Constellium and renault group complete r&d project advancing lightweight aluminium solutions

February 5, 2025
Source: ASM International

Constellium and renault group complete r&d project advancing lightweight aluminium solutions

Constellium, Paris, announced the successful completion of the “ISA3” R&D project, an initiative launched in 2021 to advance lightweight aluminium solutions for automotive applications. Conducted in collaboration with Renault Group, ESI Group, the Institut de Soudure, and the University of Lorraine, the project was supported by a grant from the France Relance investment program. The research focused on developing cost-efficient, recyclable aluminium components to enhance vehicle performance and sustainability.

A key achievement of the project was the development of a lightweight aluminium door in partnership with Renault. Utilizing Constellium’s proprietary uni-alloy 6xxx rolled and extrusion-based solutions, the door design achieved a 14% weight reduction compared to existing aluminium doors used in compact battery electric vehicles. By employing a single alloy series, the project streamlined closed-loop recycling, reducing the door’s overall carbon footprint. This innovation resulted in a 33% reduction in Global Warming Potential (GWP), reinforcing the project’s emphasis on sustainability.

Beyond material advancements, the project also explored more efficient and flexible production processes to enhance performance while optimizing costs. Ludovic Piquier, senior vice president, manufacturing excellence and chief technical officer at Constellium, emphasized that the results highlight the company’s commitment to providing sustainable, high-performance aluminium solutions for the automotive sector.

Patrice Belliard, expert in flat products at Renault Group, noted that the project demonstrated how aluminium can support both weight reduction and cost efficiency in automotive manufacturing. Mathilde Chabin, manufacturing product director at ESI Group, added that the use of advanced pre-certification and validation technologies eliminated the need for physical prototypes, accelerating innovation while reducing costs and environmental impact.

The completion of Project ISA3 underscores the potential of aluminium to contribute to the automotive industry’s decarbonization efforts while delivering economic and environmental benefits.

Read further here. 

Solar Manufacturing ships Mentor Pro Furnace to a global leader of wire mesh products

April 15, 2024
Source: ASM International

Solar Manufacturing ships Mentor Pro Furnace to a global leader of wire mesh products

Solar Manufacturing, Sellersville, PA, has shipped a Mentor Pro Model HFL-3036-2IQ vacuum furnace to a customer specializing in engineered knitted wire mesh solutions. 

They are a USA-based company and a global supplier for the automotive, food service, and janitorial industries. The furnace will be primarily utilized for vacuum annealing materials that are susceptible to adverse effects of their mechanical properties when exposed to any levels of oxygen or nitrogen.

The Mentor® Pro features a molybdenum shielded hot zone measuring 18” wide x 18” high x 36” deep, capable of operating temperatures up to 2400°F, and a workload weight capacity of up to 1,000 lbs and includes the SolarVac® Essentials PLC-based control system. The internal gas cooling system with a 50 HP drive motor is capable of quenching workloads at 2-bar positive pressure in either nitrogen or argon.

Jason Davidson, regional sales manager, said that, “Our customer started running trials with our affiliate commercial heat treater, Solar Atmospheres. Once the trial results proved the heat-treat cycle, and the furnace demonstrated it could process the required quantities, the customer had confidence to place the purchase order with us.”

Read further here.

Can-Eng commissions mesh belt furnace overseas


Source: ASM International

Can-Eng commissions mesh belt furnace overseas

Can-Eng Furnaces, Niagara, Ontario,  has commissioned a continuous mesh belt heat-treat system for the production of high-quality automotive fasteners in Italy.

This project in the Piedmont region of Italy was one of four installation locations for this globally recognized producer of specialty automotive fasteners that span from Europe, South America, Mexico, and the United States of America.

