Alcoa Dura-Bright commercial truck wheel is ten times more resistant to corrosion

January 24, 2014
Source:

Alcoa, Pittsburgh, introduces the surface-treated Dura-Bright EVO commercial truck wheel, said to be ten times more resistant to corrosion that is primarily caused by road salts and weather. Dura-Bright is not a coating, but rather a surface treatment that penetrates the aluminum and becomes an integral part of the wheel. In addition, Alcoa's wheels are made from one piece of forged aluminum, making them lighter and five times stronger than steel wheels, increasing payload and fuel efficiency.

In addition, the wheel is up to three times more resistant to chemicals, including hydrofluoric acid, found in the toughest truck wash cleaning agents. This enables the use of a wider variety of cleaning solutions to simplify maintenance, while preserving the integrity and brightness of the wheel.

Alcoa's surface treatment experts at the Alcoa Technical Center developed the Dura-Bright wheel technology in collaboration with the Alcoa Wheel and Transportation Products business. The Company launched the first Dura-Bright product in 2003. Three years later, Alcoa's experts improved the brightness and corrosion performance of the Dura-Bright treatment and introduced Dura-Bright wheels with XBR technology. Alcoa's scientists have now enhanced the patented Dura-Bright technology with the development of Dura-Bright EVO wheels.

The Dura-Bright EVO wheel is now commercially available in Europe, where the Company has already seen significant adoption of its Dura-Bright wheels. Alcoa has begun producing the wheel at its manufacturing plant in Székesfehérvár, Hungary. The wheel is expected to be available in all other markets in 2015.

http://www.alcoa.com/global/en/news/news_detail.asp?pageID=20140123000187en&newsYear=2014

 

Alcoa Dura-Bright commercial truck wheel is ten times more resistant to corrosion

Alcoa, Pittsburgh, introduces the surface-treated Dura-Bright EVO commercial truck wheel, said to be ten times more resistant to corrosion that is primarily caused by road salts and weather.

Continue reading

ThyssenKrupp Aerospace acquires aerospace operations of Alimex Metallhandelsgesellschaft

January 22, 2014
Source:

 

ThyssenKrupp Aerospace, Germany, has acquired the aerospace operations of Alimex Metallhandelsgesellschaft GmbH, Willich, Germany. ThyssenKrupp Aerospace will continue Alimex's business of distributing and processing aluminum mill products (rod, sheet, plate) for the aviation industry. All inventories and the customer network will also be transferred to ThyssenKrupp Aerospace. Alimex is withdrawing completely from the aerospace sector but will continue its other areas of business.

"The acquisition of Alimex's aerospace business is a further step in our strategy to strengthen our market position and expand our product and service portfolio. For existing customers of Alimex, nothing will change - on the contrary, all supply and processing services will continue in the same quality and will be complemented by ThyssenKrupp Aerospace's product line," says Management Board member Sebastian Gudel.

http://www.thyssenkrupp.com/en/presse/art_detail.html&eid=TKBase_1389976375500_1633998296&source=newsletter

ThyssenKrupp Aerospace acquires aerospace operations of Alimex Metallhandelsgesellschaft

ThyssenKrupp Aerospace will continue Alimex’s business of distributing and processing aluminum mill products (rod, sheet, plate) for the aviation industry.

Continue reading

Uddeholm SuperClean Concept PM tool steels resist abrasion, chipping, elevated temperatures


Source:

Uddeholm AB, Sweden, introduces Uddeholm SuperClean Concept powder metallurgy (PM) tool steels, building on the proven success of its current PM tool steel grades. The Uddeholm PM production process eliminates the macro segregation encountered in conventional ingot metallurgical production of higher-alloy tool steel. The process also eliminates the inclusions that limit the performance of most other PM steels.

