Hybrid Manufacturing Technologies system combines CNC machining with additive manufacturing

April 2, 2015
Source:

Hybrid Manufacturing Technologies Ltd., Leicestershire, U.K., has developed a system that can be integrated into any CNC machine to allow for metal deposition (via laser cladding), as well as finishing and inspection of parts, all on a single machine. The hybrid methodology integrates directed energy deposition into a multi-axis CNC machine, using a tool changer between processes.

"Adding tool-changeable deposition heads to an existing CNC machine enables 3D printing of metal, without the need to buy a separate machine," stated Dr. Jason Jones, co-founder and CEO of Hybrid Manufacturing Technologies. "This significantly reduces costs and provides an intuitive adoption path for CNC operators. The combination of additive manufacturing with machining offers new capabilities, including in-process finishing, that cannot be delivered by either technology independently."

Hybrid Manufacturing was announced as the winner of the inaugural International Additive Manufacturing Award (IAMA) during a reception at the MFG Meeting in Orlando, March 4-7, 2015. Along with the award, Hybrid Manufacturing will receive a $20,000 cash prize and a media package valued at $80,000.

www.hybridmanutech.com   

 

Hybrid Manufacturing Technologies Ltd., Leicestershire, U.K., has developed a system that can be integrated into any CNC machine to allow for metal deposition (via laser cladding), as well as finishing and inspection of parts, all on a single machine. The hybrid methodology integrates directed energy deposition into a multi-axis CNC machine, using a tool changer between processes.

“Adding tool-changeable deposition heads to an existing CNC machine enables 3D printing of metal, without the need to buy a separate machine,” stated Dr. Jason Jones, co-founder and CEO of Hybrid Manufacturing Technologies. “This significantly reduces costs and provides an intuitive adoption path for CNC operators. The combination of additive manufacturing with machining offers new capabilities, including in-process finishing, that cannot be delivered by either technology independently.”

Hybrid Manufacturing was announced as the winner of the inaugural International Additive Manufacturing Award (IAMA) during a reception at the MFG Meeting in Orlando, March 4-7, 2015. Along with the award, Hybrid Manufacturing will receive a $20,000 cash prize and a media package valued at $80,000.