Oil quench tank is custom-designed for metal stamping dies heated to 1550°F

November 23, 2018
Source:

L&L Special Furnace Co. Inc., Aston, Pa., has supplied a custom designed and manufactured oil quench tank that was designed to quench metal stamping dies that are heated to 1550°F. The quench tank, which has usable dimensions 12 x 12 x 24 inches, has an oil medium that is agitated by a one-horsepower pump that is directed up under the parts basket. An oil-to-water cooling heat exchanger controls the oil temperature. The system is designed to run one cycle per hour with 35 pounds of parts.

 

A resting stand is designed with the quench tank to allow the parts to drain after quenching. The oil flows back into the quench tank through an integrated drip tray that is attached to the stand. Ball valves located on the inlet and outlet of the quench tank allow further control of the quench medium.

 

www.llfurnace.com.

 

Oil quench tank is custom-designed for metal stamping dies heated to 1550°F

L&L Special Furnace Co. Inc., Aston, Pa., has supplied a custom designed and manufactured oil quench tank that was designed to quench metal stamping dies that are heated to 1550°F.

Continue reading

One Minute Mentor: Variations in Cooling Rate

November 20, 2018
Source:

Variations in cooling rate, from point to point, can exaggerate the production of residual stresses because, in some instances, it is possible for austenite transformation products to be different in sections with different cooling rates. For example, in rapidly cooled sections in moderately alloyed irons, it is possible for the austenite to transform to martensite, a very hard and brittle microconstituent that expands a different amount than the normal pearlitic or bainitic constituent when it forms from austenite.

This difference in expansion rates between differing transformation products adds to differences in contraction rates due to differences in section sizes. Typical cast shapes that could be expected to have different cooling rates from point to point are illustrated in the diagram.

The diagram shows four cast shapes and corresponding causes of residual stresses in castings.

(a) Differences in cooling rates due to shape.

(b) Nonuniform metal sections.

(c) Mechanical mold restraint.

(d) Surface peening during cleaning. Diagram courtesy of the American Foundry Society

Volume 4D, Heat Treating of Irons and Steels -> Heat Treatment of Cast Irons -> Introduction to Cast Iron Heat Treatment -> Heat Treatment Processes

One Minute Mentor: Variations in Cooling Rate

Variations in cooling rate, from point to point, can exaggerate the production of residual stresses because, in some instances, it is possible for austenite transformation products to be different in sections with different cooling rates.

Continue reading

Instron expands Calibration Laboratory services to North America, Europe, and Asia

November 17, 2018
Source:

Instron, Norwood, Mass., announces that its Calibration Laboratory has expanded its global reach to include providing accredited calibration services to its customers in North America, Europe, and Asia under a single National Voluntary Laboratory Accreditation Program (NVLAP).

 

Instron's Calibration laboratory is accredited to ISO/IEC 17025 for the calibration of Force, Angularity, Length, Electromagnetics, Time & Frequency, Hardness, Temperature, and Pressure by NVLAP, a program administered by the National Institute of Standards and Technology.

 

“One of the main advantages is that the calibration services for our multi-national customers will all fall under the same accreditation, simplifying internal processes associated with the validation of quality systems and much more,” says Jim Ritchey of Instron Service.

 

The NVLAP coverage includes both in-house calibration services and field calibration services. The biggest change to Instron’s coverage is that the company’s Limited Calibration Laboratory in the United Kingdom is now part of the Instron Calibration Laboratory in Norwood, covered under the NVLAP certificate. The U.K. lab was previously accredited to ISO 17025 for Force, Extension and Hardness by the United Kingdom Accreditation Service, Laboratory Number 0019.

 

NIST maintains an online register of certificates that can be found here:

https://www-s.nist.gov/niws/index.cfm?event=directory.search#no-back.

 

www.Instron.com

 

Instron expands Calibration Laboratory services to North America, Europe, and Asia

Instron, Norwood, Mass., announces that its Calibration Laboratory has expanded its global reach to include providing accredited calibration services to its customers in North America, Europe, and Asia under a single National Voluntary Laboratory Accreditation Program (NVLAP).

Continue reading

HRE Wheels, GE Additive build 3D-printed titanium wheel via electron beam melting

November 16, 2018
Source:

HRE Wheels, Vista Calif., and GE Additive, Cincinnati, Ohio, announced a partnership agreement and showed the first titanium wheel built via electron-beam melting of titanium powder. Known as “HRE3D+”, this new prototype wheel shows how advanced materials such as titanium can be harnessed to create complex designs.

 

The goal of the “HRE3D+” project was to test the capabilities of additive manufacturing in a practical application and to create a highly-sophisticated wheel design. With a traditional aluminum Monoblok wheel, 80% of material is removed from a 100-pound forged block of aluminum to create the final product. With additive manufacturing, only 5% of the titanium is removed and recycled, making the process far more efficient. Titanium also has a much higher specific strength than aluminum and is corrosion resistant, allowing it to be extremely lightweight and to be shown in its raw finish.

