One Minute Mentor: Distortion in Plasma-Carburized Stainless Steel

December 19, 2016
Source:

The graph shows the XRD patterns of low-temperature plasma-nitrided (PN), plasma-carburized (PC), and untreated AISI 316 stainless steel samples. It illustrates the displacement of the peaks corresponding to the γ-phase to the left, with increasing nitrogen or carbon. The shift is smaller for the PC sample than for the PN sample, indicating less lattice expansion and less distortion in the carbon S-phase.

Volume 4D, Heat Treating of Irons and Steels ⇒ Heat Treated High-Alloy Steels ⇒ Nitriding of Stainless Steels ⇒ Stainless Steels 

One Minute Mentor: Distortion in Plasma-Carburized Stainless Steel

The graph shows the XRD patterns of low-temperature plasma-nitrided (PN), plasma-carburized (PC), and untreated AISI 316 stainless steel samples.

Continue reading

Vertical drop bottom furnace to heat treat aerospace aluminum alloys

December 14, 2016
Source:

Consolidated Engineering Co., Kennesaw, Ga., announces that it has received a purchase order for a mobile gantry drop bottom heat treat furnace system from a leading provider of aluminum alloys for aerospace applications. The solution furnace is a vertical tower furnace for aluminum alloys. It is supported by one of two quench tanks – water and glycol in water. Also included is a vertical rinse with glycol thermal separation/reclamation.

The new solution furnace is a key component in a large expansion by this company to satisfy increasing demand for its aluminum alloys. CEC was chosen as a partner based on technical competence and successful prior furnace installation in 2012.

Drop bottom furnaces are used when material properties are critical and the time from solution heat treating to quench must be minimal. CEC has a standard line of furnaces covered in its drop bottom system (DBS) series. For instance, a DBS 200 has 200 cubic feet of load basket capacity. CEC units range in sizes from 50 cubic feet to 300 cubic feet in standard configurations and designs. Mobile quench tanks can be heated and cooled, and percent glycol can be controlled

www.cec-intl.com

 

Vertical drop bottom furnace to heat treat aerospace aluminum alloys

Consolidated Engineering Co., Kennesaw, Ga., announces that it has received a purchase order for a mobile gantry drop bottom heat treat furnace system from a leading provider of aluminum alloys for aerospace applications.

Continue reading

Belt casting to cut steel production costs, enable casting of TWIP and TRIP steels


Source:

The University of Warwick, England, announces that engineers at its Advanced Steels Research Centre are evaluating belt casting technology as a way to cut steel production costs and reduce energy costs by a factor of three.

Belt casting is a near-net-shape casting process that produces strip needing minimal hot deformation to achieve the required product thickness. It is also very efficient because it can minimize or eliminate any reheating processes. The technology can also cast certain advanced high strength strip (AHSS) steel grades that are commercially attractive but cannot be produced by conventional casting techniques. These include TWIP (twinning induced plasticity) and TRIP (transformation induced plasticity), which have twice the strength and three times the ductility of conventional steels – as well as high-aluminum steels, which have a combination of good strength and lower density.

The Assure2 project team, led Prof. Claire Davis, has simulated belt cast microstructures, including dynamic direct observation of the solidifying steel at different cooling rates. The team has demonstrated that the microstructures are altered by the higher cooling rate of belt casting, compared to conventional slab casting, and that further beneficial modifications (such as reduction in grain size in high-aluminum steels) can be achieved by composition control.

In the Assure2 project, quantitative relationships between composition, process parameters and microstructure (and hence final product properties) are being established, taking into account the higher cooling rates of belt casting and the reduced hot deformation after casting to final thickness compared to conventional processing

http://www2.warwick.ac.uk/newsandevents/news/uk_steel_production/

 

Belt casting to cut steel production costs, enable casting of TWIP and TRIP steels

The University of Warwick, England, announces that engineers at its Advanced Steels Research Centre are evaluating belt casting technology as a way to cut steel production costs and reduce energy costs by a factor of three.

Continue reading

Portable heat treating system reduces crack sensitivity in aluminum plate

December 13, 2016
Source:

The Navy Metalworking Center, Johnstown, Pa., reports that it has designed and fabricated a heat treating system for aluminum plate that reduces sensitivity to cracking in the aluminum superstructure of the U.S. Navy's CG 47 class cruisers.  Prior to this development, cracked aluminum superstructures required extensive repairs or replacement (i.e., removing and replacing the affected plate, as well as all of the outfitting obstructing the area).

