PTFE/NanoDiamond coating doubles surface durability and reduces friction by up to 66%

March 9, 2014
Source:

Carbodeon, Helsinki, Finland, has released a new PTFE/NanoDiamond coating with twice the durability and up to 66% less friction than current products. The new coating has huge potential to cost-effectively reduce CO2 output and fuel demand, as well as to improve equipment lifespan, in fields such as the automotive, aerospace and industrial machinery industries.

NanoDiamond particles are hard, small, and offer very low surface friction. Carbodeon has developed a liquid dispersion of 4-6nm NanoDiamond particles with surface chemistry that has been specially created to integrate the particles with PTFE molecules without the use of additional surfactants. The new dispersion, called uDiamond Vox D, is the latest addition to Carbodeon's range of NanoDiamond materials.

The improvements in durability and friction result partly from the properties of the diamond material, but equally important are the changes to the overall coating structure caused by the presence of the particles. The use of hard particles to improve the durability of coatings is well known, but the combination of small size and surface functionalization in the uDiamond Vox D coating means that Carbodeon's particles are interfaced with PTFE molecules in a fundamentally different way.

Formulation of the coatings is straightforward – the uDiamond Vox D is supplied as an aqueous or solvent-based dispersion ready for direct mixing into a PTFE coating, followed by application by spray or screen printing with little or no change to the process parameters.

www.carbodeon.com

 

Carbodeon, Helsinki, Finland, has released a new PTFE/NanoDiamond coating with twice the durability and up to 66% less friction than current products. The new coating has huge potential to cost-effectively reduce CO2 output and fuel demand, as well as to improve equipment lifespan, in fields such as the automotive, aerospace and industrial machinery industries.

NanoDiamond particles are hard, small, and offer very low surface friction. Carbodeon has developed a liquid dispersion of 4-6nm NanoDiamond particles with surface chemistry that has been specially created to integrate the particles with PTFE molecules without the use of additional surfactants. The new dispersion, called uDiamond Vox D, is the latest addition to Carbodeon’s range of NanoDiamond materials.

The improvements in durability and friction result partly from the properties of the diamond material, but equally important are the changes to the overall coating structure caused by the presence of the particles. The use of hard particles to improve the durability of coatings is well known, but the combination of small size and surface functionalization in the uDiamond Vox D coating means that Carbodeon’s particles are interfaced with PTFE molecules in a fundamentally different way.

Formulation of the coatings is straightforward – the uDiamond Vox D is supplied as an aqueous or solvent-based dispersion ready for direct mixing into a PTFE coating, followed by application by spray or screen printing with little or no change to the process parameters.

www.carbodeon.com

 