One MInute Mentor: X-Ray Diffraction Patterns in AISI 316

July 20, 2017
Source:

The graph shows X-ray diffraction patterns of nitrided (and carburized) stainless steel AISI 316. Carburizing was carried out in 20% CO-80% H2 gas atmosphere at 515°C (788 K) for five hours. X-ray diffraction analysis corroborates that the nitrogen content is significantly higher in the sample nitrided at the highest nitriding potential. The 111 Bragg reflections (peaks) are shifted to lower scattering angles, where the largest shift is observed for the highest nitriding potential.

The peak shift is caused primarily by dissolution of nitrogen, leading to a dilation of the fcc lattice; residual stress and stacking faults also contribute. Peaks originating from the unexpanded austenite are visible in the sample nitrided at KN = 0.293, indicating that the γN zone is not as thick as for the samples nitrided at high potentials.

Volume 4D, Heat Treating of Irons and Steels â‡’ Heat Treated High-Alloy Steels ⇒ Low-Temperature Surface Hardening of Stainless Steel ⇒ Gaseous Low-Temperature Surface Hardening of Austenitic Stainless Steel 

One MInute Mentor: X-Ray Diffraction Patterns in AISI 316

The graph shows X-ray diffraction patterns of nitrided (and carburized) stainless steel AISI 316.

Continue reading

Bodycote combines AM with powder metallurgy processes to produce complex parts


Source:

Bodycote, England, introduces Bodycote Powdermet technologies, a group of additive manufacturing processes for the production of complex components via powder metallurgy.

Powdermet technologies incorporate new, patent-pending techniques that combine 3D printing with well-established net-shape and near-net-shape processes. They greatly reduce manufacturing time and production cost compared to 3D printing alone.

Powdermet technologies ensure complete powder consolidation, achieve structural homogeneity, and eliminate internal porosity and unconsolidated powder flaws. The process can produce components with varying surface features and thicknesses, with higher structural integrity than alternative production techniques. The need for brazing or welding parts to form larger structures is eliminated. Instead, the finished article can be produced as one seamless component and largely avoid the size limitations imposed by the constraints of 3D printing.

Different parts of a component can be formed from different alloys, presenting the ideal and most cost-efficient solution. Component design can be tailored to the actual requirements for performance, and not limited by subsequent machining operations.

According to Stephen Harris, Group Chief Executive, "The recent breakthroughs are truly game changing technologies for component design and manufacturing. Industry applications are wide ranging, with early adoption expected in aerospace, oil and gas, power generation, and mining."

Bodycote continues to invest in resources and capital for developments in additive manufacturing technology to create significant value for customers and meet future growth demands. In addition to its Powdermet technologies, Bodycote provides a full range of heat treatment, hot isostatic pressing, and electrical discharge machining services across North America and Europe, tailored specifically to support the needs of companies manufacturing metal components by 3D printing.

www.bodycote.com

 

Bodycote combines AM with powder metallurgy processes to produce complex parts

Bodycote, England, introduces Bodycote Powdermet technologies, a group of additive manufacturing processes for the production of complex components via powder metallurgy.

Continue reading

United Process Controls upgrades heat treating systems controls for axle manufacturer


Source:

United Process Controls Inc., Bethlehem, Pa., is nearing the completion of a large, multi-year control systems upgrade project for a manufacturer of automotive axles. Planning and executing the phased migration started in 2014 and encompassed four Ipsen pusher furnaces, four Ipsen batch IQ furnaces, four parts washers, three temper furnaces, one preheat oven, four endo generators, and a SCADA system.

Given the number of furnaces, as well as secondary and auxiliary equipment, a key parameter of the upgrade project was the seamless switchover and deployment of new control systems without interruption or shutdown of production. Another requisite was to get more flexibility from the new controls to improve operational efficiency, traceability, preventive maintenance, and production throughput. 

The solution from UPC included Protherm 700 controllers with new PLCs and Waukee Valve-Tronic Plus flow controllers on the furnaces, Protherm 470 controllers on the parts washers, and an AccuBlendor Plus endothermic generator control system supporting all furnaces. Furnaces were similarly outfitted with a number of sensors capable of generating volumes of data that are processed through the Protherm diagnostic tools, giving managers, operators, and maintenance techs the power to troubleshoot equipment as well as predict anomalies in the process. The use of redundant probes along with resident SAT thermocouples has dramatically increased equipment reliability and virtually eliminated scrap and/or rework. 

