EWI additive manufacturing projects include alloys, powders, processes, testing

June 17, 2019
Source:

Edison Welding Institute (EWI), Columbus, Ohio, announces that its Additive Manufacturing Consortium (AMC) research projects for 2019 include studies of Inconel 625 and 718, powder measurement techniques, surface finishing, and more.

 

AMC member companies pool their membership fees to conduct pre-competitive research on high interest topics chosen by its members. In addition to receiving millions of dollars of research data each year, they are also able to take part in quarterly AMC meetings, learn directly from experts, and network with professionals who face similar challenges.

 

Projects for 2019:

--Study of Inconel 625 & 718 with a focus of looking at the creep and fatigue resistance of the parts

--Comparison of the various powder measurement techniques to identify what technology provides the best comparable data for a specific type of powder

--Exploration of the best parameters to use in Laser Power Bed Fusion (L-PBF) system for specific complex features (ie: bridges or thin walls)

--Evaluation of all of the melt pool monitoring systems on the market and comparing the results from each

--Examination NDE techniques work to see which are best for complex AM printed part geometries

--Study of surface finishing techniques, focusing on how they improve fatigue resistance

--Comparison of “new” AM technologies and existing AM processes.

 

www.ewi.org

 

EWI additive manufacturing projects include alloys, powders, processes, testing

Edison Welding Institute (EWI), Columbus, Ohio, announces that its Additive Manufacturing Consortium (AMC) research projects for 2019 include studies of Inconel 625 and 718, powder measurement techniques, surface finishing, and more.

Continue reading

Seco Warwick introduces new integral quench furnace and gas quench system

June 13, 2019
Source:

Seco Warwick, Meadville, Pa., introduces its Super IQ integral quench furnace and UCM 4D Quench system.

 

The Super IQ (integral or sealed quench furnace), offers all of the benefits of low pressure carburizing and vacuum hardening, with none of the added costs. The system combines clean processing with the exceptional performance of oil quenching in the industry’s most innovative integral quench furnace design in decades. With a Super IQ, users get super clean parts while still getting the benefit of a simple atmosphere oil quench.

 

The UCM 4D Quench enables customers with gas quenchable materials to replace oil quenching with an environmentally friendly, cost-effective technology. It provides a solution that eliminates the need for press quenching systems and the problems associated with their operation. First, no more finishing treatment is needed to remove the oxidized layer. Second, it provides parts with higher surface quality and savings due to eliminating the need for heat treatment fixtures and material logistics. Third, it eliminates oil and oil vapor contamination, ensuring personnel safety and reduced environmental impact in addition to eliminating washers and chemicals.

 

www.secowarwick.com

 

 

Seco Warwick introduces new integral quench furnace and gas quench system

Seco Warwick, Meadville, Pa., introduces its Super IQ integral quench furnace and UCM 4D Quench system.

Continue reading

Solar Atmospheres 14-foot car-bottom air furnace can treat loads up to 30,000 pounds


Source:

Solar Atmospheres of Western PA, Hermitage, recently installed a 14-foot long car bottom air furnace for the tempering of large tool steel components, as well as the age hardening processes of nickel-based alloys and precipitation hardenable stainless steels.

 

The furnace was surveyed in accordance with AMS2750 Rev E and is uniform within ±10°F (Class 2). With a working zone measuring 60 x 54 x 168 inches, the furnace is capable of handling workloads up to 30,000 pounds and feataures maximum operating temperature of 1400°F.

 

According to Bob Hill, President of Solar Atmospheres of Western PA, “This new air tempering furnace will be a good complement its larger counterpart, a recently installed 20-foot car bottom furnace. Expanding our large air furnace capability will enhance the turnaround for our ’raw material’ customers, and is more cost-effective than processing in a vacuum environment.”

 

www.solaratm.com

 

Solar Atmospheres 14-foot car-bottom air furnace can treat loads up to 30,000 pounds

Solar Atmospheres of Western PA, Hermitage, recently installed a 14-foot long car bottom air furnace for the tempering of large tool steel components, as well as the age hardening processes of nickel-based alloys and precipitation hardenable stainless steels.

Continue reading

One Minute Mentor: Martensitic heat treating

June 12, 2019
Source:

The graph shows the tempering response of hardened 52100 bearing steel. In North America, the 1C-1.5Cr through-hardening steel was given the designation of 52100. One of the main reasons this steel became popular as a bearing steel is its consistent response to salt-bath and furnace heat treatment and oil quenching (assuming the incoming raw material conditions met hardness, microstructure, and grain size specifications).

 

The standard heat treating cycle for martensitic hardening of 52100 bearing steel is:

Austenitize 815–855C (1500–1570F) 15–40 min + 30 min for each additional inch of thickness, endo or neutral atm with 0.9–1 C potential;

 

Quench ≤150C (300F) agitated oil (martensitic hardening); ≥230C (445F) molten salt (bainitic hardening)

Temper 150–230C (300–445F) 2–4 h (58–64 HRC).

 

As-quenched hardness after heat treating is typically 64–67 HRC. Figure 1 shows hardness as a function of tempering temperature.

