Spray Tips: Fluidized Bed Powder Feeders

October 10, 2017
Source:

In fluidized-bed powder feeders, a bed of powder is continuously agitated by a fluidizing gas, in this case the carrier gas. The intent by design is to suspend a controlled volume of powder in a bed using a controlled volume of gas such that a sample of powder can be drawn off at a uniform rate. To accomplish this, the bed must be in continuous motion—that is, fluidized—and the volumes of gas and powder being removed must be continuously replaced.

Vibrators and/or gravity feed are used to assist and maintain flow from the hopper into the bed. The diagram shows  how the powder-laden carrier gas is aspirated through openings in the carrier-gas tube, using the venturi effect created by gas flowing through the tube.

Volume 5A, Thermal Spray Technology â‡’ Thermal Spray Processes and Coatings â‡’ Process Control and Control Equipment â‡’ Material Feed

In fluidized-bed powder feeders, a bed of powder is continuously agitated by a fluidizing gas, in this case the carrier gas. The intent by design is to suspend a controlled volume of powder in a bed using a controlled volume of gas such that a sample of powder can be drawn off at a uniform rate. To accomplish this, the bed must be in continuous motion—that is, fluidized—and the volumes of gas and powder being removed must be continuously replaced.

Vibrators and/or gravity feed are used to assist and maintain flow from the hopper into the bed. The diagram shows  how the powder-laden carrier gas is aspirated through openings in the carrier-gas tube, using the venturi effect created by gas flowing through the tube.