One Minute Mentor: Iron-Nickel Precipitation-Hardenable Superalloys
November 7, 2016
Source:
It is important to note that tensile properties are influenced not only by heat treatment, but also by control of structure during thermomechanical processing. The graph shows the effects of temperature and grain size on tensile properties of Incoloy 901 forgings in the solution-treated, stabilized, and aged condition. (AC = air cooled.)
Specifically, the graph shows the effect of solution temperatures from 1750 to 2000°F and grain sizes ranging from ASTM 2 to 12 on tensile properties of Incoloy 901 processed using this method. The high-cycle fatigue strength of Incoloy 901 doubled as a result of the reduction in grain size from ASTM 2 to 12. The low-cycle fatigue also improved greatly with decreasing grain size.
Volume 4D, Heat Treating of Irons and Steels ⇒ Heat Treated High-Alloy Steels ⇒ Heat Treating of Precipitation-Hardenable Stainless Steels and Iron-Base Superalloys ⇒ Iron-Nickel Precipitation-Hardenable Superalloys
It is important to note that tensile properties are influenced not only by heat treatment, but also by control of structure during thermomechanical processing.
Continue reading
PdMetrics software now included with Ipsen Titan heat treat systems
Source:
Ipsen, Cherry Valley, Ill., announces that its PdMetrics platform is now included standard with its Titan heat treating systems. PdMetrics securely connects to a network of integrated sensors on the furnace to gather and analyze data, run algorithms, and provide real-time diagnostics. As a result, these Titan furnaces provide sophisticated monitoring of critical systems and key parameters that improve the health and integrity of the equipment.
Ipsen recently delivered two Titan H2-size vacuum furnaces with 1.9-bar gas quenching and the PdMetrics platform to Japan. Shipped within three weeks of each other, these furnaces will be used by separate commercial heat treaters and feature 18 x 24 x 18-inch graphite hot zones with a 1000-pound load capacity. They operate at temperatures up to 2400°F with ±10°F uniformity, and are capable of meeting applicable AMS 2750E and Nadcap requirements.
Both companies also took a proactive approach to preventive maintenance by ordering one of Ipsen's many spare parts kits. These kits consist of consumable and preventive maintenance items to help ensure equipment uptime and keep the furnace running smoothly.
www.IpsenUSA.com/TITAN
Ipsen, Cherry Valley, Ill., announces that its PdMetrics platform is now included standard with its Titan heat treating systems.
Continue reading
Russian scientists develop strong shape memory alloy based on Fe-Ni-Co-Al
Source:
The Tomsk University Laboratory for Physics of High-Strength Crystals, Russia, announces that its researchers have designed a new high-strength iron-base shape-memory alloy whose properties are developed through a heat treatment technology that they have patented. "We especially use iron-nickel-cobalt-aluminum, plus a fifth element that could be titanium, niobium, or tantalum," says Prof. Yury Chumlyakov, head of the laboratory. "These alloys can compete with nickel titanium."
In particular, the researchers claim that the alloys have a reversible change in shape of about 15%, while nickel-titanium alloys have about 10%. Thus, the sensors and actuators made of the alloys would work more effectively. The iron-base alloys are also said to have high strength, important for practical use in devices that must withstand high external loads, such as components for the aerospace and engineering industries.
The laboratory researchers emphasize that these sensors and actuation devices would be not only stronger, but also cheaper than nickel-titanium. Thus, they can reduce the cost of production of household equipment, fire alarm sensors, connecting elements for aerospace and automotive components, and many other devices.
The scientists developed the material within the framework of the project called "Mechanisms of Phase and Structural Transformations in High-Strength Crystals of Iron and Nickel-Titanium Based Alloys with Conventional and Magnetic Shape Memory Effect." This project is supported by a grant from the Russian Science Foundation in the amount of $790,000. The goal of the program is to improve the quality of actuating mechanisms and sensors for mechanical engineering, aerospace, and other industries. The laboratory plans to continue studying these alloys.
The results of their study were presented at the international conference Alloys with Shape Memory Effect (St. Petersburg).
http://en.tsu.ru/news/tsu-physicists-have-created-a-high-strength-material-for-the-aerospace/
http://en.tsu.ru/

The Tomsk University Laboratory for Physics of High-Strength Crystals, Russia, announces that its researchers have designed a new high-strength iron-base shape-memory alloy whose properties are developed through a heat treatment technology that they have patented.
Continue reading
American Axle acquires Metaldyne Performance Group
November 6, 2016
Source:
American Axle & Manufacturing Holdings Inc., Detroit, and Metaldyne Performance Group Inc., Southfield, Mich., announce that they have entered into a definitive merger agreement under which AAM will acquire MPG for approximately $1.6 billion in cash and stock, plus the assumption of $1.7 billion in net debt. The combination brings together highly complementary businesses and forms a global Tier 1 supplier with broad capabilities across powertrain, drivetrain, and driveline product lines, as well as a diversified customer base and end-markets.