 

The goal of tempering 52100 bearing steel is to achieve a measure of toughness in the steel while maintaining high as-tempered hardness. A bearing must have a minimum hardness of 58 HRC to achieve the expected rolling contact fatigue performance in service. This requirement dictates a maximum tempering temperature of 260°C (500°F).

 

Another goal of tempering bearing steels is to achieve the required level of dimensional stability as described in specification DIN-623. This topic is discussed more thoroughly in an upcoming section.

 

For more information, click on the link below (subscription required), then scroll down the Chapter Contents on the left of the page, and click on Martensitic Heat Treating.

 

https://dl.asminternational.org/handbooks/book/9/chapter/110017/Heat-Treatment-of-Bearings

 

One Minute Mentor: Martensitic heat treating

The graph shows the tempering response of hardened 52100 bearing steel.

Continue reading

ITSC 2019 presentation: Solid-State Additive Manufacturing

June 11, 2019
Source:

Inovati, Santa Barbara, Calif., presented a discussion about the application of its impact consolidation Kinetic Metallization (KM) process to an advanced and superior 3D manufacturing technology.

When integrated with CAD/CAM, Inovati characterizes this new technology as Solid-State Additive Manufacturing (SSAM). This innovative spray deposition process provides unique opportunities for development of a 3D fabrication technique with material properties not currently feasible with conventional fusion-based AM processes.

 In particular, the low temperature attribute of the process enables fabrication of metallic and composite parts with metallurgically uniform properties, while fusion-based processes tend to be unstable or degrade at high melting temperatures. The SSAM deposition rates associated with Kinetic Metallization permit an order of magnitude faster fabrication rate of parts when compared to many conventional AM methods. The paper presented the developments of the technology to date and the potential applications.

Dr. Ralph Tapphorn , Mr. Howard Gabel , Mr. Travis Crowe , Inovati, Santa Barbara, California

www.inovati.com

ITSC 2019 presentation: Solid-State Additive Manufacturing

Inovati, Santa Barbara, Calif., presented a discussion about the application of its impact consolidation Kinetic Metallization (KM) process to an advanced and superior 3D manufacturing technology.

Continue reading

Sintavia opens additive manufacturing facility for large-scale aerospace production


Source:

Sintavia LLC, Hollywood, Fla., has opened the doors to its new 55,000-square-foot advanced manufacturing facility, which is said to be the first of its kind in North America to offer large-scale AM production coupled with a robust aerospace quality management system.

 

The facility houses over $25 million of advanced manufacturing equipment, including medium and large scale metal printers, EDMs, post-processing machines, wet-booths, and multiple furnaces. Some of the industrial engineering improvements of the building include separate manufacturing rooms segregated by alloy, a large-scale powder management system, an uninterruptable power supply, an inert gas farm, and a final production acceptance quality-control room.

 

The new facility is capable of producing tens of thousands of parts representing in excess of $100mm of AM revenue annually. The expansion is anticipated to bring more than 130 new jobs for skilled employees and support staff to South Florida.

 

“As we grow, it will serve as a template for future vertically aligned advanced manufacturing facilities around the United Staets and the world,” said Brian Neff, Sintavia’s Chairman and Chief Executive Officer.

 

The grand opening was attended by over 150 customers and industry partners, including Sumitomo Corporation, a growth equity investment partner of Sintavia and one of the largest international trading companies in the world. “Sintavia has again proven itself as a leader in the industrialization of AM production,” said Mr. Masaki Nakajima, CEO and President of Sumitomo Corporation of Americas.

 

www.Sintavia.com

Sintavia opens additive manufacturing facility for large-scale aerospace production

Sintavia LLC, Hollywood, Fla., has opened the doors to its new 55,000-square-foot advanced manufacturing facility, which is said to be the first of its kind in North America to offer large-scale AM production coupled with a robust aerospace quality management system.

Continue reading

Keyence VHX 7000 digital microscope features expanded memory, one-click focus

June 10, 2019
Source:

Keyence, Itasca, Ill., introduces the VHX-7000 Series digital microscope, the first model to feature the Focus View function, which enables simultaneous viewing of the lens and the target. Thanks to the intuitive software interface, focusing can be carried out easily with just a click.

 

Even when the target has an uneven surface, a fully-focused image is obtained instantly, composed of multiple images with varying focus positions. Additionally, 3D display can be used to observe surface contours.

 

The Auto-Measurement Teaching function enables repeated measurements to be made automatically on identically-shaped samples. Not only XYZ coordinates, but also magnification and light settings are reproduced automatically. The user simply places the target on the stage, and everything else – including alignment, focus adjustment, magnification switching and so on – is fully automatic. 

 

The VHX Series offers observation that exceeds conventional imaging tools. With advanced measurement capabilities, this system enables a variety of analyses. Expanded memory capacity allows for storage of millions of images. Its easy-to-use interface can be used effectively by expert and novice users. The VHX Series is equipped with all of the features needed to enhance your analysis.

 

https://www.keyence.com/ss/products/microscope/vhx-7000

Keyence VHX 7000 digital microscope features expanded memory, one-click focus

Keyence, Itasca, Ill., introduces the VHX-7000 Series digital microscope, the first model to feature the Focus View function, which enables simultaneous viewing of the lens and the target

Continue reading