EOS expands 3D printing materials with Ti64ELI and StainlessSteel 316L for medical devices
March 20, 2014
Source:
EOS of North America, Novi, Mich., expands its metal materials portfolio with EOS Titanium Ti64ELI and EOS StainlessSteel 316L. The goal is to offer a broader range of titanium and stainless steel materials and open up new fields of application for components fabricated by laser sintering of powder metals. Ti64ELI provides high-detail resolution. StainlessSteel 316L provides high ductility for medical applications such as surgical instruments and orthopedics.
Parts built in EOS Titanium Ti64 have a chemical composition and mechanical properties corresponding to ASTM F136. Providing a high-detail resolution, this alloy can be processed on an EOSINT M 280 (400 Watt) metal laser-sintering system and shows an excellent corrosion resistance. Due to its biocompatibility and high grade of purity it is particularly suited for the additive manufacturing of medical implants.
EOS StainlessSteel 316L has been optimized specifically for processing on the EOSINT M 280 metal laser-sintering system. It shows a good corrosion resistance and a high ductility. Parts built from EOS StainlessSteel 316L have a chemical composition corresponding to ASTM F138 ("Standard Specification for Wrought 18Cr-14Ni-2.5Mo Stainless Steel Bar and Wire for Surgical Implants UNS S31673"). In the medical industry, this alloy is particularly suited for surgical instruments, endoscopic surgery, orthopedics and implants.
The material is also a good choice for use in the watch and jewelry industries, where the designer benefits from extensive freedom of design. Shaping and structural restrictions as such are a thing of the past. Parts such as watch cases (thanks to defined hollow spaces) can be manufactured more cost-efficiently and easily, saving resources. The material is also well suited for additive manufacturing applications such as spectacle frames or functional elements in yachts. In the aerospace industry, EOS StainlessSteel is a good choice for the manufacture of clamping elements or heat exchangers. Parts manufactured from that material can be mechanically post-processed or polished.
www.eos.info

EOS of North America, Novi, Mich., expands its metal materials portfolio with EOS Titanium Ti64ELI and EOS StainlessSteel 316L.
Continue reading
Basque Research studies effects of short, fast, cryogenic cycles on steel
Source:
Basque Research, Spain, has been developing cryogenic treatments for steel in a program that has the goal of understanding both the microstructural changes and the mechanisms that cause them when steel is cooled to cryogenic temperatures below −153°C. One process currently being explored is a multi-phase cryogenic treatment based on the repetition of short, fast, cryogenic cycles.
It allows processing time to be considerably reduced, which enables energy consumption and costs to be cut. The results achieved with this type of process are said to be better than those achieved by conventional cryogenic treatments. Researchers are also exploring the application of cryogenic treatment between hardening and tempering.
Conventional cryogenic treatment consists of slowly cooling the material to about −180 ºC, keeping it at that temperature for a long period of time, and then reheating it to ambient temperature. The fact that it takes so long is a clear problem.
http://www.basqueresearch.com
Basque Research, Spain, has been developing cryogenic treatments for steel in a program based on the repetition of short, fast, cryogenic cycles.
Continue reading
QuesTek to serve as research partner for lightweight materials innovation institute
March 11, 2014
Source:
QuesTek Innovations, Evanston, Ill., announces that it has been selected as a research partner by the U.S. Department of Defense under the Lightweight and Modern Metals Manufacturing Innovation (LM3I) solicitation. It is led by the collaboration between the Edison Welding Institute, the University of Michigan, and the Ohio State University. This institute brings together the collaborative partnership of the federal government and a Detroit-based consortium of more than 50 universities, non-profits, and companies from around the country, including QuesTek Innovations LLC as a research partner.
The effort addresses a critical need for affordable and high-performance lightweight metals, as well as advances in their associated design and manufacturing processes, that will benefit large sectors of the U.S. economy such as metal production, casting, and metalworking.
