IBC Advanced Alloys to collaborate with Nu-Cast on Be-Al investment casting projects for aerospace

February 12, 2014
Source:

IBC Advanced Alloys Corp., Vancouver, has signed a non-binding memorandum of understanding with Nu-Cast Inc., Londonderry, N.H., to collaborate on new beryllium-aluminum investment casting projects and opportunities, initially for the aerospace sector. The goal is to increase manufacturing capacity and improve production efficiencies of IBC's proprietary near-net-shape beryllium-aluminum castings.

The two companies have identified opportunities for beryllium aluminum castings to support future growth. Nu-Cast has extensive experience with aluminum investment castings that will complement IBC's beryllium aluminum casting expertise. Pursuant to the MOU, the parties will initially evaluate and develop opportunities to expand IB-EMC's proprietary Beralcast alloys for aerospace applications.

The parties will also focus on joint business development initiatives aimed at increasing market share for IBC's castings, which offer significant cost savings and improved delivery times compared to the existing production methods.

"Nu-Cast has successfully served the aerospace sector for almost three decades and is an excellent complement to IBC's technology and corporate vision," said Don McKitterick, President of Nu-Cast. "By combining IBC's propriety and cost effective castings with Nu-Cast's manufacturing and marketing experience, we believe there is enormous potential for growth and we look forward to working with IBC on this opportunity."

Beralcast alloys can be used in virtually any high performance application requiring complex, lightweight and high-stiffness parts and can be substituted for aluminum, magnesium, titanium, metal matrix composites as well as pure beryllium or powder metallurgy beryllium-aluminum. Beralcast's principal alloys are more than three times stiffer than aluminum with 22% less weight and can be precision-cast for simple and complex three-dimensional stability. These high-modulus alloys are ideal for high-performance industrial and high-tech components, as well as for a wide range of aerospace applications.

www.ibcadvancedalloys.com 

IBC Advanced Alloys Corp., Vancouver, has signed a non-binding memorandum of understanding with Nu-Cast Inc., Londonderry, N.H., to collaborate on new beryllium-aluminum investment casting projects and opportunities, initially for the aerospace sector. The goal is to increase manufacturing capacity and improve production efficiencies of IBC’s proprietary near-net-shape beryllium-aluminum castings.

The two companies have identified opportunities for beryllium aluminum castings to support future growth. Nu-Cast has extensive experience with aluminum investment castings that will complement IBC’s beryllium aluminum casting expertise. Pursuant to the MOU, the parties will initially evaluate and develop opportunities to expand IB-EMC’s proprietary Beralcast alloys for aerospace applications.

The parties will also focus on joint business development initiatives aimed at increasing market share for IBC’s castings, which offer significant cost savings and improved delivery times compared to the existing production methods.

“Nu-Cast has successfully served the aerospace sector for almost three decades and is an excellent complement to IBC’s technology and corporate vision,” said Don McKitterick, President of Nu-Cast. “By combining IBC’s propriety and cost effective castings with Nu-Cast’s manufacturing and marketing experience, we believe there is enormous potential for growth and we look forward to working with IBC on this opportunity.”

Beralcast alloys can be used in virtually any high performance application requiring complex, lightweight and high-stiffness parts and can be substituted for aluminum, magnesium, titanium, metal matrix composites as well as pure beryllium or powder metallurgy beryllium-aluminum. Beralcast’s principal alloys are more than three times stiffer than aluminum with 22% less weight and can be precision-cast for simple and complex three-dimensional stability. These high-modulus alloys are ideal for high-performance industrial and high-tech components, as well as for a wide range of aerospace applications.