Buehler receives ISO certification for Vickers, Knoop reference hardness testing blocks

Buehler, Lake Bluff, Ill., announces that the Buehler Wilson Reference Block Laboratory in Binghamton, N.Y., has achieved accreditation to ISO/IEC 17025 by A2LA (American Association for Laboratory Accreditation) for Rockwell, Knoop, Vickers, and Brinell hardness test blocks and indenters.