Solar Atmospheres of Western Pennsylvania, Hermitage, participated in a Boeing Supplier Assessment. The on-site, preventative engagement resulted in zero findings and Solar, once again, achieved preferred status for heat treating, hardness, and non-destructive liquid penetrant testing.
Notably, Solar Atmospheres added a state-of-the-art metallurgy lab since Boeing’s last visit and will be seeking D1-4426 approval for process codes 802 and 803 by end of 2020.
Quality manager, Melissa Gruszka states, “Adding a full-time metallurgist, technicians, and in-house lab capabilities give us many significant advantages. We can provide more expertise, better quality, and shorter lead times; enabling us to better serve Boeing and all others.”
Approved Scope Highlights:
- BAC 5613, 5616, 5617, 5619, AMS 2774, HP1-25, DPS6.33, MIL-H-81200, AMS-H-81200 [Heat Treatment of Alloy Steels, Corrosion Resistant Steel, Nickel-Cobalt Base Alloy, Wrought Nickel Alloy & Cobalt Alloy Parts, Titanium & Titanium Alloys]
- BAC 5423, BSS 7039, ASTM-E-1417, HP6-13 [Penetrant, Liquid Penetrant, Fluorescent]
- AWS C3.6 [Furnace Brazing]