The Navy Metalworking Center led a project to address the major contributor to the cracking – the sensitized microstructure in the 5456 aluminum-magnesium alloy used in the construction of the structure. An Integrated Project Team developed and demonstrated a portable heat treatment system that reverses the sensitization in the 5456 aluminum alloy, thereby restoring the affected material in the ship's superstructure to a stabilized condition, which greatly reduces the propensity for cracking.

NMC conducted laboratory tests and finite element simulations to derive the optimized parameters for the reverse sensitization process. Based on this data, NMC designed and fabricated a prototype reverse sensitization unit (RSU), which imparts the necessary heat treatment to the aluminum plate in the CG class cruiser superstructure. The RSU was tested on laboratory sensitized panels, and a mockup of a CG superstructure was designed by NMC. The RSU was then demonstrated onboard two cruisers (one decommissioned, one active duty).

The final RSU prototype system was transitioned to PMS 407 for additional evaluation and use during maintenance intervals. A procurement specification was also developed by NMC, so that additional units may be built after successful implementation. The new process and RSU were implemented in September 2016 with the transition of the equipment to Ingalls Shipbuilding, the planning yard for CG repairs.

Reverse sensitization will give the Navy a low-cost alternative to the current process of cutting out and replacing the sensitized plate.  The reverse sensitization repair process can save as much as $2.4M per CG 47 ship availability, resulting in a cost avoidance of as much as $43.2M for 18 ships. The Littoral Combat Ship program will also benefit from this improved technology at a conservative estimate of $500K avoidance per hull, resulting in an additional $4M in cost avoidance for the LCS hulls in service over the next five years.

 

https://www.navalmetalworking.org/

 

Portable heat treating system reduces crack sensitivity in aluminum plate

The Navy Metalworking Center, Johnstown, Pa., reports that it has designed and fabricated a heat treating system for aluminum plate that reduces sensitivity to cracking in the aluminum superstructure of the U.S. Navy’s CG 47 class cruisers.

Continue reading

Scanning lasers evaluated as part of an industrial process for hardening steel

December 11, 2016
Source:

Researchers at the UPV/EHU-University of the Basque Country, Spain, say they have validated a laser scanning optics system that may enable laser hardening of steel parts of varying shape and thickness at an industrial scale. The UPV/EHU's High Performance Manufacturing group conducted the study.

Because laser beams are highly localized, the process hardens only the selected surface, leaving the core of the part in its original state. "Therefore, the parts are not as brittle, and because little heat is inserted, the part does not become as distorted," explains Aitzol Lamikiz, professor of the UPV/EHU's department of Mechanical Engineering. Although laser hardening has been used since 2000, it is limited: "The laser sweeps a constant bandwidth, so the hardened zone thus ends up with a constant thickness."

To make the technology more flexible, researchers decided to assess the viability of incorporating scanning optics into the process. Based on a galvanometric scanner, the technology involves moving a very small laser at high speed, sweeping across the surface line by line. That way, the hardening width can be adapted simply by changing the program parameters.

Prof. Lamikiz says that conventional laser hardening "would be like painting a wall with a roller, so the width that is painted corresponds to that of the roller. However, with the new technique, we replace the roller with a marker with the finest point.

"The experiments showed that it is possible to use this technique to carry out the hardening process. Then we saw how the result of the treatment changed according to the speed of the laser movement, the power used, etc. According to our tests, when the laser moves very fast, the results are similar to those of the conventional laser hardening process."

The researchers then partnered with companies in the Basque Country and Piedmont (Italy), in a project known as Hardlas, to see how far the process was viable. "We can say that the project was a success, as we saw that it was viable, and that it could be transferred to industry."

One of the main difficulties they came up against was controlling the process: "It is very important to get the material treated to the necessary temperature so that the hardening takes place, but it must not be exceeded, otherwise we would melt the material," explains Prof. Lamikiz. "In our process, as the laser is constantly moving, control is more complex." In addition, the tests were carried out at the university on lab equipment. To develop the process for an industrial scale, it would be important to try it out with more powerful lasers, different types of lasers, and on other materials.