QuesTek's Chief Science Officer, Dr. Gregory B. Olson, will serve as the leader of "Novel Materials," one of 15 key technology development pillars that bring together experts within the respective fields. Dr. Jason Sebastian, QuesTek's Manager of Technology and Product Development, will serve as one of seven experts in the technology development area of Integrated Computational Materials Engineering (ICME). QuesTek's unique role and expertise will contribute to the innovative "ecosystem" that draws together the full spectrum of capabilities and spans the entire value chain of lightweight manufacturing.
QuesTek has been developing new breakthrough alloys since 1997 using ICME methodologies and its Materials by Design technology. Four QuesTek high performance steels (Ferrium M54, Ferrium S53, Ferrium C61 and Ferrium C64 steels) were successfully developed and licensed to Carpenter Technology. These Ferrium steels are displacing materials that have been used for decades in demanding applications such as aircraft landing gear, arresting hook shanks and hook points; and helicopter power transmission gears and rotor shafts. The steels also serve oil and gas applications and other industries. In addition, novel alloys based on Al, Ni, Co, Cu, Mo are being designed and developed by QuesTek, based on ICME ensuring successful design and accelerated implementation.
Other members of ALMMII with whom QuesTek will be closely collaborating include Northwestern University, Thermo-Calc, Boeing Company, General Electric, and Lockheed Martin.
www.questek.com
QuesTek Innovations, Evanston, Ill., announces that it has been selected as a research partner by the U.S. Department of Defense under the Lightweight and Modern Metals Manufacturing Innovation (LM3I) solicitation.
Continue reading
Ambrell induction heating equipment enables fast repeatable heating for aerospace manufacturers
Source:
Ambrell, an Ameritherm Company, Scottsville, N.Y., designs fast, repeatable, controllable, noncontact heating equipment with a minimal footprint that makes it an ideal solution for aerospace manufacturers. Induction heating is used for decarburization, brazing, and preheating, among other applications, during the manufacture of fasteners, turbine blades, and much more. It provides the ability to increase production and boost quality within the aerospace industry.
Additionally, Ambrell offers monitoring and logging of temperature and other key operating parameters via eView induction heating software. This software often helps suppliers to meet aerospace manufacturer specifications for parts. One such example is numerous aerospace fastener suppliers using eVIEW to meet data logging requirements.
Ambrell also offers free application testing in its Applications Lab. From the testing, engineeers determine the optimal system for the client's application, accounting for their parts and required heating time. Systems from 1 kW to over 1 MW enable a solution whether the application is large or small.
Ambrell will be exhibiting and demonstrating its induction heating solutions for aerospace at MFG4 in Hartford, Conn., May 6-8 in booth 1208.
www.ambrell.com
Ambrell, an Ameritherm Company, Scottsville, N.Y., designs fast, repeatable, controllable, noncontact heating equipment with a minimal footprint that makes it an ideal solution for aerospace manufacturers.
Continue reading
Aviation seating to be made of magnesium for the first time
Source:
Magnesium Elektron, England, announces the first use of its proprietary Elektro 43 alloy in aviation seating. Zim Flugsitz GmbH, a German manufacturer of seating for the aerospace industry, is now producing seats with major structural components made from Elektron 43. The new seats will provide a significant weight reduction compared to aluminum alloys, while retaining strength and ductility. The first new seats are scheduled to enter service later in 2014 in a low-volume non-commercial aviation platform.
"The use of our Elektron 43 magnesium alloy has enabled Zim Flugsitz to surpass their weight-reduction targets and improve the fuel efficiency and endurance in this new application," says Steve Montisci, European Technical Sales Manager, Wrought Products. "This project is an important step and will demonstrate the benefits that Elektron magnesium alloys can bring to future lightweighting strategies for commercial aircraft designers and operators."