Can-Eng Furnaces International Ltd was chosen to supply its state-of-the-art systems based on proven reliability, efficiency, and soft-part-handling features — hallmarks of Can-Eng’s mesh belt furnace systems. The new, high-volume fastener system features energy efficient combustion and waste heat recovery systems, atmosphere-controlled mesh belt hardening system, oil quench, post wash system, temper furnace, soluble oil system, bi-directional conveyor discharge, and Can-Eng’s Level 2 SCADA system. Can-Eng’s PET™ system provides the user with access to vital Industry 4.0 data which includes product traceability, detailed process data for continuous process improvements, comprehensive equipment diagnostics, cost analysis, and inventory management.

https://thermalprocessing.com/news/can-eng-commissions-mesh-belt-furnace-overseas/

Ipsen Launches “Ipsen Connect,” to Streamline Customers’ Operations

March 26, 2024
Source: ASM International

Ipsen Launches “Ipsen Connect,” to Streamline Customers’ Operations

Ipsen, Cherry Valley, IL, announced a new digital gateway, Ipsen Connect. The customer service portal simplifies access to essential resources, including order history, service requests, and furnace documentation.

Key features of Ipsen Connect include:

  • Convenient part management: Request or reorder parts, view order history, and access furnace documentation seamlessly.
  • Streamlined service requests: Schedule maintenance, troubleshooting, or calibration appointments in just a few clicks.
  • Best practices and expert insights: Access troubleshooting guides, online training videos, and answers to frequently asked questions.
  • Real-time updates: Keep your operations informed and on track with live updates, including order status, active quotes, planned maintenance, and scheduled service appointments.

https://ipsenglobal.com/knowledge-center/ipsen-launches-a-cutting-edge-digital-platform-ipsen-connect-to-streamline-customers-operations/

One Minute Mentor: High-Performance Line

February 6, 2024
Source: ASM International

One Minute Mentor: High-Performance Line

The continuous heat treatment of tool steel is applied to low- or medium-alloyed carbon steel strips as well as martensitic stainless steels. The described lines produce high-quality strip with respect to uniform structure, flatness, and bright surface finish. High quenching rates are necessary, especially for plain carbon steels. Cooling gradients of up to 600 K/s are possible in a molten lead-bismuth quench. Because two-stage quenching technology provides considerable advantages over quenching in oil, this method has been adopted worldwide. It is also possible to achieve isothermal transformation to bainite and pearlite using a molten metal quench, so this type of hardening and tempering line is extremely versatile.

The configuration of a high-performance line involves an entry and exit section of the strip handling equipment. The hardening section consists of the austenitizing furnace, the molten metal quench or hydrogen quench, and a martensite cooler.

For more information, click on the link below (subscription required). Then scroll to Figure 10. R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014 

Read further here.

One Minute Mentor: Continuous Operating Furnaces for Tool Steel Strips

December 4, 2023
Source: ASM International

One Minute Mentor: Continuous Operating Furnaces for Tool Steel Strips

The continuous heat treatment of tool steel is applied to low- or medium-alloyed carbon steel strips as well as martensitic stainless steels. The described lines produce high-quality strip with respect to uniform structure, flatness, and bright surface finish. Steel grades with 0.4 to 1.2% C, low and high alloyed, can be processed. 

Strip dimensions range between 10 to 750 mm (0.4 to 29.5 in.) wide and 0.05 to 4 mm (0.002 to 0.16 in.) thick. High quenching rates are necessary, especially for plain carbon steels. Cooling gradients of up to 600 K/s are possible in a molten lead-bismuth quench. Because two-stage quenching technology provides considerable advantages over quenching in oil, this method has been adopted worldwide. It is also possible to achieve isothermal transformation to bainite and pearlite using a molten metal quench, so this type of hardening and tempering line is extremely versatile.

For more information, click on the link below (subscription required). Then scroll to Figure 9. R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014  https://doi.org/10.31399/asm.hb.v04d.a0005958

One Minute Mentor: Indirectly heated fluidized-bed furnace

October 16, 2023
Source: ASM International

One Minute Mentor: Indirectly heated fluidized-bed furnace

Most fluidized-bed furnaces are used at temperatures below 1095 °C (2000 °F), although some manufacturers have furnaces capable of treating components to temperatures through 1205 °C (2200 °F). Initially, the gas flows upward through the permeable base to agitate the particles as the pressure is gradually increased. (b) Eventually, the gas flow is sufficient to lift the small particles of refractory materials and to transform the particle movement into a violent turbulent motion.