The customer also implemented the Protherm 9800 platform to enable total data management, as well as remote control and diagnostics of the furnaces. In addition to its data management capabilities, the Protherm 9800 provides real-time data logging and storage functions that conform to CQI-9 requirements. In a future implementation, an add-on module will allow the company's personnel to preplan and route batches for processing within the production cell. 

www.group-upc.com

 

 

United Process Controls upgrades heat treating systems controls for axle manufacturer

United Process Controls Inc., Bethlehem, Pa., is nearing the completion of a large, multi-year control systems upgrade project for a manufacturer of automotive axles.

Continue reading

Alcoa to restart three potlines in Indiana to supply Warrick aluminum rolling mill


Source:

Alcoa Corp., Pittsburgh, announces plans to restart three of five potlines at its Warrick Operations aluminum smelter near Evansville, Indiana, an action that will further improve the competitiveness of the on-site rolling mill.

The process to restart the three lines, with 161,400 metric tons of annual capacity, will begin immediately and is expected to be complete in the second quarter of 2018. The three potlines will directly supply the Warrick rolling mill, which serves the North American market with flat-rolled aluminum for the food and beverage can packaging industry. The smelter's molten metal will supplement purchased scrap metal and other raw materials that the Warrick site will continue to procure.

"By restarting a portion of the Warrick smelter, we will provide an efficient source of metal for the co-located rolling mill and help it meet an anticipated increase in production volumes," said Tim Reyes, President of Alcoa's Aluminum business unit. "The action will enable us to more fully utilize the assets at this integrated site."

The smelter at Warrick closed in March of 2016. Two of the five smelting potlines will be classified as curtailed capacity and will remain idle. After this partial restart, Alcoa will have approximately 886,000 metric tons idled of its total smelting capacity of 3.4 million metric tons.

Alcoa Warrick Operations is comprised of the smelter and the rolling operations, which includes state-of-the-art casting, hot and cold rolling, slitting and coating capabilities. The operations also include the power supply for the smelter and rolling operations, consisting of a coal mine that fuels four generating units with a combined net capacity of about 750 megawatts. Three of those units are wholly-owned by Alcoa Power Generating Inc. A fourth unit, Warrick Unit 4, with 300 megawatts of net capacity, is owned in a 50-50 partnership with Vectren, a utility headquartered in Evansville.

www.alcoa.com

 

Alcoa to restart three potlines in Indiana to supply Warrick aluminum rolling mill

Alcoa Corp., Pittsburgh, announces plans to restart three of five potlines at its Warrick Operations aluminum smelter near Evansville, Indiana, an action that will further improve the competitiveness of the on-site rolling mill.

Continue reading

NASA grants $10M to cut supersonic aircraft sonic booms by shape-memory-alloy morphing

July 14, 2017
Source: ASM International

NASA grants $10M to cut supersonic aircraft sonic booms by shape-memory-alloy morphing

The National Aeronautics and Space Administration, Washington, announces that it has granted $10 million to a CASMART industry-academic team that will lead research into designing commercially viable civil supersonic transport aircraft that can modify shape during flight under a range of conditions to meet noise and efficiency requirements for overland flight.

Continue reading

U.S. Steel Corp. finalizes sale of U.S. Steel Canada to Bedrock Industries

July 12, 2017
Source:

United States Steel Corp., Pittsburgh, announces that it has finalized an agreement with Bedrock Industries Group LLC, New York, for the sale and transition of ownership of U.S. Steel Canada Inc. to Bedrock. The transaction was finalized following requisite court and other approvals. 

In connection with the closing, U.S. Steel received approximately $127 million in satisfaction of its secured claims, including interest, and unsecured claims. The terms of the plan and closing also included an agreement to provide mutual releases among key stakeholders, as well as a release of all claims against U.S. Steel regarding environmental, pension, and other liabilities. 

As part of the transition in ownership, U.S. Steel will continue to provide certain transition services to USS Canada, and entered an agreement to supply USS Canada with all of its requirements for iron ore pellets through January 31, 2022. 