"MPG's expertise in complex, highly-engineered powertrain components and its global footprint will be tremendous assets to AAM," says David C. Dauch, AAM's Chairman and Chief Executive Officer. "Together, we are forming a company with increased earnings potential and enhanced cash flow generation that will allow us to rapidly reduce leverage while fueling growth and delivering value to our shareholders."
According to George Thanopoulos, MPG's Chief Executive Officer, "MPG and AAM share a similar culture and value system, laser focused on quality, operational excellence and technology leadership, which creates a natural fit and clear path to value creation for stakeholders of both companies."
Under the terms of the agreement, each share of MPG's common stock will be converted into the right to receive $13.50 per share in cash and 0.5 share of AAM common stock. Upon closing of the transaction, AAM's shareholders will own approximately 70% of the combined company and MPG's shareholders will own approximately 30%. The transaction has been unanimously approved by the boards of directors of both companies and is anticipated to close in the first half of 2017 subject to shareholder and regulatory approval and other customary closing conditions.
Concurrent with the signing of the merger agreement, AAM entered into a voting agreement with an affiliate of American Securities LLC, the controlling stockholder of MPG, pursuant to which American Securities LLC has agreed to vote in favor of and otherwise support the transaction, subject to the terms of the voting agreement. Following the transaction, an affiliate of American Securities LLC will own approximately 23% of the combined company.
www.mpgdriven.com
American Axle & Manufacturing Holdings Inc., Detroit, and Metaldyne Performance Group Inc., Southfield, Mich., announce that they have entered into a definitive merger agreement under which AAM will acquire MPG for approximately $1.6 billion in cash and stock, plus the assumption of $1.7 billion in net debt.
Continue reading
Electric oxidizing oven heat treats Inconel trays for nuclear power fuel cell rods
November 2, 2016
Source:
Baker Furnace Inc., Yorba Linda, Calif., has shipped an electric oxidizing oven to a manufacturer of components for nuclear power plants to heat treat Inconel support trays that hold nuclear fuel cell rods in place. The heat treating process extends the life of the trays and reduces production costs for the manufacturer.
The heat treating oven has a maximum temperature rating of 1350°F and work zone dimensions of 5 x 5 x 5 feet. The unique Baker Furnace door design offers a lifetime no-sag guarantee along with a pneumatic door locking mechanism. A recirculation fan provides approximately 25 air changes per minute through adjustable air distribution via sidewall ducts, with the return air at the rear of the work chamber for temperature uniformity of ±25°F at 1300°F. The oxidizing oven utilizes a programmable temperature controller with ramp and soak capabilities.
Unique features of this oxidizing oven include a 316L stainless steel interior; pneumonic door locking mechanism; 90kW rod style heating elements; 3000 CFM recirculation fans.
www.bakerfurnace.com
Baker Furnace Inc., Yorba Linda, Calif., has shipped an electric oxidizing oven to a manufacturer of components for nuclear power plants to heat treat Inconel support trays that hold nuclear fuel cell rods in place.
Continue reading
Alcoa completes separation from parent company Arconic
Source:
Alcoa Corp., Pittsburgh, announces that it has completed the separation from its parent company Alcoa Inc. (now named Arconic Inc.) and has begun operating as an independent, publicly traded company listed on the New York Stock Exchange under the symbol AA. Alcoa Corporation is a globally cost-competitive industry leader in bauxite, alumina, and aluminum products, positioned to succeed throughout the market cycle.
The separation was completed through a pro rata distribution by Alcoa Inc. of 80.1% of the outstanding shares of the newly formed Alcoa Corporation. Arconic will retain 19.9% of Alcoa Corporation common stock.
"We are launching Alcoa Corporation as a world leader in the aluminum industry with distinct competitive advantages across the value chain," says Roy Harvey, Chief Executive Officer of Alcoa. "Our bauxite and alumina portfolios enjoy strong first quartile cost positions and our aluminum portfolio has a highly competitive second quartile position. We've made a commercial success of our cast products business. Our can sheet business is a leader in North America, and our substantial energy assets are also driving value for maximum profitability."
"Today we launch Arconic as a strong independent company," said Arconic Chairman and CEO Klaus Kleinfeld on Nov. 1. "Our multi-year transformation while part of Alcoa Inc. substantially improved our competitiveness and profitability. Today, we are very well positioned as a leader in attractive markets."
Within aerospace, which accounts for approximately 40% of Arconic total revenues, the company develops and manufactures high-performance, engineered products and solutions for airframe structures and aero engines. Since 2008, the company has significantly grown its capabilities through a combination of organic and inorganic technology and innovation-focused investments.
As a result, Arconic has gained significant share on next generation aero engines and aero structures. The company can today supply over 90% of the components within the jet engine, and it is a leader in structural parts for both metallic and carbon fiber reinforced plastic (CFRP) aircraft. In fact, 85% of aerospace revenues come from products where it holds either the number one or number two market position.
