<oembed><version>1.0</version><provider_name>Heat Treating Society</provider_name><provider_url>https://www.asminternational.org/hts</provider_url><author_name>Heat Treating Society</author_name><author_url>https://www.asminternational.org/hts</author_url><title>One Minute Mentor: Quench hardenability - Heat Treating Society</title><type>rich</type><width>600</width><height>338</height><html>&lt;blockquote class="wp-embedded-content" data-secret="ceRDHKYKFc"&gt;&lt;a href="https://www.asminternational.org/hts/one-minute-mentor-quench-hardenability/"&gt;One Minute Mentor: Quench hardenability&lt;/a&gt;&lt;/blockquote&gt;&lt;iframe sandbox="allow-scripts" security="restricted" src="https://www.asminternational.org/hts/one-minute-mentor-quench-hardenability/embed/#?secret=ceRDHKYKFc" width="600" height="338" title="&#x201C;One Minute Mentor: Quench hardenability&#x201D; &#x2014; Heat Treating Society" data-secret="ceRDHKYKFc" frameborder="0" marginwidth="0" marginheight="0" scrolling="no" class="wp-embedded-content"&gt;&lt;/iframe&gt;&lt;script type="text/javascript"&gt;
/* &lt;![CDATA[ */
/*! This file is auto-generated */
!function(d,l){"use strict";l.querySelector&amp;&amp;d.addEventListener&amp;&amp;"undefined"!=typeof URL&amp;&amp;(d.wp=d.wp||{},d.wp.receiveEmbedMessage||(d.wp.receiveEmbedMessage=function(e){var t=e.data;if((t||t.secret||t.message||t.value)&amp;&amp;!/[^a-zA-Z0-9]/.test(t.secret)){for(var s,r,n,a=l.querySelectorAll('iframe[data-secret="'+t.secret+'"]'),o=l.querySelectorAll('blockquote[data-secret="'+t.secret+'"]'),c=new RegExp("^https?:$","i"),i=0;i&lt;o.length;i++)o[i].style.display="none";for(i=0;i&lt;a.length;i++)s=a[i],e.source===s.contentWindow&amp;&amp;(s.removeAttribute("style"),"height"===t.message?(1e3&lt;(r=parseInt(t.value,10))?r=1e3:~~r&lt;200&amp;&amp;(r=200),s.height=r):"link"===t.message&amp;&amp;(r=new URL(s.getAttribute("src")),n=new URL(t.value),c.test(n.protocol))&amp;&amp;n.host===r.host&amp;&amp;l.activeElement===s&amp;&amp;(d.top.location.href=t.value))}},d.addEventListener("message",d.wp.receiveEmbedMessage,!1),l.addEventListener("DOMContentLoaded",function(){for(var e,t,s=l.querySelectorAll("iframe.wp-embedded-content"),r=0;r&lt;s.length;r++)(t=(e=s[r]).getAttribute("data-secret"))||(t=Math.random().toString(36).substring(2,12),e.src+="#?secret="+t,e.setAttribute("data-secret",t)),e.contentWindow.postMessage({message:"ready",secret:t},"*")},!1)))}(window,document);
/* ]]&gt; */
&lt;/script&gt;
</html><description>The quench hardenability of forged steels is increased by grain coarsening and higher dislocation density, and research has shown that control of factors such as forge finish temperature and quench temperature allow the optimization of hardness and microstructure.</description></oembed>