One Minute Mentor: Salt Bath Furnaces

August 15, 2023
Source: ASM International

One Minute Mentor: Salt Bath Furnaces

The salt bath method of hardening is predominant with high-speed steel tools. With correct operating conditions, tools can be heat treated without carburization, decarburization, and scaling. The surface will be fully hard with a minimum of distortion. The four types of salt baths generally used are preheating baths, high-temperature baths, quenching baths, and tempering baths.

Molten salts of various compositions are well adapted to all operations in the heat treatment of tool steels. For tools that cannot be ground after hardening or for tools that require an excellent surface condition and the maintenance of sharp edges, salt bath heating provides excellent results. These salt baths contain different compositions of BaCl2, NaCl2, and KCl as well as additional additives to avoid decarburization. The higher the working temperature, the higher the content of BaCl2 usually is. Higher additions of CaCl2 are typically used in salt baths for the quenching step.

For more information, click on the link below (subscription required). Then scroll to Figure 2.

R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014, https://doi.org/10.31399/asm.hb.v04d.a0005958

Steel Dynamics named one of America’s best employers for women by Forbes


Source: ASM International

Steel Dynamics named one of America’s best employers for women by Forbes

Steel Dynamics, Fort Wayne, Ind., has been named one of America’s Best Employers for Women for 2023 by Forbes. Steel Dynamics was the only steel producer receiving this designation.

“We are appreciative and honored by this recognition,” said Mark D. Millett, chairman and chief executive officer. “Our people are the foundation of our success and our most important resource. We strive to create a welcoming, open, and inclusive environment. We value our team members, creating meaningful opportunities for growth, leadership development, and career advancement. We believe empowering our people and providing them with the necessary tools for success creates significant value for everyone and will drive our continued success.”

Forbes partnered with Statista to compile the list of America’s Best Employers for Women. Statista surveyed over 60,000 U.S. employees working for companies with a minimum of 1,000 employees. More than 40,000 women were asked to rate their company in areas such as working environment, salary and employee diversity, and then whether they would recommend their company to a friend or family member.

Read further here.

Special fasteners to be processed in a Seco/Warwick vacuum furnace


Source: ASM International

Special fasteners to be processed in a Seco/Warwick vacuum furnace

Seco/Warwick, Meadville, Pa., will deliver a  Vector vacuum furnace to a plant producing highly advanced fasteners for the largest manufacturers in the aerospace industry. 

The machine will process self-locking nuts, nut plates, barrel nuts, stud nuts, spline nuts, clamp nuts, as well as a wide range of washers and flanges. The Italian Partner is an innovator in the field of comprehensive fastening solutions. The Vector furnace will become part of a modern production plant, increasing not only its efficiency, but also guaranteeing thermally treated fasteners of the highest quality.

The furnace on order is a standard solution perfectly suited to aviation industry needs. Thanks to a very refined design without any additional modifications, the furnace will perform at high operating temperatures, up to 1300°C.

The furnace on order is equipped with a dew point sensor for each of the gases. It is a system solving one of heat treatment’s very critical requirements, which is to control the quality/purity of the gas used during the process. Vector also features a partial pressure control system which helps prevent evaporation and sublimation of alloying elements from the load surface during the vacuum heat treatment.

Read further here.

One Minute Mentor: Distortion in Tool Steels

August 7, 2023
Source: ASM International

One Minute Mentor: Distortion in Tool Steels

Distortion in tool steels encompasses all irreversible dimensional changes. There are two main types: size distortion and shape distortion. Size distortion involves expansion or contraction in volume or linear dimensions without changes in geometrical form. Shape distortion entails changes in curvature or angular relations, as in twisting, bending, and/or nonsymmetrical changes in dimensions. In most cases both types of distortion occur during a heat-treatment operation.

Some of the main interactions occur between temperature, microstructure, and stress/strain. Especially for tool steels these interactions are mainly influenced by the carbon content in the steel matrix, the types and relative amounts of the alloying elements, and the carbide formation/transformation/precipitation characteristics of the alloy system.

For more information, click on the link below (subscription required). Then scroll to Figure 1..

R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014, https://doi.org/10.31399/asm.hb.v04d.a0005958

One Minute Mentor: Plasma Nitriding Equipment

August 2, 2023
Source: ASM International

One Minute Mentor: Plasma Nitriding Equipment

Cold-walled (double-walled water-cooled) systems were the first generation of plasma nitriding furnaces. This technology is also a vacuum-based process but employs the principle of glow discharge to provide energy for heating and nitriding at one time. Therefore, the independent control of the temperature stability and the nitriding intensity is not possible because both processes are using the same energy source—the plasma.

The hot-wall plasma nitriding furnaces, the next generation of cold-wall ion nitriding systems, are mainly used and built now. This system ensures optimal nitriding quality by fulfilling the highest demands on temperature and nitriding process control. The big advantage of this technology is the separation of the control of the heating and the plasma nitriding parameters. 

For more information, click on the link below (subscription required). Then scroll to Figure 26

R Schneider; R. Mesquita; H. Altena; T. Müller; P. Seemann, Processes and Furnace Equipment for Heat Treating of Tool Steels, ASM International, 2014, https://doi.org/10.31399/asm.hb.v04d.a0005958

Seco/Warwick delivers Vector vacuum furnace to revolver manufacturer


Source: ASM International

Seco/Warwick delivers Vector vacuum furnace to revolver manufacturer

Seco/Warwick, Meadville, Pa.,  received another order for the supply of a Vector vacuum furnace to a South American international manufacturer of weapons and military equipment. The furnace will process various components including barrels, reels, locks, and firearm magazines, which are expected to be reliable, of the highest quality, and perform with outstanding resistance to negative external conditions.