In the North American automotive market, Arconic invented the bonding process to enable the mass-market shift from steel to aluminum, and it is today at the forefront of capturing growing demand for aluminum sheet as the industry shifts to light-weighting. The Company expects its North American automotive sheet revenues to grow six-fold, from $229 million in 2013 to $1.3 billion in 2018. Across its North American automotive portfolio, 96% of the company's revenues come from products where it is number one or number two in its market.
www.alcoa.com
www.arconic.com
Alcoa Corp., Pittsburgh, announces that it has completed the separation from its parent company Alcoa Inc. (now named Arconic Inc.) and has begun operating as an independent, publicly-traded company listed on the New York Stock Exchange under the symbol AA.
Continue reading
Buehler IsoMet High Speed precision cutter enables consistent metal sample sectioning
November 1, 2016
Source:
Buehler, Lake Bluff, Ill., introduces the IsoMet High Speed, a precision sectioning machine designed specifically to create consistent and efficient cuts in metals and other materials using diamond or abrasive blades. It features a robust saw that provides consistent sectioning performance for busy laboratories with the following key features:
Automated three-axis movement allows precise alignment and quick cutting.
Automatic dressing system maintains consistent cut quality and reduces the frequency of changing the dressing stick.
Rapid laser alignment saves time with instant visual alignment with laser.
Intuitive controls allow programming for repeatable and consistent single or serial sections.
Quick sample adjustments offer easy adjusting of sample with the Rapid Rail and tool-less vising system.
According to Product Manager Chelsea Frid, "The IsoMet High Speed is available in two formats – the High Speed and the High Speed Pro. Both provide strength and power to produce quality cut surfaces. In the High Speed Pro version, Buehler has added additional abilities to improve user experience with a laser for visual blade alignment and an automatic dressing system to maintain diamond blade quality throughout the cut."
Buehler offers a complete selection of IsoMet High Speed accessories, including Rapid Rail Vise Holder, Single Saddle Chuck, Double Saddle Chuck, quick clamp vises, dressing wheels, and external recirculation tank.
Buehler is a leading provider of scientific equipment, supplies, consumables and analysis techniques for use in materials preparation, image analyses and hardness testing.
www.buehler.com
Buehler, Lake Bluff, Ill., introduces the IsoMet High Speed, a precision sectioning machine designed specifically to create consistent and efficient cuts in metals and other materials using diamond or abrasive blades.
Continue reading
Iowa State wins $2.8 million DOE grant to make ductile 6.5% Si electrical steel
October 31, 2016
Source:
Iowa State University and its Ames Laboratory report that researchers have received a three-year, $2.8 million grant to develop a ductile electrical steel containing 6.5% silicon, twice the amount in electric motor steel today. The extra silicon increases the electrical resistivity of the material by about 50%, helping to make the motors smaller, lighter, more powerful, and more cost effective. Associate Professor of Materials Science and Engineering Jun Cui says he thinks these motors could run at much higher frequencies – jumping from today's 60 hertz all the way to 400 hertz — but the alloy is currently too brittle and too expensive to make.
Therefore, the U.S. Department of Energy is supporting the work with a three-year, $3.8 million grant from the DOE's Vehicle Technologies Program. Of that, $2.8 million will support research at Iowa State. The project also includes research partners from the United Technologies Research Center in East Hartford, Connecticut; and the University of Delaware in Newark.
The Iowa State-Ames Laboratory researchers will study and characterize different processes for making the new electrical steel to increase ductility and reduce manufacturing costs. Prof. Cui says that the researchers are also committed to developing materials and motors that do not depend on magnets made with rare-earth materials, which are rising in cost.
"The fundamental drive for this project is that we want more cost-effective and efficient electric motors," Prof. Cui says. "In about ten years, if we're lucky, we should see a real impact of this work. We should see these motors on the road." (Image courtesy Nucor)
http://www.news.iastate.edu/news/2016/09/27/electricalsteel
Iowa State University and its Ames Laboratory report that researchers have received a three-year, $2.8 million grant to develop a ductile electrical steel containing 6.5% silicon, twice the amount in electric motor steel today.
Continue reading
One Minute Mentor: Variations in Heat-Treating Cycles of PH Stainless Steels
Source:
One of the principal advantages of these materials is their versatility. Although certain heat treatments are classified as standard, there are applications where deviations from these standards are desirable.
The graphs show the effect of variations in annealing temperature on typical mechanical properties of 17-7 PH sheet, strip, and plate.
Heat Treating of Precipitation-Hardenable Stainless Steels and Iron-Base Superalloys ⇒ Heat Treated High-Alloy Steels ⇒ Heat Treating of Martensitic Stainless Steels ⇒ General Procedures
One of the principal advantages of these materials is their versatility.
Continue reading
Thermo-Calc and QuesTek partner for advanced modeling and materials design
October 28, 2016
Source: ASM International
Thermo-Calc Software AB, Stockholm, and QuesTek International LLC, Evanston, Ill., have partnered to establish a joint company, QuesTek Europe AB, which will offer Integrated Computational Materials Engineering modeling services and novel materials design and development to the European market.