Seco Warwick supplies vacuum furnace to Wisconsin heat treating company

December 2, 2014
Source:

Seco Warwick, Meadville, Pa., announces that it has sold a standard Vector 2 bar vacuum furnace to Service Heat Treating, Milwaukee, a provider of case hardening and vacuum processing of medium to large production runs. Vector high-pressure quench furnaces are available in 2, 10, 15, or 25 bar, and are designed for hot, cold, and high-speed steels. 

In addition to patented vacuum carburizing technology, these furnaces can be used for tempering, annealing, solution heat treating, brazing, and sintering. With the FineCarb and PreNit (high speed) carburizing options, a SimVac process simulation package is included at no extra charge.

Service Heat Treating offers standard stainless steel and tool steel processing quickly and cost effectively, and has the capability to design vacuum carburizing processes for the most distortion-critical applications.

www.secowarwick.com/en/products/vacuum-heat-treatment/

 

Seco Warwick, Meadville, Pa., announces that it has sold a standard Vector 2 bar vacuum furnace to Service Heat Treating, Milwaukee, a provider of case hardening and vacuum processing of medium to large production runs. Vector high-pressure quench furnaces are available in 2, 10, 15, or 25 bar, and are designed for hot, cold, and high-speed steels. 

In addition to patented vacuum carburizing technology, these furnaces can be used for tempering, annealing, solution heat treating, brazing, and sintering. With the FineCarb and PreNit (high speed) carburizing options, a SimVac process simulation package is included at no extra charge.

Service Heat Treating offers standard stainless steel and tool steel processing quickly and cost effectively, and has the capability to design vacuum carburizing processes for the most distortion-critical applications.

www.secowarwick.com/en/products/vacuum-heat-treatment/

 