S. Martínez, A. Lamikiz, E. Ukar, A. Calleja, J.A. Arrizubieta, L.N. Lopez de Lacalle (2016) 'Analysis of the regimes in the scanner-based laser hardening process'. Optics and Lasers in Engineering, 90: 72–80. DOI: http://dx.doi.org/10.1016/j.optlaseng.2016.10.005

Matxalen Sotillo    [email protected]    

www.ehu.eus

 

 

Scanning lasers evaluated as part of an industrial process for hardening steel

Researchers at the UPV/EHU-University of the Basque Country, Spain, say they have validated a laser scanning optics system that may enable laser hardening of steel parts of varying shape and thickness at an industrial scale.

Continue reading

One Minute Mentor: The S-Phase

December 9, 2016
Source:

The success of plasma and gas nitriding at low temperatures (lower than 840°F) and solution nitriding at high temperatures is associated with the absence of chromium nitride or carbide precipitation, and thus with the formation in the surface layer of a particular phase called the S-phase. This nitrogen- and/or carbon-rich phase presents higher concentration of the interstitials when treated at lower treatment temperatures and when high-chromium alloys are used, resulting in better properties. 

The figure shows the XRD patterns of untreated and plasma-nitrided AISI 316 stainless steel at 790°F. It illustrates the displacement of the peaks corresponding to the γ-phase to the left, with increasing nitrogen, as well as the broadening of these peaks, compared to the γ-phase peaks of the untreated steel.

Volume 4D, Heat Treating of Irons and Steels â‡’ Heat Treated High-Alloy Steels ⇒ Nitriding of Stainless Steels ⇒ Stainless Steels 

One Minute Mentor: The S-Phase

The success of plasma and gas nitriding at low temperatures (lower than 840°F) and solution nitriding at high temperatures is associated with the absence of chromium nitride or carbide precipitation, and thus with the formation in the surface layer of a particular phase called the S-phase.

Continue reading

Nucor to acquire Southland Tube for its high-strength steel hollow tubing

December 7, 2016
Source:

Nucor Corp., Charlotte, N.C., has agreed to acquire Southland Tube, an independent manufacturer of hollow structural section steel tubing, because "It is an excellent fit for our Nucor family and our strategy for profitable growth," said John Ferriola, Chairman, CEO and President of Nucor. Cost was $130 million, or approximately eight times average EBITDA over the 2011-2016 period.

"The acquisition of Southland Tube complements our recent acquisition of Independence Tube in the HSS steel tubing market., added Mr. Ferriola. "We see this market as a great opportunity to leverage Nucor's capabilities and strengths while also adding to our portfolio of products and services for our customers."

HSS is used in a broad array of structural and mechanical applications, including nonresidential construction, infrastructure, and heavy equipment end-use markets. Southland Tube has one facility located in Birmingham, Alabama, which is well situated to serve the HSS market.

With annual shipments of about 240,000 tons, Southland Tube has the third largest market share in HSS steel tubing.

Through the acquisitions of Independence Tube and Southland Tube, Nucor is building a market leadership position in the HSS steel tubing market and providing an additional channel to market for Nucor's sheet steel mills.  In 2006, 8% of Nucor's total steel mill shipments were to its downstream businesses.  The company expects that number to grow to about 20% with these acquisitions.

www.nucor.com

 

 

Nucor to acquire Southland Tube for its high-strength steel hollow tubing

Nucor Corp., Charlotte, N.C., has agreed to acquire Southland Tube, an independent manufacturer of hollow structural section steel tubing, because “It is an excellent fit for our Nucor family and our strategy for profitable growth,” said John Ferriola, Chairman, CEO and President of Nucor.

Continue reading

Developers of Constellium Airware aluminum-lithium alloys receive award


Source:

Constellium N.V., Amsterdam, announces that three of its researchers were awarded the Medal of the Academy by the Air and Space Academy for their achievement in developing groundbreaking Airware aluminum-lithium alloys: ASM member Timothy Warner, Knowledge Director and Metallurgy Group Manager; Alireza Arbab, Project Manager;  and Bruno Chenal, Strategic Innovation Director. They received the medal at the annual Solemn Session held by the AAE on November 25 in Toulouse, France.

"We are particularly proud that Airware  is now flying on the most prestigious aircraft and space programs, such as the Airbus A350 XWB, Bombardier's CSeries, the SpaceX Falcon Launcher, and Lockheed Martin's Orion Capsule," said Mr. Chenal.

Airware is a major component in the advanced materials portfolio of the A350 XWB manufactured by Airbus. At the same session, Fabrice Brégier, President and CEO of Airbus, received the Academy's Grand Award for his decisive role in the success of the A350 XWB program.

