One Minute Mentor: Effect of Ledeburite Carbides
November 13, 2015
Source:
For ledeburitic tool steels (typical 8-12%-Cr cold-work tool steels and high-speed steels) the interaction of carbides with the matrix must be taken into account, especially when these carbides are strongly oriented after plastic deformation (rolling, forging) of the pre-material.
The longitudinal direction of the carbides is usually parallel to this forming direction. Different authors suggest that the orientation of forming is the preferred direction of change in length caused by hardening. For the tool maker it is important to take this behavior into account.
Results from investigations of a ledeburitic cold work tool steel are shown in the graph. The micromechanical interactions between carbides and the matrix cause an inhomogeneous change in length during austenitizing as well as during quenching. Finally, an elongation in the longitudinal direction and a shrinking in the transverse direction remain.
Volume 4D, Heat Treating of Irons and Steels -> Tool Steels -> Distortion in Tool Steels -> Nature and Causes of Distortion
For ledeburitic tool steels (typical 8-12%-Cr cold-work tool steels and high-speed steels) the interaction of carbides with the matrix must be taken into account, especially when these carbides are strongly oriented after plastic deformation (rolling, forging) of the pre-material.
Continue reading
White House Energy Summit focuses on advancing technology safety and low-cost energy
November 12, 2015
Source:
Speaking at the White House Summit on Nuclear Energy on November 6, physicist Christina Back of General Atomics (GA), San Diego, highlighted the urgency of developing next-generation fast-gas reactors with new materials to enhance safety and ensure energy security.
As GA's Director of Nuclear Technologies and Materials, Back specializes in developing new heat-resistant ceramics to enable delivery of cost-competitive clean energy with unprecedented safety via the innovative gas-cooled reactor, the Energy Multiplier Module or EM2.
She participated as one of five expert panelists at a forum spotlighting the Obama Administration's commitment to advanced nuclear energy and maintaining U.S. technology leadership in the industry. Back emphasized during her remarks that nuclear energy is the dominant energy source that is sustainable, compatible with 21st century power grids and free of greenhouse gases.
Panelists featured nuclear energy industry leaders including John Kotek, Acting Assistant Secretary for Nuclear Energy in the Department of Energy. The invited audience included leaders in academia, government, labor, environmental organizations, the nuclear industry, non-governmental organizations, think tanks and the investment community.
The panel focused on innovations in nuclear energy, with Back explaining that the design of EM2 draws on GA's 60 years of experience in designing and building safe reactors and aims to solve four big challenges: safety, waste, economics, and nonproliferation.
"Nuclear energy is important for the security of our country," says Back, noting that to turn new technology innovation into clean-energy reality, "We need investment and support from the DOE and Congress and the nation to understand what the challenges are, but also to understand what the huge payoff and benefits are for our country."
EM2 is a gas-cooled fast reactor designed to deliver low-cost nuclear energy by using a high-efficiency system, a "convert-and-burn" fuel cycle able to produce 265 megawatts-electric, in a compact modular design. It incorporates industry-leading safety and nonproliferation features and can run on nuclear waste.
The White House Summit on Nuclear Energy was billed by officials as a forum for highlighting the Administration's commitment to nuclear energy as a clean energy solution and "for maintaining U.S. leadership in nuclear energy to realize economic competitiveness, national security and nonproliferation objectives."
GA continues to be a leader in fission and fusion focused on a wide range of energy solutions. The DIII-D National Fusion Facility, operated by GA for the U.S. Department of Energy, is the largest magnetic fusion device in the nation and one of the largest in the world. GA is also a leading manufacturer of precision technology for inertial confinement fusion.
Image caption — EM2 waste-to-energy fast-gas reactor being developed by General Atomics with unprecedented safety innovations.
Speaking at the White House Summit on Nuclear Energy physicist Christina Back of General Atomics highlighted the urgency of developing next-generation fast-gas reactors with new materials to enhance safety and ensure energy security.
Continue reading
Ipsen furnace enables California Brazing to increase aluminum brazing capacity
November 11, 2015
Source:
Ipsen USA, Cherry Valley, Ill., reports that California Brazing recently purchased its third vacuum aluminum brazing (VAB) furnace from Ipsen, to expand capacity and manufacture a variety of aluminum-brazed assemblies. These include cold plates, heat exchangers, waveguides, and antennas, for customers in the aerospace, defense, and semiconductor industries.
The furnace features an all-metal hot zone with dimensions 38 x 40 x 62 inches. It has a 1500-pound load capacity, and it operates at temperatures of 500 to 1200°F, with ±5°F temperature uniformity. It is also equipped with a 35-inch diffusion pump and Ipsen's CompuVac control system.
Featuring multiple individually controlled heating zones, Ipsen's VAB furnaces provide fast cycle times and precise, uniform heating of the workload. In addition, joint-free heating elements eliminate resistance buildup and hot spots.