In the early 1980s, this furnace technology seemed to be on the right track as an alternative to salt bath technology, showing similar advantages and applications but without the environmental hazard of salt compounds, waste disposal, recycling of salts, and so on. Nowadays it can be concluded that salt bath technology was partially substituted by vacuum technology, but especially for bainitic hardening (austempering processes), salt baths are still commonly used and show a slightly growing tendency, whereas fluidized beds are hardly used any more.

This temperature limitation is related to the wear and tear on the retort materials at high temperatures, which was one of the reasons for the reduced interest in this furnace type after the initial hype.

For more information, click on the link below (subscription required). Then scroll to Figure 8.

R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014, https://doi.org/10.31399/asm.hb.v04d.a0005958

Lindberg/MPH completes roller hearth furnace system for the energy industry


Source: ASM International

Lindberg/MPH completes roller hearth furnace system for the energy industry

Lindberg/MPH, Mich., announced the installation of a roller hearth furnace system for a manufacturer of products used in the energy industry. The heat treat system is comprised of two box furnaces with quench tanks, a dual directional load transfer car, four companion draw batch ovens, and two stationary load/unload tables.

The maximum operating temperature of the box furnaces is 1850°F and they are designed for nitrogen-based atmosphere applications. The load space dimensions of the box furnaces are 48” W x 96” D x 36” H, and the internal chambers are larger to provide clearance for baskets or fixtures. A snake chain pusher assembly is used by each furnace to transfer the loads from the chamber to the quench elevator deck.

Read further here.

Wisconsin Oven to ship three custom conveyor ovens to the molded-fiber industry


Source: ASM International

Wisconsin Oven to ship three custom conveyor ovens to the molded-fiber industry

Wisconsin Oven, East Troy, is scheduled to ship three custom dryers to a manufacturer in the molded-fiber industry. The ovens will be used for drying thick-walled paper pulp molded fiber packaging material used in a variety of products. Molded fiber packaging is made of 100% recycled materials, making them an environmentally friendly solution for companies looking to use sustainable packaging and reduce their environmental impact.

These paper pulp drying conveyor ovens are designed with four temperature zones, and each has the sufficient capability to remove 850 pounds of water per hour from the molded pulp. The ovens feature a maximum temperature rating of 500°. The work chamber dimensions are 8’ W x 120’ L x 1’ H. A total of twelve personnel access doors with explosion relief latches are located on the sides of each unit. Each unit also has stainless steel sheet metal and structure on the wet end to reduce corrosion.

The conveyor ovens are designed with top-down and bottom-up airflow to maximize the drying rate of the paper pulp shapes. The flat wire belt continuous conveyor system uses a variable frequency drive that is adjustable from 0-3 FPM. Emergency stop buttons are located at the load and unload sections of each oven for operator safety.

Read further here. 

Medical implant hardening in a SECO/WARWICK furnace


Source: ASM International

Medical implant hardening in a SECO/WARWICK furnace

SECO/WARWICK, Meadville, PA, announced that they will supply a Vector vacuum furnace to the Marle Group, a global manufacturer of orthopedic prostheses. The furnace on order will be used for the heat treatment of cobalt implants. Cobalt alloy hardening requires very high temperatures, and the heating process for these materials require a high puriity environment, temperature uniformity and very fast and effective cooling.

In order for cobalt alloys to be used in implantology, they must be deprived of their ferromagnetic properties. This shiny, hard metal loses this property only when it reaches a temperature higher than 1131°C. Such a high temperature makes it necessary to use a vacuum furnace in the implant production process. The furnace can not only provide such a temperature, but also guarantees its maintenance over a longer period of time. As a comparison, the temperature, above which a ferSECO/WARWICK, Meadville, PA, announced that they will supply a Vector vacuum furnace to the Marle Group, a global manufacturer of orthopedic prostheses. The furnace on order will be used for the heat treatment of cobalt implants. Cobalt alloy hardening requires very high temperatures, and the heating process for these materials require a high puriity environment, temperature uniformity and very fast and effective cooling.