Magnesium Elektron alloys have been widely used in military aircraft for many years, as well as in critical engine components for civil aircraft. During the past decade, Magnesium Elektron has been working with regulatory agencies, aircraft manufacturers, and seat manufacturers around the world to gain acceptance for magnesium in civil aircraft interiors, including changing provisions of SAE standard AS8049 so that magnesium can be approved for commercial aircraft with 20 seats or more.
In June 2013, the Federal Aviation Administration (FAA) announced: "With the results of the Magnesium Full Scale Testing and the progress demonstrated in the development of the lab scale test method, the FAA would now allow magnesium in aircraft seats, providing the requirements and conditions as set out in the Special Conditions are satisfied."
The FAA, European Aviation Safety Agency (EASA) and the aircraft industry continue their work to finalize the framework of the Special Conditions route for commercial aircraft applications.
www.magnesium-elektron.com
Magnesium Elektron, England, announces the first use of its proprietary Elektro 43 alloy in aviation seating.
Continue reading
Harper wins contracts worth $38 million for carbon fiber production systems
March 10, 2014
Source:
Harper International, Buffalo, N.Y., has been awarded contracts worth $38 million for advanced three meter wide oxidation ovens, LT and HT carbonization systems, waste gas abatement systems, fiber handling, and integrated additional unit operations, controls, and services. Harper's proprietary atmospheric seals reduce fugitive emissions, increase the active volume of the oven, and offer reduced energy consumption over alternatives.
For the customer, this and other technology advancements equal optimized fiber quality and production rates due to faster oxidation, improved velocity uniformity and range capability, assured temperature uniformity, and optimal control of the reaction.
"Harper's cutting-edge technology combined with our respected Pulse service program provides customers with the most secure path to success in Carbon Fiber production," says Charles Miller, President at Harper. "We strive to be identified as offering the most superior technology on the market for a range of fiber precursors, from research scale Microlines, to the largest scale production plants in the industry."
www.harperintl.com
Harper International, Buffalo, N.Y., has been awarded contracts worth $38 million for advanced three meter wide oxidation ovens, LT and HT carbonization systems, waste gas abatement systems, fiber handling, and integrated additional unit operations, controls, and services.
Continue reading
Easier access to journal content for member subscribers
March 7, 2014
Source:
Now with the new ASM website accessing your ASM journal subscriptions is easier than ever. Now you need less clicks to access your content. Follow the new instructions below.
Instructions for ASM members to access journal content:
-
Login to the ASM website at www.asminternational.org.
-
Click on the "My Subscriptions" tab in the left navigation pane.
-
Select the name of the journal (in blue) you wish to access. This will take you to the journal page on Springer. If you have subscriptions to other ASM content in addition to journals, such as the member magazine, Advanced Materials and Processes, and the ASM Desk Editions Online, you will see those listed on this page as well.
-
-
If you are already logged into the ASM site and on another page, you can access the subscription page by clicking on "Welcome" and your name at the top of the screen, or by clicking on "My ASM."
-
Troubleshooting
If you have recently been to the Springer site other than through the ASM website, it may remember you as a non-subscriber and indicate that access is not available or ask you to log in or pay for access.
If that happens, you may need to clear out the cookies and temporary history files on your computer and close your internet connection. When you go back in through the ASM site, it should recognize you as a subscriber.
Now with the new ASM website accessing your ASM journal subscriptions is easier than ever. Now you need less clicks to access your content.
Continue reading
ThyssenKrupp completes sale of Alabama rolling/coating plant
March 5, 2014
Source:
ThyssenKrupp Steel USA, Alpharetta, Ga., has completed the sale of its rolling and coating plant in Calvert, Ala., to a consortium of ArcelorMittal and Nippon Steel & Sumitomo Metal Corp. Upon closing, ThyssenKrupp received a purchase price of $1.55 billion from the consortium.
