3-D printed aluminum electronics enclosure flies on Lockheed Martin military satellite

April 7, 2017
Source:

Lockheed Martin, Sunnyvale, Calif., announces that an electronics enclosure fabricated via additive manufacturing will be the first 3D printed part certified for service on a Lockheed Martin military satellite. By going from multiple machined parts to one 3-D printed part, the team was able to save time in the design and production of the Remote Interface Unit, as well as increase the quality and consistency of the units.

The lead time for manufacturing the part went from six months to only 1.5 months, with assembly time also reduced, from 12 hours to just three hours.

"3-D printing provides the ability to rapidly implement innovation by controlling production from design through implementation with one digital model," says Iris Bombelyn, vice president of Protected Communications at Lockheed Martin Space Systems. "By providing affordable, innovative solutions with a reduced timeline, we are able to adjust to the rapidly changing environment of military space."

AEHF is a global military satellite communications system that provides protected, assured communication for strategic commanders and tactical warfighters. Lockheed Martin will deliver the fourth AEHF vehicle in 2017. AEHF-5 and AEHF-6 are in production and are on track to launch in 2018 and 2019, respectively.

The qualified part onboard AEHF-6 was built by Laser Powder Bed Fusion additive manufacturing, in which a laser melts and fuses aluminum metal powder layer-by-layer to build a part based on a digital design. The electronic enclosure will serve as a model for other programs that are designed based on the A2100 satellite bus.

Across Lockheed Martin, 3-D printing is applied for design prototyping, tooling, and the production of affordable components. The company produced the first 3-D printed parts to fly on an interplanetary spacecraft, Juno, which is currently orbiting Jupiter, and a 3-D printed part flew on Orion's first flight. Additionally, technicians are qualifying large 3-D printed fuel tanks for the modernized A2100 satellite bus.

 www.lockheedmartin.com/aehf

 

Lockheed Martin, Sunnyvale, Calif., announces that an electronics enclosure fabricated via additive manufacturing will be the first 3D printed part certified for service on a Lockheed Martin military satellite. By going from multiple machined parts to one 3-D printed part, the team was able to save time in the design and production of the Remote Interface Unit, as well as increase the quality and consistency of the units.

The lead time for manufacturing the part went from six months to only 1.5 months, with assembly time also reduced, from 12 hours to just three hours.

“3-D printing provides the ability to rapidly implement innovation by controlling production from design through implementation with one digital model,” says Iris Bombelyn, vice president of Protected Communications at Lockheed Martin Space Systems. “By providing affordable, innovative solutions with a reduced timeline, we are able to adjust to the rapidly changing environment of military space.”

AEHF is a global military satellite communications system that provides protected, assured communication for strategic commanders and tactical warfighters. Lockheed Martin will deliver the fourth AEHF vehicle in 2017. AEHF-5 and AEHF-6 are in production and are on track to launch in 2018 and 2019, respectively.

The qualified part onboard AEHF-6 was built by Laser Powder Bed Fusion additive manufacturing, in which a laser melts and fuses aluminum metal powder layer-by-layer to build a part based on a digital design. The electronic enclosure will serve as a model for other programs that are designed based on the A2100 satellite bus.

Across Lockheed Martin, 3-D printing is applied for design prototyping, tooling, and the production of affordable components. The company produced the first 3-D printed parts to fly on an interplanetary spacecraft, Juno, which is currently orbiting Jupiter, and a 3-D printed part flew on Orion’s first flight. Additionally, technicians are qualifying large 3-D printed fuel tanks for the modernized A2100 satellite bus.

 www.lockheedmartin.com/aehf

 