Aluminum products producer Aleris acquires sheet producer Nichols Aluminum

February 12, 2014
Source:

Aleris, Cleveland, Ohio, has signed a definitive agreement to acquire Nichols Aluminum, LLC, a wholly owned subsidiary of Quanex Building Products Corp. Nichols is a leading producer of aluminum sheet for the transportation, building and construction, machinery and equipment, consumer durables, and electrical industries in North America. The acquisition includes two production facilities in Davenport, Iowa; a facility in Decatur, Alabama; and a facility in Lincolnshire, Illinois.  The company has agreed to pay $110 Million in an all-cash transaction.

"Nichols has a long history of producing flat-rolled aluminum sheet products for customers in a number of key industries across North America and we look forward to continuing that long-standing tradition,"  says Steve Demetriou, Aleris chairman and CEO. "This acquisition is consistent with our strategy to expand our footprint and enhance our capabilities to ensure we are well-positioned to respond to projected growth in our key end uses as the economy begins to recover."

Upon the close of the transaction, Nichols will become part of Aleris' Rolled Products North America business, adding more than 500 Nichols employees to the Aleris team.

Aleris is a privately held, global leader in aluminum rolled products and extrusions, aluminum recycling and specification alloy production. Headquartered in Cleveland, Ohio, Aleris operates approximately 40 production facilities in North America, Europe, and Asia.

www.aleris.com

Aluminum products producer Aleris acquires sheet producer Nichols Aluminum

Aleris, Cleveland, Ohio, has signed a definitive agreement to acquire Nichols Aluminum, LLC, a wholly owned subsidiary of Quanex Building Products Corp.

Continue reading

Missile canard for use in EAPS test flight

January 3, 2014
Source:

Liquidmetal Technologies Inc., Rancho Santa Margarita, Calif., delivered missile canards that are being fitted for a future test of Lockheed Martin's (Bethesda, Md.) EAPS (Extended Area Protection and Survivability) missile, an advanced performance, highly affordable hit-to-kill missile interceptor designed to defeat rocket, artillery, and mortar (RAM) targets with significantly reduced probabilities for collateral damage.

Working in collaboration with Lockheed Martin's advanced design team, Liquidmetal's unique alloy and process methods yield parts with dimensional consistency and precision at an affordable cost. Canards made from the new alloy meet the close geometric tolerances required for supersonic flight. The parts consistently meet tolerances and the shape and weight of each part is nearly identical, which is desirable for this application. The parts also have greater strength to weight than steel or titanium. Once the design is finalized, parts can be produced in high volumes with short lead times.

"Lockheed Martin has been an ideal development partner for this breakthrough application for Liquidmetal Technologies, creating a high precision, high performance part at a lower cost," said Bruce Bromage, EVP of Business Development with Liquidmetal Technologies.

More information:

Liquidmetal Technologies

Lockheed Martin

 

 

Missile canard for use in EAPS test flight

Liquidmetal Technologies Inc., Rancho Santa Margarita, Calif., delivered missile canards that are being fitted for a future test of Lockheed Martin’s (Bethesda, Md.) EAPS (Extended Area Protection and Survivability) missile.

Continue reading