium will provide Airbus with bars and a range of small and large extrusions manufactured in […]
SECO/WARWICK USA delivers second vacuum tempering furnace to aerospace manufacturer
SECO/WARWICK USA, Meadville, Pa., announced that a leading international aircraft motion-control manufacturer has placed a repeat order for an identical low-temperature vacuum tempering furnace, following the success of the first unit installed at the customer’s facility. The new furnace is designed for tempering, ageing, and other sub-critical heat-treat processes, with a maximum operating temperature of […]





