One Minute Mentor: Advantages and Limitations of Heat Treatment Simulation

April 3, 2025
Source: ASM International

One Minute Mentor: Advantages and Limitations of Heat Treatment Simulation

Heat treatment simulation can be a tool for optimization of heat-treatment processes, but at the present this method is still limited. Therefore most HTS is based on rough simplifications of the process. Simplifications can involve the process, number of phases, transformation kinetics, continuums models instead of micro-mechanical models, etc. These simplifications also result in inaccuracies in the calculations.

For more information, click on the link below (subscription required). Then scroll to Figure 16. R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014  https://doi.org/10.31399/asm.hb.v04d.a0005980

ECM establishes new vacuum furnace entity in mexico under MEXVAC ECM name


Source: ASM International

ECM establishes new vacuum furnace entity in mexico under MEXVAC ECM name

ECM USA, Pleasant Prairie, WI, announced the official launch of its new Mexican subsidiary, ECM Mexico, operating as MEXVAC ECM, S.A. DE C.V. This development marks a significant step in expanding ECM’s presence and service capabilities within the Mexican heat treatment industry.

The ECM Mexico team is led by operations manager Juan Cruz and field service and PLC engineer José López, under the direction of Pierre-Loic Rousset and Dennis Beauchesne. The team will work closely with ECM USA to provide localized support, reflecting ECM’s long-term commitment to strengthening service infrastructure for customers across Mexico.

The new entity will serve as a dedicated supplier of vacuum furnace technologies and support services, aiming to meet growing demand in the region for high-performance thermal processing equipment.

Read more

Bodycote joins energy industries council to expand engagement with global energy sector


Source: ASM International

Bodycote joins energy industries council to expand engagement with global energy sector

Bodycote, Macclesfield, UK, announced its membership with the Energy Industries Council (EIC), a leading global trade association for the energy sector. This move strengthens Bodycote’s strategic alignment with the evolving needs of the industry and reinforces its role as a provider of heat treatment and specialist thermal processing services across power generation and energy infrastructure markets.

Through its membership, Bodycote gains broader access to key industry stakeholders, enabling stronger supply chain collaboration and the pursuit of new business opportunities within the energy sector. The company serves a wide range of EIC members, fostering synergies that support innovation and operational excellence.

Bodycote’s engagement with the EIC supports its commitment to sustainability, particularly in nuclear and renewable energy markets. The partnership enhances customer access to Bodycote’s services via EIC platforms and events, further promoting solutions that improve performance, efficiency, and reliability in critical energy applications.

Read more

One Minute Mentor : Phase Transformations in Numerical Simulation

December 3, 2024
Source: ASM International

One Minute Mentor : Phase Transformations in Numerical Simulation

Heat treatment of tool steels means several phase transformations. Every phase transformation must be described by start amount, end amount, and kinetics (change of phases depending on temperature and time). Start and end amount can be calculated with different thermodynamic software. For example, Thermocalc is well validated for tool steels. The most common method for determining the transformation kinetics of main phases (e.g. ferrite, austenite, martensite, bainite) is to use dilatometric investigations. TTT (time-temperature-transformation) diagrams obtained from dilatometer measurements can be easily implemented in HTS software. An example is shown in the figure. 

For more information, click on the link below (subscription required). Then scroll to Figure 14. R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014  https://doi.org/10.31399/asm.hb.v04d.a0005980

HAI Romania enhances sustainable extrusion production with Nitrex system

November 30, 2024
Source: ASM International

HAI Romania enhances sustainable extrusion production with Nitrex system

Nitrex, Quebec, announced that it has implemented a new nitriding system at Hammerer Aluminium Industries (HAI) Romania, marking a significant step in advancing the sustainability of aluminum extrusion production. This installation aligns with HAI’s corporate commitment to environmental leadership and operational modernization.

HAI Romania, a subsidiary of Austria-based Hammerer Aluminium Industries, operates a state-of-the-art extrusion plant in Chișineu-Criș, near the Hungarian border. The facility features five extrusion presses, including a recently added 10-inch press, and serves key industries such as automotive, construction, and packaging, with strategic access to both Western and Eastern European markets.

The newly installed Nitrex NX-815 nitriding system replaces the traditional salt bath nitriding process. Unlike its predecessor, which generates environmentally challenging waste, the gas nitriding process offers a sustainable alternative. The system utilizes Nitreg® controlled nitriding and Nitreg®-C ferritic nitrocarburizing technologies, ensuring superior and consistent performance while minimizing environmental impact. With a 3,300-pound load capacity, the furnace is specifically designed for treating extrusion dies.

By adopting Nitreg® technologies, HAI Romania eliminates hazardous waste, reduces energy consumption, and enhances the durability of aluminum extrusion dies. This shift not only supports eco-friendly practices but also optimizes production efficiency by eliminating costly post-finishing operations, contributing to the company’s sustainability and operational goals.

Read further here

Solar Manufacturing ships Mentor Pro furnaces for renewable energy applications

October 14, 2024
Source: ASM International

Solar Manufacturing ships Mentor Pro furnaces for renewable energy applications

Solar Manufacturing, Sellersville, Pa., announced that it has shipped two Mentor Pro vacuum furnaces to a customer focused on developing advanced renewable energy technologies for large-scale industrial applications. The furnaces were selected after a collaborative process with the customer’s engineers, supported by the Research and Development team from Solar Manufacturing’s affiliate, Solar Atmospheres. The customer valued the furnace’s capabilities and compact design.