"There is a growing need for aluminum-brazed assemblies across multiple industries," says Jeff Ager, General Manager at California Brazing. "California Brazing is committed to meeting our customers' requirements by continuing to invest in brazing and machining equipment to further improve capabilities, lead times, and quality."
www.IpsenUSA.com/VAB
Ipsen USA, Cherry Valley, Ill., reports that California Brazing recently purchased its third vacuum aluminum brazing (VAB) furnace from Ipsen, to expand capacity and manufacture a variety of aluminum-brazed assemblies.
Continue reading
Nucor to acquire Gerdau’s cold-drawn steel bar assets in Ohio and Georgia
Source:
Nucor Corp., Charlotte, N.C., has agreed to acquire Gerdau Long Steel's Bright Bar assets located in Orrville, Ohio, and Cartersville, Georgia, which manufacture cold-drawn steel bars and have a combined production capacity of 75,000 tons per year.
"This acquisition advances Nucor's strong competitive position in cold-finished bar and increases our downstream participation in this important channel to market," says John Ferriola, Chairman, CEO, and President of Nucor. "This acquisition improves our geographic coverage and expands our range of products in this market segment.
Nucor and its affiliates are manufacturers of steel products, with operating facilities primarily in the United States and Canada. Products include carbon and alloy steel – in bars, beams, sheet and plate; steel pilings; steel joists and joist girders; steel deck; fabricated concrete reinforcing steel; cold-finished steel; steel fasteners; metal building systems; steel grating and expanded metal; and wire and wire mesh.
Through the David J. Joseph Company, Nucor also brokers ferrous and nonferrous metals, pig iron, and HBI/DRI; supplies ferro-alloys; and processes ferrous and nonferrous scrap. Nucor is North America's largest recycler.
http://www.nucor.com
Nucor Corp., Charlotte, N.C., has agreed to acquire Gerdau Long Steel’s Bright Bar assets located in Orrville, Ohio, and Cartersville, Georgia, which manufacture cold-drawn steel bars and have a combined production capacity of 75,000 tons per year.
Continue reading
Ambrell launches Ekoheat with VPA for improved induction processes
Source:
Ambrell, Scottsville, N.Y., has launched a line of Ekoheat products featuring Versatile Performance Architecture (VPA), which enables a product to integrate into manufacturing systems, or to function as a stand-alone induction heating solution. The Autoscan capability includes easy-to-use functionality to scan a new application and auto-set the starting frequency, and then recommend RF setup parameters.
The products include soft-start circuitry, a safety feature that eliminates the risk of tripping up other equipment when a power supply is turned on. System power is tightly controlled on start-up to minimize transient spikes and electrical noise.
Ekoheat VPA includes a universal printed circuit board that can be used across the entire product line. This means fast availability of service repair and replacement parts, assuring business continuity and long-lasting product life. Regardless of system size and frequency, common PCBs are integrated into the designs. A single board-set addresses multiple systems, thereby minimizing inventory and eliminating model-specific versions.
These products are enabled for remote diagnostics and data collection with industrial Ethernet communication capabilities. In the industrial and automation environment, networking is fully supported using Ekoheat VPA's chosen gateway and includes CIPs (Common Industrial Protocols) such as EthernetIP, Modbus/TCP, and PROFINET protocols.
www.ambrell.com
Ambrell, Scottsville, N.Y., has launched a line of Ekoheat products featuring Versatile Performance Architecture (VPA), which enables a product to integrate into manufacturing systems or to function as a stand-alone induction heating solution.
Continue reading
Air Force selects Northrop Grumman to build new long-range bomber
Source:
The U.S. Air Force has selected Northrop Grumman Corp., Falls Church, Va., the company that developed and manufactured the B-2 Spirit stealth bomber, to deliver the new Long-Range Strike Bomber, which is also to be stealthy. The company has continued to develop stealthy systems, such as the stealthy X-47B unmanned aircraft.
"The Air Force has made the right decision for our nation's security," said Wes Bush, chairman, chief executive officer, and president of Northrop Grumman. "We look forward to providing the Air Force with a highly capable and affordable next-generation Long-Range Strike Bomber."
Northrop Grumman is a leading global security company providing innovative systems, products and solutions in unmanned systems, cyber, C4ISR, and logistics and modernization to government and commercial customers worldwide.
www.northropgrumman.com
The U.S. Air Force has selected Northrop Grumman Corp., Falls Church, Va., the company that developed the B-2 Spirit stealth bomber, to deliver the new Long-Range Strike Bomber, which is also to be stealthy.
Continue reading
Titanium strength and ductility grow when large grains are added to microstructure
Source: ASM International
A team from North Carolina State University, Raleigh, and the Chinese Academy of Sciences announces that titanium strength and ductility are both increased when large grains are added to an ultrafine-grain matrix.
Continue reading
Lockheed Martin closes acquisition of Sikorsky Aircraft
November 9, 2015
Source:
Lockheed Martin, Bethesda, Md., has closed its acquisition of Sikorsky Aircraft, a world leader in military and commercial rotary-wing aircraft. Aligned under the Lockheed Martin Mission Systems and Training (MST) business segment, Sikorsky Aircraft is now known as Sikorsky, a Lockheed Martin company.