Grades include:

Uddeholm Vanadis 4 Extra SuperClean – with chipping resistance that none can match

Uddeholm Vanadis 10 SuperClean – with extremely high abrasive wear resistance

Uddeholm Vanadis 23 SuperClean – perfect for high volume cold work applications

Uddeholm Vanadis 30/Vanadis® 60 SuperClean – for tooling at elevated temperature

Uddeholm Vancron 40 SuperClean – the Marathon runner of tool steel

Uddeholm Elmax SuperClean – specially developed for high-tech applications

http://www.uddeholm.com/superclean.htm

 

Uddeholm SuperClean Concept PM tool steels resist abrasion, chipping, elevated temperatures

Uddeholm AB, Sweden, introduces Uddeholm SuperClean Concept powder metallurgy (PM) tool steels, building on the proven success of its current PM tool steel grades.

Continue reading

Instron 5900 Series universal testing instruments enable acquisition rates up to 2500 points/second


Source:

Instron, Norwood, Mass., offers the 5900 Series universal testing instruments, which are designed with enhancements that deliver unparalleled accuracy and reliability, improved ergonomics, and an enhanced overall experience for the operator. Industry-leading features include load measurement accuracy to +/-0.5% of reading down to 1/1000 of load cell capacity; and fast, synchronized data acquisition rates up to 2500 points per second.

The most common uses of these mechanical testing systems are for tensile, compression, bend, peel, shear, tear and cyclic tests. Configured systems are fully capable of meeting test requirements per ASTM, ISO, DIN, TAPPI, GB, JIS, ANSI, NAS, etc.

Frame types include the 5940 single column tabletop for low-force testing up to 2 kN; the 5960 dual column tabletop systems for mid-range testing up to 50 kN; and the 5980 floor model systems for heavy- duty, robust testing up to 600 kN. The control panel is an integral component of the testing system, reducing setup time and increasing testing efficiency through the use of programmable live displays and soft keys. Tests can be set up and run directly from the control panel.

www.instron.com

 

Instron 5900 Series universal testing instruments enable acquisition rates up to 2500 points/second

Instron, Norwood, Mass., offers the 5900 Series universal testing instruments, which are designed with enhancements that deliver unparalleled accuracy and reliability.

Continue reading

Vac Aero ships horizontal vacuum furnace to an R&D center

January 20, 2014
Source:

Vac Aero, Burlington, Ontario, recently shipped a horizontal vacuum furnace to the Québec Metallurgy Centre, a research institute affiliated with the Trois-Rivières college in Québec. The VAH2636 HV-2 furnace will be housed in a new a state-of-the-art facility in Trois-Rivières. The chamber size is 23 X 18 X 36 inches, with a metal hot zone designed for operating at temperatures up to 2400°F. The furnace operating system is based on Vac Aero's versatile HC900 interactive hybrid control package with SCADA and complete network integration capabilities, as well as remote monitoring and control.

Created in 1985, the Québec Metallurgy Centre is a collegiate center of technological transfer affiliated with the Trois-Rivières College. The center's focus is to support the technological development of Québec-based manufacturing companies in the metallurgical sector. The Québec Metallurgy Centre provides an incomparable knowledge base on metallic and ceramic materials as well as on metallurgical processes.

www.vacaero.com

 

Vac Aero ships horizontal vacuum furnace to an R&D center

Vac Aero, Burlington, Ontario, recently shipped a horizontal vacuum furnace to the Québec Metallurgy Centre, a research institute affiliated with the Trois-Rivières college in Québec. The VAH2636 HV-2 furnace will be housed in a new a state-of-the-art facility in Trois-Rivières.

Continue reading

Tapping energy from the sun through heat and light


Source:

A new approach to harvesting solar energy, developed by Massachusetts Institute of Technology, Cambridge, researchers, could improve efficiency by using sunlight to heat a high-temperature material whose infrared radiation would then be collected by a conventional photovoltaic cell. This technique could also make it easier to store the energy for later use, say researchers.

Adding the extra step in this case improves performance because it makes taking advantage of wavelengths of light that ordinarily go to waste possible. A conventional silicon-based solar cell "doesn't take advantage of all the photons," explains associate professor of mechanical engineering Evelyn Wang. That's because converting the energy of a photon into electricity requires that the photon's energy level match that of a characteristic of the photovoltaic (PV) material called a bandgap. Silicon's bandgap responds to many wavelengths of light, but misses many others.

