Seco Warwick enables constant control of temperature in multi-chamber heat-treat furnaces

March 14, 2017
Source:

Seco Warwick, Meadville, Pa., announces that its engineering team has designed an innovative way to continuously control the heating and cooling of the entire cycle in multi-chamber heat treating furnaces. The company says that this is a unique technological solution on a global scale that could revolutionize the heat treatment process and exceed the aerospace sector's standards.

"All of our customers set the bar high," says Katarzyna Sawka, Global Marketing Director. "Nevertheless, the aerospace industry sets the bar the highest."

The patented solution, designed to meet the highest AMS standard, is based on thermocouples that move between chambers during the heat treatment cycle. Temperature control is achieved based on a special construction that allows the operator to monitor the temperature in both chambers. This provides full temperature control of the processed parts in multi-chamber vacuum furnaces during the entire process.

The technology has already been successfully implemented in a two-chamber vacuum furnace, the CaseMaster Evolution, which enables precise  vacuum case-hardening for the most challenging industries. It has been successful in applications for aerospace, automotive, machinery, wind energy, and commercial heat treating facilities.

In 2016, Seco Warwick received a number of prestigious awards and nominations. The company won the Symbol of Innovation 2016, for implementing research and development projects with technical universities, and for developing an innovative graphene production line. Seco Warwick was also one of the first companies in the world to introduce augmented reality technology into heavy industry (SECO/LENS).

www.secowarwick.com

 

Seco Warwick, Meadville, Pa., announces that its engineering team has designed an innovative way to continuously control the heating and cooling of the entire cycle in multi-chamber heat treating furnaces. The company says that this is a unique technological solution on a global scale that could revolutionize the heat treatment process and exceed the aerospace sector’s standards.

“All of our customers set the bar high,” says Katarzyna Sawka, Global Marketing Director. “Nevertheless, the aerospace industry sets the bar the highest.”

The patented solution, designed to meet the highest AMS standard, is based on thermocouples that move between chambers during the heat treatment cycle. Temperature control is achieved based on a special construction that allows the operator to monitor the temperature in both chambers. This provides full temperature control of the processed parts in multi-chamber vacuum furnaces during the entire process.

The technology has already been successfully implemented in a two-chamber vacuum furnace, the CaseMaster Evolution, which enables precise  vacuum case-hardening for the most challenging industries. It has been successful in applications for aerospace, automotive, machinery, wind energy, and commercial heat treating facilities.

In 2016, Seco Warwick received a number of prestigious awards and nominations. The company won the Symbol of Innovation 2016, for implementing research and development projects with technical universities, and for developing an innovative graphene production line. Seco Warwick was also one of the first companies in the world to introduce augmented reality technology into heavy industry (SECO/LENS).

www.secowarwick.com

 