United States Steel  is a leading integrated steel producer and Fortune 300 company with major production operations in the United States and Central Europe. The company manufactures a wide range of value-added steel sheet and tubular products.

Bedrock Industries is a privately funded holding company focused on owning and operating metals, mining, and natural resources assets and related special situations. 

http://www.ussteel.com

www.bi15.com

 

U.S. Steel Corp. finalizes sale of U.S. Steel Canada to Bedrock Industries

United States Steel Corp., Pittsburgh, announces that it has finalized an agreement with Bedrock Industries Group LLC, New York, for the sale and transition of ownership of U.S. Steel Canada Inc. to Bedrock.

Continue reading

Oxford Instruments Industrial Analysis business joins Hitachi to form new company


Source:

Oxford Instruments, England, announces that its Industrial Analysis business will join Japan's Hitachi High-Technologies to form a new company, Hitachi High-Tech Analytical Science. The new company brings together Hitachi High-Technologies' extensive scientific instrumentation portfolio with Oxford Instruments' 40-year heritage of innovative analytical instruments and services developed in close partnership with industry customers. The collaboration will provide a wider-ranging product portfolio, more contact points with customers, and more opportunities to meet customer needs.

Hitachi High-Tech Analytical Science is a new global company created in July 2017 within the Hitachi High Technologies Group. The company is headquartered in Oxford, England, with research and development and assembly operations in Finland, Germany,  and China, with sales and support operations in a number of countries around the world.

Hitachi High-Tech Analytical Science will continue to specialize in delivering high-tech analysis solutions, developed in close collaboration with industry customers and designed to meet the tough challenges of a rapidly evolving industrial sector.  Its range of laboratory-based and robust high-performance field testing instruments deliver materials and coatings analyses that add value throughout the production lifecycle.

http://www.hitachi-hightech.com/hha/

 

Oxford Instruments Industrial Analysis business joins Hitachi to form new company

Oxford Instruments, England, announces that its Industrial Analysis business will join Japan’s Hitachi High-Technologies to form a new company, Hitachi High-Tech Analytical Science.

Continue reading

Molten aluminum poured over 3D-printed steel lattice multiplies damage tolerance


Source:

Oak Ridge National Laboratory, Tenn., and Rice University, Houston, report that a new manufacturing method developed by Oak Ridge and Rice combines 3D printing with traditional casting to produce damage-tolerant components composed of multiple materials. Engineers discovered that by pouring molten aluminum over a 3D printed steel lattice, the damage tolerance of the part increases by an order of magnitude over aluminum.

The process, published in  Materials and Design, was developed for potential automotive and other applications for which thermal and mechanical properties must be optimized simultaneously.

"This scalable processing strategy can be used to fulfill specific component functions, giving materials designers unprecedented control over both microstructure and material properties," says ORNL's Amit Shyam.

www.ornl.gov

 

Molten aluminum poured over 3D-printed steel lattice multiplies damage tolerance

Oak Ridge National Laboratory, Tenn., and Rice University, Houston, report that a new manufacturing method developed by Oak Ridge and Rice combines 3D printing with traditional casting to produce damage-tolerant components composed of multiple materials.

Continue reading

One Minute Mentor: Nitrogen-Expanded Austenite

July 7, 2017
Source:

The graph shows hardness-depth profiles of nitrided AISI 316. A profile for carburizing is shown for comparison.

Lines obtained by fitting a sigmoidal function are given to guide the eye. The hardness values measured directly at the surface (with the same load) were 1585 HV for KN = 2.49;  and 1417 HV for KN= 0.293.

The effect of the nitriding potential is also reflected in the hardness-depth profiles. A smooth decrease near the surface is  followed by a sharp drop at a position close to the transition from γN to γ. Nitrogen-expanded austenite is very hard, and the transition from the hardened case to the (soft) core occurs within a few microns.

Volume 4D, Heat Treating of Irons and Steels â‡’ Heat Treated High-Alloy Steels ⇒ Low-Temperature Surface Hardening of Stainless Steel ⇒ Gaseous Low-Temperature Surface Hardening of Austenitic Stainless Steel 

One Minute Mentor: Nitrogen-Expanded Austenite

The graph shows hardness-depth profiles of nitrided AISI 316. A profile for carburizing is shown for comparison.