"Today we are proud to welcome the Sikorsky team to Lockheed Martin," said Marillyn Hewson, Lockheed Martin chairman, president, and CEO. "Lockheed Martin and Sikorsky share a legacy of innovation and performance that has shaped the history of aviation for more than a century. Together, we are even better positioned to provide the best value for our customers, employees, and shareholders."
The acquisition advances Lockheed Martin's commitment to provide its customers with mission-ready solutions that are affordable and efficient, while expanding its core business into the growing areas of helicopter production and sustainment. Sikorsky's ability to leverage Lockheed Martin's scale will ensure that it remains a technology leader at the forefront of vertical lift.
Dan Schultz has been named president of Sikorsky, a Lockheed Martin Company. Mr. Schultz led the integration efforts for Lockheed Martin leading up to the closure, and he previously served as the vice president for Lockheed Martin's Ship & Aviation Systems line of business within MST.
"Dan is a former Marine helicopter pilot and has decades of experience in the rotary-wing segment, including leading Lockheed Martin's helicopter system integration business," Ms. Hewson said. "He brings a wealth of leadership experience and a deep understanding of our international customer base. I am confident he is the right person to lead Sikorsky at this pivotal time."
Sikorsky, a Lockheed Martin company, will retain its headquarters in Stratford, Connecticut. The line of business employs nearly 15,000 employees in 11 countries. Its helicopters are used by all five branches of the U.S. armed forces, along with military services and commercial operators in 40 nations.
www.lockheedmartin.com/sikorsky
Lockheed Martin, Bethesda, Md., has closed its acquisition of Sikorsky Aircraft, a world leader in military and commercial rotary-wing aircraft.
Continue reading
Silver nanoparticles in polymer coating prevent infections in dental implants
November 8, 2015
Source:
Researchers at the Fraunhofer Institute, Germany, have reportedly developed DentaPlas, an antimicrobial coating for dental implants that consists of three layers, with two plasma polymer layers surrounding a center layer of silver nanoparticles. Within this structure, a biocide reservoir is formed, and the outermost layer releases the ions.
Scientists can tailor the silver concentration as well as the thickness of the layers and their porosity. This allows the silver ions to penetrate the outermost plasma polymer layer over a set period of time. When the silver reservoir is exhausted, no more silver ions are released, thus avoiding any long-term toxic effects.
In trials of finished implants and titanium test samples, the team demonstrated that the DentaPlas coating is not only anti-microbial, but also fully biocompatible and sterilizable. They confirmed the mechanical stability and robustness of the DentaPlas coating in trials using the lower jawbones of pigs taken from butcher shops. Here, they subjected the DentaPlas-coated implants to the rigors of being screwed into place with instruments in modern dental practice.
The DentaPlas coating passed this stress test with no problems. Project partner and Fraunhofer spinoff Bio Gate AG successfully transferred the processes of coating the test samples and titanium screws to its own production facilities. This medical technology company is also the manufacturer of the DentaPlas three-layer coating system.
A demonstration unit of the plasma polymer coating is currently available. Researchers will be presenting a dental implant featuring the DentaPlas coating at the MEDICA trade fair in Düsseldorf from November 16 -19 at the joint Fraunhofer booth (Hall 10, Booth G05).
https://www.fraunhofer.de/en/press/research-news/2015/november/preventing-dental-implant-infections.html
Researchers at the Fraunhofer Institute, Germany, have reportedly developed DentaPlas, an antimicrobial coating for dental implants that consists of three layers, with two plasma polymer layers surrounding a center layer of silver nanoparticles.
Continue reading
Nomination deadline for the 2016 Class of Fellows is fast approaching
November 5, 2015
Source:
The honor of Fellow of the Society was established to provide recognition to members for distinguished contributions in the field of materials science and engineering, and to develop a broadly based forum for technical and professional leaders to serve as advisors to the Society.
If you are interested in nominating someone for this prestigious award, please contact Christine Hoover, for a unique nomination link. This link will be exclusive to you, as the nominator, and will provide you the ability to work through the nomination at different times to add content and attachments until you submit the final nomination.
-
The ASM Fellow Award is first and foremost an award for technical achievement and not intended to exclusively award contributions to ASM International. To the extent possible, the selection committee shall select a diverse slate of nominees from all the constituencies of ASM.
-
Five years of current, continuous membership in ASM International as an individual is required at the time of nomination.
-
Candidates for the award may be proposed by Chapters through their Executive Committee, Affiliate Societies, Regional Councils, Committees/Councils, Award Selection Committee, Awards Policy Committee, ASM Fellow or any five members of the Society.
-
Please be aware that the nominee, and nominator(s), must be current ASM members in good standing, or the nomination will not be accepted. If you have any question regarding the status of membership, please contact me.
-
The nomination is limited to ten pages, plus up to five letters of support for a total of 15 pages (this is in addition to the nomination form).
Please refer to our website to view the rules and lists of past recipients. The deadline for submission is November 30.
The honor of Fellow of the Society was established to provide recognition to members for distinguished contributions in the field of materials science and engineering, and to develop a broadly based forum for technical and professional leaders to serve as advisors to the Society. The deadline for submission is November 30.
Continue reading