To address that limitation, the team inserted a two-layer absorber-emitter device—made of novel materials including carbon nanotubes and photonic crystals—between the sunlight and the PV cell. This intermediate material collects energy from a broad spectrum of sunlight, heating up in the process. When it heats up, as with a piece of iron that glows red hot, it emits light of a particular wavelength, which in this case is tuned to match the bandgap of the PV cell mounted nearby.

This basic concept has been explored for several years, since in theory such solar thermophotovoltaic (STPV) systems could provide a way to circumvent a theoretical limit on the energy-conversion efficiency of semiconductor-based photovoltaic devices. That limit, called the Shockley-Queisser limit, imposes a cap of 33.7% on such efficiency, but Wang says that with TPV systems, "the efficiency would be significantly higher—it could ideally be over 80%."

There have been many practical obstacles to realizing that potential; previous experiments have been unable to produce a STPV device with efficiency of greater than 1%. But Lenert, Wang, and their team have already produced an initial test device with a measured efficiency of 3.2%, and they say with further work they expect to be able to reach 20% efficiency—enough, they say, for a commercially viable product.

The design of the two-layer absorber-emitter material is key to this improvement. Its outer layer, facing the sunlight, is an array of multiwalled carbon nanotubes, which very efficiently absorbs the light's energy and turns it to heat. This layer is bonded tightly to a layer of a photonic crystal, which is precisely engineered so that when it is heated by the attached layer of nanotubes, it "glows" with light whose peak intensity is mostly above the bandgap of the adjacent PV, ensuring that most of the energy collected by the absorber is then turned into electricity.

In their experiments, the researchers used simulated sunlight, and found that its peak efficiency came when its intensity was equivalent to a focusing system that concentrates sunlight by a factor of 750. This light heated the absorber-emitter to a temperature of 962°C.

This level of concentration is already much lower than in previous attempts at STPV systems, which concentrated sunlight by a factor of several thousand. But the MIT researchers say that after further optimization, it should be possible to get the same kind of enhancement at even lower sunlight concentrations, making the systems easier to operate.

Such a system, the team says, combines the advantages of solar photovoltaic systems, which turn sunlight directly into electricity, and solar thermal systems, which can have an advantage for delayed use because heat can be more easily stored than electricity. The new solar thermophotovoltaic systems, they say, could provide efficiency because of their broadband absorption of sunlight; scalability and compactness, because they are based on existing chip-manufacturing technology; and ease of energy storage, because of their reliance on heat.

Some of the ways to further improve the system are quite straightforward. Since the intermediate stage of the system, the absorber-emitter, relies on high temperatures, its size is crucial: The larger an object, the less surface area it has in relation to its volume, so heat losses decline rapidly with increasing size. The initial tests were done on a 1 cm chip, but follow-up tests will be done with a 10 cm chip, they say.

Zhuomin Zhang, a professor of mechanical engineering at the Georgia Institute of Technology who was not involved in this research, says, "This work is a breakthrough in solar thermophotovoltaics, which in principle may achieve higher efficiency than conventional solar cells because STPV can take advantage of the whole solar spectrum. … This achievement paves the way for rapidly boosting the STPV efficiency."

The research team also included MIT graduate students David Bierman and Walker Chan, former postdoc Youngsuk Nam, and research scientist Ivan Celanović. The work was funded by the U.S. Department of Energy through MIT's Solid-State Solar Thermal Energy Conversion (S3TEC) Center, as well as the Martin Family Society, the MIT Energy Initiative, and the National Science Foundation.

More information:

MIT

Image caption — A nanophotonic solar thermophotovoltaic device composed of an array of multi‑walled carbon nanotubes as the absorber, a one‑dimensional silicon/silicon dioxide photonic crystal as the emitter, and a 0.55 eV photovoltaic cell. Courtesy of John Freidah.

Tapping energy from the sun through heat and light

A new approach to harvesting solar energy, developed by Massachusetts Institute of Technology, Cambridge, researchers, could improve efficiency by using sunlight to heat a high-temperature material whose infrared radiation would then be collected by a conventional photovoltaic cell.