At the same time a valuable long-term slab supply contract has been agreed upon that will provide a sustainable solution for the ThyssenKrupp CSA steel mill in Brazil. The consortium will purchase two million tons of slabs per year from ThyssenKrupp CSA through 2019. The agreement will reliably secure a minimum 40% capacity utilization of the plant for several years. In addition, stronger penetration of the slab markets in South and North America will further increase ThyssenKrupp CSA's capacity utilization.
The combination of the sale and the slab supply contract will help ThyssenKrupp improve its cash flow profile and key financials in the future.
http://www.thyssenkrupp.com/
ThyssenKrupp Steel USA, Alpharetta, Ga., has completed the sale of its rolling and coating plant in Calvert, Ala., to a consortium of ArcelorMittal and Nippon Steel & Sumitomo Metal Corp.
Continue reading
Tecnalia achieves NadCap accreditation for testing and surface treatments
Source:
Tecnalia Research & Innovation, Spain, has received Nadcap accreditation, which recognizes the company´s technical competence as a testing laboratory for control of surface treatment baths and also as testing on metal materials – mechanical, metallography and corrosion testing – in the aeronautical sector.
Nadcap accreditations constitute an international recognition of technical competence and reliability to provide products and services in the aeronautical sector.
This accreditation is granted by the Performance Review Institute (PRI), a worldwide organization comprising the main aircraft manufacturers: Airbus, Boeing, Bombardier, GE Aviation. The main objective is to develop programs and services designed to improve product manufacturing processes and quality processes in the aeronautical sector.
The PRI guarantees the unbiased assessment of these products and services, ensuring that the suppliers of the aeronautics sector can meet the complex requirements of their customers.
Although Tecnalia already has Airbus authorization, it is now an internationally recognized, independent and impartial organization.
Tecnalia´s technological services in the aerospace sector, in which it has been working for the last 20 years, comprise characterization of materials, nondestructive testing (NDT), failure analysis, materials assessment and diagnosis, welding processes, and comprehensive outsourcing of calibration.
"The NadCap accreditation is an important step in our strategy for specialization within the business of materials characterization and in generating new business opportunities for our clients," said Jose Miguel Iturrioz, Head of Tecnalia's Materials Services Area.
http://www.basqueresearch.com/berria_irakurri.asp?Berri_Kod=4941&hizk=I
Tecnalia Research & Innovation, Spain, has received Nadcap accreditation, which recognizes the company´s technical competence as a testing laboratory for control of surface treatment baths and also as testing on metal materials – mechanical, metallography and corrosion testing – in the aeronautical sector.
Continue reading
Instron motorized pendulum impact testers measure 300 to 900 joules to Charpy and Izod standards
Source:
Instron, Norwood, Mass., offers the MPX Series of motorized pendulum impact testers for metals impact testing to Charpy and Izod standards. The MPX Series offers a range of testing capabilities from 300 to 900 Joules. The testers come standard with Fracta Software, which allows for reliable data acquisition and reporting of absorbed energy. If more advanced impact analysis and reporting are needed, upgrading to Impulse Data Acquisition Software and instrumentation will allow for direct measurement of impact force and striker velocity.
The MPX is designed with an automatic test start as soon as the door closes, allowing for rapid testing and improved throughput while conforming to the international standards for non-ambient testing. The feature fully complies with NIST 5-second guidelines, specifiying the time it should take for the specimen to leave the temperature conditioner and for the test to be complete.
Most other pendulum impact testers on the market still require the hammer assembly to be completely removed in order to change weights. On the MPX, interchangeable hammer weights allow for quick and simple adjustment of the impact energy, removing the need for the time-consuming process of changing hammer shafts.
The MPX features an integrated guard and safety control system that meets the stringent requirements for the European CE mark and for ISO 13849. The operator is protected at all times during machine operation.
www.instron.com
Instron, Norwood, Mass., offers the MPX Series of motorized pendulum impact testers for metals impact testing to Charpy and Izod standards.
Continue reading