Seco-Warwick case-hardening system reduces distortion in gears

October 28, 2015
Source:

Seco Warwick, Meadville, Pa., introduces UniCase Master, a single flow, precision case-hardening system said to reduce distortion in gears; and the ZeroFlow gas nitriding process.  ZeroFlow is an ammonia-only nitriding process characterized by extremely low gas consumption and low emission of post-process gases. It features a simpler control system and reportedly delivers even better precision than processes with double-component atmospheres.

UniCase Master is said to offer not only a step forward in minimizing production cost and maximizing reliability, but also a real breakthrough in quality and repeatability in case hardening of gears by high-pressure gas quenching. It was created in collaboration with Professor Leszek Małdziński from the Institute of Work Machines and Vehicles of the Technical University in Poznan as a new method of controlled gas nitriding and nitrocarburizing.

The ZeroFlow method is based on performing the nitriding process in a single-component atmosphere: raw ammonia (NH3). The adjustment of nitriding atmosphere chemical composition and therefore control of nitriding potential Kn is performed only by a temporary stop and reactivation of NH3 feeding into the furnace.

www.secowarwick.com

 

Seco Warwick, Meadville, Pa., introduces UniCase Master, a single flow, precision case-hardening system said to reduce distortion in gears; and the ZeroFlow gas nitriding process.  ZeroFlow is an ammonia-only nitriding process characterized by extremely low gas consumption and low emission of post-process gases. It features a simpler control system and reportedly delivers even better precision than processes with double-component atmospheres.

UniCase Master is said to offer not only a step forward in minimizing production cost and maximizing reliability, but also a real breakthrough in quality and repeatability in case hardening of gears by high-pressure gas quenching. It was created in collaboration with Professor Leszek Ma?dzi?ski from the Institute of Work Machines and Vehicles of the Technical University in Poznan as a new method of controlled gas nitriding and nitrocarburizing.

The ZeroFlow method is based on performing the nitriding process in a single-component atmosphere: raw ammonia (NH3). The adjustment of nitriding atmosphere chemical composition and therefore control of nitriding potential Kn is performed only by a temporary stop and reactivation of NH3 feeding into the furnace.

www.secowarwick.com

 