Constellium's Airware was launched in 2010 as a group of high-performance aluminum-lithium alloys suitable for applications in all parts of the primary aerostructure. Airware's lower density and improved properties allow optimization of structural designs, which leads to an overall weight reduction and a drop in CO2 emissions. Airware guarantees higher durability due to its greater resistance to fatigue and corrosion, which enables airlines to target extended intervals of heavy maintenance. Airware is endlessly recyclable without any loss of properties. The technology contributes to the development of a sustainable aerospace industry.

www.constellium.com

 

Developers of Constellium Airware aluminum-lithium alloys receive award

Constellium N.V., Amsterdam, announces that three of its researchers were awarded the Medal of the Academy by the Air and Space Academy for their achievement in developing groundbreaking Airware aluminum-lithium alloys: ASM member Timothy Warner, Knowledge Director and Metallurgy Group Manager; Alireza Arbab, Project Manager; and Bruno Chenal, Strategic Innovation Director.

Continue reading

Ipsen announces 2017 heat treating courses scheduled for United States


Source:

Ipsen, Cherry Valley, Ill., announces that it will begin 2017 by hosting another series of Ipsen U classes, with courses available February 7-9, April 4-6, June 6-8, August 1-3, and October 3-5. The newly remodeled, state-of-the-art space offers an ideal arena for attendees to build and refresh their knowledge of heat-treating equipment, processes, and maintenance through applied learning. For those that prefer to stay close to home, Ipsen will also be providing additional one-day trainings throughout the United States. Specific topics that will be covered during these local seminars include:

Vacuum and atmosphere furnace maintenance best practices

Optimizing operations with predictive maintenance

Achieving and maintaining Aerospace compliance

Overall, both training opportunities will teach best practices for regaining control of your equipment and offer expert insight into specific maintenance issues you might be experiencing on a daily basis. Reflecting on past courses, attendees commented that "staff and facility are top notch and very knowledgeable in the heat-treating process."

Register today for an upcoming 2017 Ipsen U course, and stay tuned for local seminars that may be coming to your area.

www.IpsenUSA.com/Seminar-Registration-Form

 

 

Ipsen announces 2017 heat treating courses scheduled for United States

Ipsen, Cherry Valley, Ill., announces that it will begin 2017 by hosting another series of Ipsen U classes, with courses available February 7-9, April 4-6, June 6-8, August 1-3, and October 3-5.

Continue reading

Seco Warwick jet cooling chambers cut heat treating costs and emissions


Source:

Seco Warwick, Meadville, Pa., announces that it has completed the installation of two replacement jet cooling chambers at Worthington Industries in Jefferson, Ohio. To provide Worthington with the most cost-efficient system upgrade, the cooling chambers were supplied so that the existing components such as rolls, bearings, gaskets, sprockets, and chain were used from the old chambers. The contract included removal of the faulty cooling chambers, and installation and start up of the updated system.

According to Jim Williams, Group Leader at Worthington Industries, ʺWe accomplished this project by partnering with the Seco Warwick team.  It was a coordinated effort to establish lead-times for all of the necessary components as well as offsite fabrication of the two jet cooling sections. We then identified a two-week window for the demolition of the ‘old' cooling zones, and installation of the ‘new' jet cooling zones. The project was completed with minimal issues; as we continued to operate our usual production schedule." 

The goal of this new design was to lower the product temperature while reducing the volume of water to achieve this result. Worthington now runs a continuous 10,000 pounds per hour of production through the system, lowering the temperature by utilizing a state of the art jet cooling system.

"Seco Warwick has the technical expertise to perform modernizations that are not only cost-effective, but also provide the newest technology available for the application," says Jonathan Markley, Managing Director of Seco Warwick USA ʺOur goal is to enable customers to extend the useful service life of their equipment and meet performance specifications at the lowest possible capital cost. We call this process of partnering with our customers to achieve the best result, Seconomy."

The Seconomy service package is geared toward companies that are searching for savings and want their facility to be environmentally friendly. It is a program of heat treatment equipment modernization through upgrades designed to meet the needs of customers and comply with strict environmental regulations. These packages are designed specifically for heat treatment equipment that has been in operation for over ten years, requiring updates to reduce production costs and emissions while increasing process efficiency.

www.secowarwick.com

worthingtonindustries.com

 

Seco Warwick jet cooling chambers cut heat treating costs and emissions

Seco Warwick, Meadville, Pa., announces that it has completed the installation of two replacement jet cooling chambers at Worthington Industries in Jefferson, Ohio.

Continue reading