Impact Innovations installs 100+ cold spray systems across 30+ countries

Impact Innovations, German cold spray AM specialist, has reached a key milestone by installing over 100 Cold Spray systems across more than 30 countries. In Q2 2025 alone, the company delivered eight new EvoCSII units, marking a record-breaking quarter and expanding its global footprint.

These systems were deployed in countries including Germany, the United States, China, India, Australia, and South Korea.

The new systems cover a wide range of applications in:

  • Aviation & Aerospace
  • Additive Manufacturing
  • Electrical Industry
  • Induction Cookware
  • Industrial Research
  • Repair – including a mobile system for on-site maintenance of ship components

Why do leading companies choose Impact Innovations?

  • Up to 99.8% deposition efficiency – enabling sustainable, cost-effective manufacturing
  • Full control with 150+ process parameters – for maximum reproducibility
  • From lab to production line – scalable systems for R&D and 24/7 industrial output.

Every system sold brings Cold Spray into new sectors, from engines and busbars to cookware and ships, demonstrating the versatility of solid-state coating and additive manufacturing.

 