Additive-manufactured components printed via melting metal alloy filaments

February 4, 2016
Source:

3D MakerJet Inc., Orlando, Fla., announces that, after a year and a half in research and development, functioning prototypes of metal components made via melting metal alloy filaments, including copper, have successfully met industry standards. Concentrating on both laser and extruder 3D printers, the company is committed to development of powderless wire-feed additive manufacturing.

"On site, on the job, these printers have the potential to eliminate the high prices and long lead times of back-ordered, hard-to-source, and even obsolete parts. The market for metal printing is continuing to grow and 3D MakerJet is poised to introduce a true breakthrough," said John Crippen, 3D MakerJet President.

The company intends to file a patent in the United States.

Simultaneously, 3D MakerJet is also working on a line of medical grade bioprinters, as well their continued dedication to perfect industrial materials including polypropylene, resins, and waxes.

According to Research and Markets, the market size of metal 3D printing is expected to grow to $2.24 billion by the year 2020 at double digit CAGR.

3D MakerJet Inc., Orlando, Fla., announces that, after a year and a half in research and development, functioning prototypes of metal components made via melting metal alloy filaments, including copper, have successfully met industry standards. Concentrating on both laser and extruder 3D printers, the company is committed to development of powderless wire-feed additive manufacturing.

“On site, on the job, these printers have the potential to eliminate the high prices and long lead times of back-ordered, hard-to-source, and even obsolete parts. The market for metal printing is continuing to grow and 3D MakerJet is poised to introduce a true breakthrough,” said John Crippen, 3D MakerJet President.

The company intends to file a patent in the United States.

Simultaneously, 3D MakerJet is also working on a line of medical grade bioprinters, as well their continued dedication to perfect industrial materials including polypropylene, resins, and waxes.

According to Research and Markets, the market size of metal 3D printing is expected to grow to $2.24 billion by the year 2020 at double digit CAGR.