One Minute Mentor: Carburizing Tool Steels
April 22, 2016
Source:
P20 mold steel is seldom carburized for molds used in compression molding, particularly for molding the more abrasive plastics. Carburizing temperatures no higher than 1650°F are recommended for this steel because higher temperatures may impair polishability; otherwise, conventional carburizing practice is used, and molds may be quenched in oil directly from the carburizing temperature. A common working range is 54 to 58 HRC.
The graph shows tempering characteristics of carburized mold steels.
(a) Upper curve represents steel carburized in hardwood charcoal 1675 to 1700°F for 8 hours, air cooled in pack, reheated at 1725 to 1750°F, cooled in air, and tempered. Middle curve represents steel carburized in cast iron chips at 1725 to 1750°F, removed from pack, cooled in air, and tempered.
(b) Surface hardness after heating at temperature for 2 hours in carburizing compound, followed by oil quenching and tempering.
Volume 4D, Heat Treating of Irons and Steels ⇒ Tool Steels ⇒ Heat Treating of Mold Steels and Corrosion-Resistant Tool Steels ⇒ Recommended Heat Treating Practices
P20 mold steel is seldom carburized for molds used in compression molding, particularly for molding the more abrasive plastics.
Continue reading
One Minute Mentor: Tempering Characteristics of P20 Mold Steel
March 11, 2016
Source:
Tempering characteristics for P20 mold steels carburized at two different temperatures are shown in the graphs. In (a), the upper curve represents steel carburized in hardwood charcoal at 1675 to 1700°F for eight hours, air cooled in pack, reheated at 1725 to 1750°F, cooled in air, and tempered. The middle curve represents steel carburized in cast iron chips at 1725 to 1750°F, removed from pack, cooled in air, and tempered. Graph (b) shows surface hardness after heating at temperature for two hours in a carburizing compound, followed by oil quenching and tempering.
Volume 4D, Heat Treating of Irons and Steels ⇒ Tool Steels ⇒ Heat Treating of Mold Steels and Corrosion-Resistant Tool Steels ⇒ Recommended Heat Treating Practices
Tempering characteristics for P20 mold steels carburized at two different temperatures are shown in the graphs.
Continue reading
Linde highlights advanced technologies at Heat Treat 2015
October 15, 2015
Source:
Linde LLC, Murray Hill, N.J., will showcase advanced gas control technologies and engineering services for heat treatment furnaces at Heat Treat 2015 next week in Detroit, booth 248. These include Carbojet gas-injection technology for improving production up to 20%; Hydroflex atmosphere control system for more reliable oxide-free annealing; world-class heat treatment engineering and laboratory services; and safety solutions for flammable atmosphere furnaces (re: NFPA 86)
These heat treatment services and proven technologies are in demand for improving process efficiency, productivity, and quality in manufacturing metal parts for automotive, aerospace, and military components; construction and industrial equipment; and electrical systems, to name a few. More consistent process quality can mean less rework and fewer rejects, and lead to higher profits, process reliability and longer service life.
Linde offers decades of experience in heat treatment across all common furnace types from continuous to batch type furnaces, including roller hearth, pusher, pit or rotary-retort. Expertise spans all typical protective atmospheres—from pure nitrogen, pure hydrogen, nitrogen/hydrogen, nitrogen/hydrocarbon type atmospheres to endothermic gas, exothermic gas and monogas atmospheres.
Improve gas flows and atmosphere homogeneity without fans
The patented CARBOJET gas-injection technology can improve efficiency and the productivity of heat treatment furnaces including roller hearth, pusher, pit, or rotary-retort. Ultrahigh-speed injection of a gas or gas mixture through special CARBOJET lances improves gas flows and atmosphere homogeneity without the use of circulation fans. This includes both the better mixing of the injected gases with the furnace atmosphere, and better movement of the gas flows within the furnace.
Oxide-free parts annealing
The HYDROFLEX atmosphere control system offers a universal solution for clean and bright oxide-free annealing of steel, stainless steel, copper, bronze or brass, with high reliability and repeatability. One or more carrier gases (nitrogen or argon) maintain the furnace pressure while a controlled ratio of hydrogen helps prevent oxidation. With the HYDROFLEX® technology, many annealing tasks can be completed with non-flammable gas mixtures containing less than 5 percent hydrogen.
Engineering and lab services
Engineering is key to optimizing heat treatment solutions. Linde engineers can perform process audits to investigate areas for improvement. This may include analyzing furnace atmospheres, gas supply and control systems, as well as upstream and downstream processes. Linde can also perform customer tests and demonstrations in furnaces at its Technology Center to support feasibility studies, and provide safety and process training.
In addition, engineers at Linde Application Centers can develop new gas supply systems for heat treatment processes and improve the control systems of existing processes. Our metallography laboratory services include material analyses, scanning electron micrography (SEM) and a variety of hardness tests.
Meeting new NFPA safety standards
The National Fire Protection Association (NFPA) is the industry accepted authority of industrial gases and furnaces. All heat treating facilities should familiarize themselves with NFPA 86 "Standard for Ovens and Furnaces". Within NFPA 86 there are specific requirements for Nitrogen Supply Systems used to purge flammable atmosphere furnaces. Linde developed the system to satisfy the NFPA 86 "Standard for Ovens and Furnaces." It includes a nitrogen supply system with an integral alarm panel for safety purge of flammable atmosphere furnaces.
Heat Treat 2015 is the premier heat treating event in North America and presented by the ASM Heat Treating Society. The conference and exposition run in conjunction with Gear Expo, presented by the American Gear Manufacturers Association.
Linde LLC, Murray Hill, N.J., will showcase advanced gas control technologies and engineering services for heat treatment furnaces at Heat Treat 2015 next week in Detroit, booth 248.
Continue reading