Wisconsin Oven delivers two-zone belt conveyor oven for steel tempering

February 5, 2025
Source: ASM International

Wisconsin Oven delivers two-zone belt conveyor oven for steel tempering

Wisconsin Oven Corporation, East Troy, WI, announced the shipment of a two-zone belt conveyor oven designed for tempering steel parts following induction hardening. The system is engineered for precise temperature control and enhanced energy efficiency, meeting industry specifications for uniform heating.

The oven has the capacity to heat 2,400 pounds of steel per hour from 70°F to 350°F, with a maximum temperature rating of 500°F. It features a top-down airflow recirculation system with a 32,000 CFM blower, evenly distributed between the two heating zones. Temperature control is managed by a Watlow F4T digital recorder/controller, which includes Ethernet communication capabilities and adaptive PID temperature control. A temperature uniformity survey verified uniformity within ±10°F at 350°F, ensuring compliance with AIAG specification CQI-9.

The conveyor system utilizes a continuous belt with a variable frequency drive for speed adjustments, and the work zone measures 4’0” W x 21’0” L x 14” H. To improve energy efficiency, the oven is equipped with the E-Pack™ Energy Efficiency Package, which includes additional insulation and variable frequency drives on the recirculation blowers. These features reduce energy consumption and operational costs, potentially providing substantial annual savings depending on utility rates and operating conditions.

The system’s design optimizes heat-up efficiency and uniformity, making it well-suited for high-volume steel tempering applications. The oven incorporates programmable temperature controls with auto-tuning functionality, ensuring consistent and repeatable performance for industrial heat treatment processes.

Read further here.

Seco/Warwick to supply Jetcaster technology to Turkish aviation company

November 30, 2024
Source: ASM International

Seco/Warwick to supply Jetcaster technology to Turkish aviation company

Seco/Warwick, Meadville, Pa, announced that it will deliver a JetCaster induction vacuum furnace to a Turkish aviation company. The advanced furnace is designed for producing castings using directional solidification, single crystal, and equiaxed structure methods, as well as gas-cooled crystallization. The technology addresses the precision and quality requirements of aviation component manufacturing.

The JetCaster VIM50 DS/SC/EQ furnace, with a maximum load capacity of 50 kilograms, supports various crystallization techniques, offering flexibility and high performance. Its innovative Engineered Gas Cooling (DGCC) system shortens processing times while maintaining superior product quality, making it particularly suited to the stringent demands of the aviation sector.

Seco/Warwick’s CEO, Sławomir Woźniak, highlighted the increasing demand for the company’s vacuum metallurgy solutions within the aviation industry, noting its critical role in producing components for both civil and military aircraft. He emphasized the company’s collaboration with leading corporations globally to meet the sector’s high-quality standards.

This marks the first order of a melting furnace from this specific partner. Seco/Warwick customized the furnace design to accommodate future modifications, such as the addition of feeders for bulk materials or briquettes, ensuring adaptability to evolving production needs. The solution aims to enhance the partner’s production efficiency and innovation, solidifying its contribution to the aviation industry.