 

The wheel was produced on two Arcam EBM machines - Q20 and a Q10 in five separate sections, then combined using a custom center section and titanium fasteners.

 

"This is an incredibly exciting and important project for us as we get a glimpse into what the future of wheel design holds,” said HRE President Alan Peltier. “Working with GE Additive’s AddWorks team gave us access to the latest additive technology and an amazing team of engineers, allowing us to push the boundaries of wheel design beyond anything possible with current methods. To HRE, this partnership with GE Additive moves us into the future.”

 

“HRE prides itself on its commitment to excellence and superior quality in the marketplace. It was a natural fit for AddWorks to work on this project with them and really revolutionize the way wheels can be designed and manufactured,” said Robert Hanet, senior design engineer, GE Additive AddWorks.

 

www.hrewheels.com  

 

www.ge.com/additive

 

HRE Wheels, GE Additive build 3D-printed titanium wheel via electron beam melting

HRE Wheels, Vista Calif., and GE Additive, Cincinnati, Ohio, announce a partnership agreement and unveiled the first titanium wheel created using electron-beam melting of titanium powder.

Continue reading

JSW Steel breaks ground on uniquely integrated plate/pipe mill complex in Texas

November 15, 2018
Source:

JSW USA, Baytown, Texas, has broken ground on what its engineers believe to be the most technologically advanced and eco-friendly electric arc furnace, slab caster, and plate mill in the world. It is the only melt-and- manufacture plate mill with a contiguous pipe mill in North America. The melt-and-manufacture electric arc furnace and slab caster are being built on 111 acres at its 700-acre Baytown campus.

 

Thanks to new policies from Washington, JSW Steel USA is embarking on a journey to hire 1000 new workers and invest up to $1 billion to modernize and expand its U.S. operations. The project was initially unveiled in March of this year before an audience of more than 200 that included Texas Congressman Brian Babin, representatives from U.S. Senators Ted Cruz and John Cornyn’s offices, local economic development officials, and employees.

 

JSW USA, based in Baytown, Texas, is a wholly-owned subsidiary of JSW Group, a $13 billion group headquartered in India with more than 40,000 employees worldwide.

 

www.jswsteel.com

JSW Steel breaks ground on uniquely integrated plate/pipe mill complex in Texas

JSW USA, Baytown, Texas, has broken ground on what it believes to be the most technologically advanced and eco-friendly electric arc furnace, slab caster, and plate mill in the world.

Continue reading

Carpenter acquires LPW Technology, continues additive manufacturing investment


Source:

Carpenter Technology Corp., Philadelphia, announces it has acquired LPW Technology Ltd., England, for approximately $81 million.  LPW provides advanced metal powders and management solutions to the additive manufacturing industry. With its additional processing operations near Pittsburgh, Pa., LPW employs approximately 80 people.

 

“The acquisition combines LPW’s metal powder lifecycle management technology and processes with our technical expertise in engineered metal powders and additively manufactured components," said Tony R. Thene, Carpenter’s President and Chief Executive Officer. Lifecycle management technology is becoming increasingly important to understanding how materials behave before, during, and after production in the powder-bed fusion process.

 

Carpenter’s additive portfolio, including recent investments in Puris, a titanium powders producer; CalRAM, a leader in electron beam and laser powder-bed fusion additive manufacturing services, and construction of an Emerging Technology Center in Athens, Alabama, represent a significant force positioned to capitalize on  rapid AM growth.

 

www.cartech.com.

 

Carpenter acquires LPW Technology, continues additive manufacturing investment

Carpenter Technology Corp., Philadelphia, announces it has acquired LPW Technology Ltd., England, for approximately $81 million.

Continue reading

One Minute Mentor: Critical Temperature Ranges

November 11, 2018
Source:

The critical temperatures at which austenite changes to ferrite or pearlite, and vice versa, for iron differ from those for carbon steel, because silicon raises the transformation temperature range. In addition, silicon in iron decreases carbon solubility in austenite and tends to dissociate iron carbide. Thus, the carbon content of pearlite in iron can be appreciably lower than in the plain carbon and low-alloy steels. Depending on the silicon content and the cooling rate, the carbon content of pearlite varies and can be as low as 0.50 wt% C with 2.5% Si.

The dependence of critical temperatures on silicon content is shown in the graph, for cooling rates of 5 °C/h (9 °F/h). In this figure, the upper critical is shown as the temperature where ferrite first begins to form on cooling, and the lower critical temperature is the temperature where there is no remaining austenite.

Critical temperature values for heating at this same rate can be obtained by adding 33°C (60°F) to the critical temperatures on cooling. Note that neither the total carbon contents nor the combined carbon contents are significant.

