Instron motorized pendulum impact testers measure 300 to 900 joules to Charpy and Izod standards

March 5, 2014
Source:

Instron, Norwood, Mass.,  offers the MPX Series of motorized pendulum impact testers for metals impact testing to Charpy and Izod standards. The MPX Series offers a range of testing capabilities from 300 to 900 Joules. The testers come standard with Fracta Software, which allows for reliable data acquisition and reporting of absorbed energy. If more advanced impact analysis and reporting are needed, upgrading to Impulse Data Acquisition Software and instrumentation will allow for direct measurement of impact force and striker velocity.

The MPX is designed with an automatic test start as soon as the door closes, allowing for rapid testing and improved throughput while conforming to the international standards for non-ambient testing. The feature fully complies with NIST 5-second guidelines, specifiying the time it should take for the specimen to leave the temperature conditioner and for the test to be complete.

Most other pendulum impact testers on the market still require the hammer assembly to be completely removed in order to change weights. On the MPX, interchangeable hammer weights allow for  quick and simple adjustment of the impact energy, removing the need for the time-consuming process of changing hammer shafts.

 The MPX features an integrated guard and safety control system that meets the stringent requirements for the European CE mark and for ISO 13849. The operator is protected at all times during machine operation.

www.instron.com          

 

Instron, Norwood, Mass.,  offers the MPX Series of motorized pendulum impact testers for metals impact testing to Charpy and Izod standards. The MPX Series offers a range of testing capabilities from 300 to 900 Joules. The testers come standard with Fracta Software, which allows for reliable data acquisition and reporting of absorbed energy. If more advanced impact analysis and reporting are needed, upgrading to Impulse Data Acquisition Software and instrumentation will allow for direct measurement of impact force and striker velocity.

The MPX is designed with an automatic test start as soon as the door closes, allowing for rapid testing and improved throughput while conforming to the international standards for non-ambient testing. The feature fully complies with NIST 5-second guidelines, specifiying the time it should take for the specimen to leave the temperature conditioner and for the test to be complete.

Most other pendulum impact testers on the market still require the hammer assembly to be completely removed in order to change weights. On the MPX, interchangeable hammer weights allow for  quick and simple adjustment of the impact energy, removing the need for the time-consuming process of changing hammer shafts.

 The MPX features an integrated guard and safety control system that meets the stringent requirements for the European CE mark and for ISO 13849. The operator is protected at all times during machine operation.

www.instron.com          

 