New graphite board insulation enables more thermally efficient furnace hot zone

August 1, 2016
Source:

Solar Manufacturing, Souderton, Pa., announces that it has been cooperating for the past year with Graphite Machining Inc., Topton, Pa., on the development and testing of a new graphite board material and its application in vacuum furnace hot zones. This new graphite board material has undergone extensive thermal and vacuum testing to prove its improved thermal efficiency and excellent vacuum performance compared to prior and present graphite board designs.

GMI intends to market this new graphite board under the name of Heatguard insulation, while Solar will incorporate this new material into its vacuum furnace hot zones under the trade name of Hefvac (High Efficiency Vacuum).

According to Frank C. Schoch, president of GMI, "After extensive testing against our existing and competitive insulating materials, Solar Manufacturing and Graphite Machining combined our respective experience and created this new thermally efficient graphite board insulation material."

By incorporating Hefvac board insulation, Solar Manufacturing has now developed a proven, more thermally efficient vacuum furnace hot zone design that is capable of achieving faster and better vacuum levels because of the Hefvac sealed and low-moisture-absorption structure.

William R. Jones, CEO of the Solar Atmospheres family of companies notes, "I will be giving a presentation at the 2016 FNA (Furnaces North America) show in Nashville, Tenn., to highlight the testing and comparisons of prior designs to this new board material and to illustrate not only the more thermally efficient aspect of the new material, but also the ease and advantages of its use. Hefvac will be on display at Solar Manufacturing's booth 301-303 with a full size hot zone."

www.solarmfg.com

 

Solar Manufacturing, Souderton, Pa., announces that it has been cooperating for the past year with Graphite Machining Inc., Topton, Pa., on the development and testing of a new graphite board material and its application in vacuum furnace hot zones. This new graphite board material has undergone extensive thermal and vacuum testing to prove its improved thermal efficiency and excellent vacuum performance compared to prior and present graphite board designs.

GMI intends to market this new graphite board under the name of Heatguard insulation, while Solar will incorporate this new material into its vacuum furnace hot zones under the trade name of Hefvac (High Efficiency Vacuum).

According to Frank C. Schoch, president of GMI, “After extensive testing against our existing and competitive insulating materials, Solar Manufacturing and Graphite Machining combined our respective experience and created this new thermally efficient graphite board insulation material.”

By incorporating Hefvac board insulation, Solar Manufacturing has now developed a proven, more thermally efficient vacuum furnace hot zone design that is capable of achieving faster and better vacuum levels because of the Hefvac sealed and low-moisture-absorption structure.

William R. Jones, CEO of the Solar Atmospheres family of companies notes, “I will be giving a presentation at the 2016 FNA (Furnaces North America) show in Nashville, Tenn., to highlight the testing and comparisons of prior designs to this new board material and to illustrate not only the more thermally efficient aspect of the new material, but also the ease and advantages of its use. Hefvac will be on display at Solar Manufacturing’s booth 301-303 with a full size hot zone.”

www.solarmfg.com

 