The Mentor Pro furnaces feature a molybdenum shielded hot zone, a maximum temperature capacity of 2500°F, and a workload capacity of up to 1000 pounds. They are equipped with SolarVac Essentials, a PLC-based control system, and include an internal gas quenching system with a 50 HP motor and variable frequency drive (VFD), offering flexibility in using nitrogen or argon gas for optimal metallurgical results. These features make the Mentor Pro well-suited for a variety of metallurgical applications in renewable energy development.

Read further here.

One Minute Mentor: Distortion of High-Speed Steels

September 30, 2024
Source: ASM International

One Minute Mentor: Distortion of High-Speed Steels

High-speed steels show a typical distortion behavior depending on the heat treatment parameters. The figure shows the change in length of cylindrical bars (diameter = 20 mm, or 0.8 in.) and length = 140 mm, or5.5 in.), with rolling direction longitudinal to the sample) for various heat treatment conditions with austenitizing, salt bath quenching, and double tempering.

Quenching and tempering up to 500 °C (930 °F) results only in very small changes in length (either growth or shrinking). Higher tempering temperatures lead to a transformation of the retained austenite into martensite and a corresponding growth in length. For typical tempering temperature of 560 °C (1040 °F) changes in length of about 0.2% take place. Additional alloying with Co (5%) leads to slightly higher changes in length. The effect of an additional third tempering shifts the curve slightly to the left, whereas oil quenching leads to a slight reduction of the change in length.

For more information, click on the link below (subscription required). Then scroll to Figure 9. R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014  https://doi.org/10.31399/asm.hb.v04d.a0005980

Lindberg/MPH ships aluminum melting and holding furnace


Source: ASM International

Lindberg/MPH ships aluminum melting and holding furnace

Lindberg/MPH, Mich., has announced the shipment of a gas-fired reverberatory aluminum melting and holding furnace equipped with a preheat hearth. The furnace, designed for manufacturing aluminum parts, boasts a melt rate of 10,000 pounds per hour and a maximum temperature rating of 1450°F. It has a holding capacity of 85,000 pounds, based on 155 pounds per cubic foot of molten aluminum.

The furnace features a vertically rising air-operated door for loading the preheat hearth and a full-width cleanout door at the rear for unloading. Designed with an elevated base, it includes a bottom-mounted magnetic stirring mechanism and an air pressure pump well for dispensing molten aluminum. This configuration allows the furnace to remain idle for extended periods without significant temperature variation.

Temperature control is managed by three controllers, while flame supervision equipment ensures safety, including forced-air purging and automatic shutdown in case of system failures.

Read further here.

 

Constellium announces significant weight savings in EV Battery enclosures through ALIVE project

September 16, 2024
Source: ASM International

Constellium announces significant weight savings in EV Battery enclosures through ALIVE project

Constellium, based in Paris, announced that its collaborative research project, Aluminium Intensive Vehicle Enclosures (ALIVE), has achieved weight savings of 12 to 35 percent for electric vehicle (EV) battery enclosures. The project, led by Constellium’s University Technology Center at Brunel University London, focused on optimizing the design and manufacturing processes for structural aluminum enclosures in EVs.

Launched in 2020, the £15 million initiative was partially funded by the UK government through the Advanced Propulsion Centre (APC). The project involved six industrial partners, including BMW, Volvo, and Innoval Technology, along with university technology partners from Brunel University London and the University of Warwick.

The ALIVE team developed new aluminum designs using Constellium’s high-strength alloys, HSA6® and HCA6®, while implementing advanced joining and forming technologies. Full-scale prototypes were produced and successfully passed rigorous testing for performance, safety, and fire resistance. The project also generated cost models to support future industrialization of the designs.

Read further here. 

Constellium’s Muscle Shoals facility receives Department of Defense grant to increase casting capacity

July 28, 2024
Source: ASM International

Constellium’s Muscle Shoals facility receives Department of Defense grant to increase casting capacity

Constellium, Muscle Shoals, AL, announces that its facility has been selected by the U.S. Department of Defense (DoD) for a $23 million investment under Title III of the Defense Production Act to rebuild its Direct Chill aluminum casting center.

The funding was awarded via the Defense Production Act Investments (DPAI) Program, overseen by the Manufacturing Capability Expansion and Investment Program (MCEIP) in the Office of the Assistant Secretary of Defense for Industrial Base Policy. Constellium will use the funds to install state-of-the-art casting equipment on the site of a dismantled casting center, adding up to 300 million pounds of annual casting capacity. With this added capacity, the plant expects to increase its recycled input, reduce its use of primary metal, and provide the U.S. industrial base with an additional, self-reliant domestic source of supply for aluminum rolling ingot.

“This investment under the Defense Production Act will enable our industry to meet the rapidly increasing demand for the aluminum products needed not only for our national security but also necessary for the overall U.S. manufacturing sector and a healthy economy,” commented Buddy Stemple, President of Constellium Muscle Shoals. “We are very excited to have this opportunity to partner with the DoD to help strengthen our industrial base.”

Constellium Muscle Shoals is a major aluminum sheet supplier for the packaging and automotive markets. The plant has the capacity to produce over 1 billion pounds per year of finished aluminum coils. Muscle Shoals also operates a world-class recycling center able to recycle the equivalent of 20 billion aluminum cans per year.

Read further here