This will be the second solution of this type in the South American defense industry leader’s internal hardening plant. It is a single-chamber gas-cooled vacuum furnace which can be used for a variety of metal heat treatment processes and applications. This solution has been adapted to the customer’s requirements so that it is as effective as possible at delivering the precision heat treatment results required for quality weaponry.

Thanks to the large working space (900x900x1200 mm), the Vector system is designed to process quite large elements. A characteristic feature of the design is convection heating, which improves heat transfer efficiency when heating at lower temperatures, and directional cooling, which enables differentiated cooling of problematic parts in terms of shapes.

Read further here

Nitrex provides nitrocarburizing system to New Zealand heat treater


Source: ASM International

Nitrex provides nitrocarburizing system to New Zealand heat treater

Nitrex, Quebec, has announced that they have provided a nitrocarburizing system to Heat Treatments, a leading provider of commercial heat treatment services in New Zealand and one of Nitrex’s earliest customers.

Heat Treatments’ partnership with Nitrex dates to 1992 when they purchased its first Nitrex system with Nitreg nitriding capabilities. As operations grew, the company later added a second system in 2004 for nitrocarburizing and post-oxidation treatments. Contrary to the first two systems, which are identical pit furnaces, the latest addition, an NXK series, features the furnace and control panel mounted on an integral platform. Delivery, installation, and startup time and costs are reduced with this design. The NXK-812 model is designed to treat workloads weighing up to 1200 kg, with a diameter of 800 mm (31.5″) and a height of 1200 mm (47.25″). The system is equipped with advanced process technologies, including Nitreg-C controlled nitrocarburizing and ONC post-oxidation, which provide precise control and consistent results.

https://www.nitrex.com/

Mark Saline receives MPIF distinguished service award

July 9, 2023
Source: ASM International

Mark Saline receives MPIF distinguished service award

Gasbarre, Dubois, PaA, announced that Mark Saline, president of Gasbarre Thermal Processing Systems, is a recipient of the 2023 MPIF Distinguished Service to Powder Metallurgy (PM) Award that recognizes individuals who have actively served the North American PM industry for at least 25 years.The award is selected by the Metal Powder Industries Federation’s (MPIF) Awards Committee.

Over 70 nominated individuals were on the ballot for review by the past 10 years of Distinguished Service Award recipients, as well as the MPIF Board of Governors and Boards of Directors of the MPIF trade associations. Mark Saline will receive his award during PowderMet 2023 in Las Vegas. Mark has been well established in the Powder Metallurgy industry for many years. His PM involvement includes teaching students at the PM Sintering Seminar, sitting on the MPIF Program Committee, judging the PM Design Excellence Awards, he has written several publications on processing in continuous furnaces, and he provides input in organizations such as the Center for Powder Metal Technology, Powder Metal Equipment Association, and the Association for Metal Additive Manufacturing. Mark will also serve at the Conference Technical Chair-Person for PowderMet 2024 in Pittsburgh.

Read further here.

Can-Eng Furnaces contracted for continuous quench and temper furnace system

May 16, 2023
Source: ASM International

Can-Eng Furnaces contracted for continuous quench and temper furnace system

Can-Eng Furnaces International Ltd., Niagara, Ontario, was recently contracted to engineer and commission a continuous quench and temper furnace system for a North American producer of mining, construction, and materials handling products. The purchase of this equipment is part of a larger plant expansion and initiative to bring foreign outsourced manufacturing in house.  

This move is not only to improve part quality but also to help eliminate overall shipping costs and reduce supply chain issues which have been plaguing many industries over the past couple of years. This equipment will be part of an automated manufacturing cell and fed automatically from upstream handling equipment. Special considerations have been made to precisely control the quench temperature to reduce hardness variations and improve overall part quality.  

The multizone belt style temper furnace employs high efficiency natural gas fired heating and recirculation systems which have been proven to provide the ultimate in temperature uniformity in even the most demanding of applications.  

 

Read further here

Ipsen installs vacuum furnace at Taiwan Hodaka Technology


Source: ASM International

Ipsen installs vacuum furnace at Taiwan Hodaka Technology

Ipsen, Tainan City, Taiwan, has announced the installation of a TurboTreater vacuum furnace for a customer in Southeast Asia. Established in 2002, Taiwan Hodaka Technology Co., Ltd. is an aluminum extrusion supplier, specializing in high-end aerospace aluminum alloys. 

They also produce products used in the sporting goods, consumer electronics and automotive industries. The TurboTreater boasts a work zone size of 36” (914 mm) x 36” (914 mm) x 48” (1219mm) with a weight capacity of 3000 lb (1360 kg) and normal operating temperature up to 2400 °F (1315 °C). The furnace was designed with convection heating, allowing for more uniform processing of large cross-section parts and dense loads. It is also capable of quenching at up to 12 bar positive pressure in nitrogen.

Hodaka chose Ipsen for their positive brand reputation, technical capabilities and process know-how.

Read further here.