 

Volume 4D, Heat Treating of Irons and Steels -> Introduction to Cast Iron Heat Treatment -> Critical Temperature Ranges

 

One Minute Mentor: Critical Temperature Ranges

The critical temperatures at which austenite changes to ferrite or pearlite, and vice versa, for iron differ from those for carbon steel, because silicon raises the transformation temperature range.

Continue reading

Gasbarre ships heat treating furnace for workloads 32 feet wide weighing 40,000 pounds


Source:

Gasbarre Furnace Group/J. L. Becker, Plymouth, Mich., recently shipped a large-capacity gas-fired temper furnace to a major specialty alloy manufacturing company located in the Northeastern portion of the United States. The furnace is designed to temper workloads after hardening. It is capable of processing workloads that are 32 feet wide by 6 feet long by 4 feet high and that weigh up to 40,000 pounds.

Temperature uniformity is achieved through five zones of heating, recirculation fans, and a custom-designed baffling system. As a result, the furnace is capable of achieving ±10°F from 800°F to 1400°F. The vertical lift door and hearth enables it to be installed in the company’s existing J. L. Becker heat treating system, and loaded and unloaded by a J. L. Becker manipulator. The control system incorporates an Allen Bradley MicroLogix PLC and PanelView HMI. A Eurotherm 3216 instrument controls the temperature in each zone.

www.gasbarrefurnacegroup.com

Gasbarre ships heat treating furnace for workloads 32 feet wide weighing 40,000 pounds

Gasbarre Furnace Group/J. L. Becker, Plymouth, Mich., recently shipped a large-capacity gas-fired temper furnace to a major specialty alloy manufacturing company located in the Northeastern portion of the United States.

Continue reading

Ipsen USA receives orders for nine Titan vacuum furnaces and seven others in October


Source:

Ipsen USA, Cherry Valley, secured multiple vacuum furnace orders last month, ending with a total of 16 new orders, including nine Titan vacuum furnaces, a record month in the 10-year production of the global platform product. Titan is known for its versatility and these furnaces continue to prove that, as they will be shipped worldwide for use in a variety of applications for companies in aerospace, automotive, and commercial heat-treating industries.

Titan furnaces:

--Are available in several sizes with horizontal or vertical configurations, nitrogen or argon quench and graphite or all-metal hot zone construction

--Incorporate a high-definition display with a touch screen

--Support a variety of standard processes, including hardening, annealing, tempering and brazing

--Are capable of meeting applicable AMS 2750, Nadcap and MedAccred requirements

--Maintain tight temperature uniformity of ±10 °F (±5 °C) from 1,000 °F to 2,400 °F (540 °C to 1,320 °C)

--Use approximately 40% less floor space¹, and its compact design allows for ease of installation

 

In addition to the strong bookings for the Titan product line, Ipsen also sold seven custom units, including MetalMaster, TurboTreater, and  vacuum aluminum brazing furnaces.

 

www.ipsenusa.com

 

_____________________________

Ipsen USA receives orders for nine Titan vacuum furnaces and seven others in October

Ipsen USA, Cherry Valley, secured multiple vacuum furnace orders last month, ending with a total of 16 new orders, including nine Titan vacuum furnaces, a record month in the 10-year production of the global platform product.

Continue reading

Nadcap recognizes Solar Atmospheres Greenville plant for superior performance


Source:

Solar Atmospheres, Greenville, S.C., announces that it has been awarded Nadcap 18-month Merit status for Heat Treating, Brazing, and Carburizing. The company is extremely pleased PRI has recognized its corporate commitment to quality. Achieving 18-month merit has been a goal set by Solar’s employees since opening its doors in 2015. Solar says that adherence to strict specification requirements, flawless process execution, and a daily commitment to quality processing is evident among all employees of Solar Atmospheres.

The Solar Atmospheres Greenville facility has held Nadcap accreditation since 2015. Having demonstrated ongoing commitment to quality by satisfying customer requirements and industry specifications, the Nadcap Task Group has determined that Solar Atmospheres – Greenville has earned this special recognition. Instead of having the next Nadcap audit in twelve months, Solar has been granted an accreditation that lasts until 30 April 2020.

“Achieving Nadcap accreditation is not easy,” says Joe Pinto, Executive Vice President and Chief Operating Officer at the Performance Review Institute. “It is one of the ways in which the aerospace industry identifies those who excel at manufacturing quality product through superior special processes. Companies such as Solar Atmospheres go above and beyond achieving Nadcap accreditation to obtain Merit status.”

www.solaratm.com

 

 

Nadcap recognizes Solar Atmospheres Greenville plant for superior performance

Solar Atmospheres, Greenville, S.C., announces that it has been awarded Nadcap 18-month Merit status for Heat Treating, Brazing and Carburizing.

Continue reading