Continue reading

Nitrex turnkey systems enable nitriding/nitrocarburizing for Polish aerospace company

January 17, 2014
Source: ASM International

Nitrex turnkey systems enable nitriding/nitrocarburizing for Polish aerospace company

Nitrex Metal, St. Laurent, Quebec, reports that Polish aircraft engine and gear transmission manufacturer WSK “PZL- Kalisz” has started production on its new NXK-609 nitriding system from Nitrex Metal. The self-contained turnkey system, which has a diameter of 24 in. and a height of 36 in., nitrides gears and housings supplied to many world-leading aerospace firms. Nitriding with Nitreg technology meets the company’s requirement for precise control of the white layer thickness on Nitralloy parts, including zero white layer.

Continue reading

Hitachi VP-SEM offers four-axis motorized stage for smaller samples


Source: ASM International

Hitachi VP-SEM offers four-axis motorized stage for smaller samples

The Nanotechnology Systems Division of Hitachi High Technologies America Inc., Clarksburg, Md., announces that its latest VP-SEM system, Model SU3500, is now available with a four-axis motorized stage, in addition to the existing five-axis motorized stage system. The new four-axis version is targeted for smaller sample applications (max. 200 mm in diameter and 70 mm in height).

Continue reading

Ipsen ships large aluminum brazing furnace to aerospace company


Source:

Ipsen, Cherry Valey, Ill., announces that it shipped a large vertical vacuum aluminum brazing furnace to a major aerospace company, a longstanding customer. This furnace, the customer's second vertical furnace, will be installed in Mexico. Two other TurboTreaters will be shipped to Southeast Asia for the same aerospace company. One of these furnaces will be used for high-pressure gas quenching; the other includes AvaC  for low-pressure vacuum carburizing.

Ipsen, known for quality products and reliability, is committed to furthering the success of its customers, including those in the aerospace industry. To ensure safety and consistency, many aerospace manufacturers, have established their own specifications that must be met or exceeded to produce their parts. Ipsen provides the expert guidance to build the furnaces best-suited for each customer's processes and capable of meeting not only their requirements, but also those of AMS 2750E and Nadcap.

www.ipsenusa.com

Ipsen ships large aluminum brazing furnace to aerospace company

Ipsen, Cherry Valley, Ill., announces that it shipped a large vertical vacuum aluminum brazing furnace to a major aerospace company, a longstanding customer. This furnace, the customer’s second vertical furnace, will be installed in Mexico. Two other TurboTreaters will be shipped to Southeast Asia for the same aerospace company. One of these furnaces will be used for high-pressure gas quenching; the other includes AvaC for low-pressure vacuum carburizing.

Continue reading

Centorr designs furnace for metal injection molding


Source:

Centorr Vacuum Industries, Nashua, N.H., has developed the MIM-Vac, a custom-engineered high temperature vacuum/ controlled-atmosphere furnace designed specifically for metal injection molding. Tight partial pressure control and even gas flow in conjunction with effective event-based programming and sound retort design allow the entire load to undergo  the same series of conditions as a function of time. This results in consistent microstructures and repeatable carbon control. The MIM-Vac  is designed primarily for second-stage binder removal and sintering, and has a number of design improvements specific for use with MIM feedstocks.

The revolutionary new gas-plenum retort has rows of perforations allowing even gas flow across all the work trays, and features alumina ceramic support members for ease of construction and replacement. The work grid assembly also incorporates alumina ceramic as tray supports for reduced metal-to-metal contact, resulting in less sticking. The grid assembly is removable for production loading outside the unit, and can be inserted into the chamber by load truck, eliminating hand loading of individual trays.

Depending on the customer's process requirements, a variety of wax and polymer condensation strategies have been developed, including vacuum delube/condensation; Sweepgas; Injectavac BRS; MIM-Vac BRS; and Thermal Incineration.

Learn more.

Centorr designs furnace for metal injection molding

Centorr Vacuum Industries, Nashua, N.H., has developed the MIM-Vac, a custom-engineered high temperature vacuum/ controlled-atmosphere furnace designed specifically for metal injection molding. Tight partial pressure control and even gas flow in conjunction with effective event-based programming and sound retort design allow the entire load to undergo the same series of conditions as a function of time.