Nitride coatings based on titanium and other metals protect jet engine components

August 30, 2016
Source:

Wallwork Heat Treating, England, reports that its Nitron Flight PVD-applied nitride coatings based on titanium, chromium, chromium-aluminum, and carbon/metal carbides improve the performance of key jet engine components. The graded coatings are precision engineered for thickness and composition, from 3 to 30 microns thick and hardness up to 3000HV. They are applied to critical flying parts such as turbine blades and other high-stress components.

Advantages include longer service life, extended service intervals, resistance to erosion and encrustation, and increased scope for material substitution to save weight.

Comparative wear tests carried out by Wallwork Cambridge on Ti-64 samples revealed that Nitron Flight coatings reduced abrasive wear by more than 75%. They can be applied to titanium, steel, and advanced alloy surfaces such as engine blades/vanes for operation at temperatures up to 1000°C. The coatings are applied in a duplex process using PVD in a variety of basic formulations of metal nitrides, and in a variety of single and multiple-layer coatings to suit specific applications.

Applications are many and include landing gear, engine bearings, high-temperature engine seals, engine compressor sections, valve components, and many others.  The company offers both  standard and customized coatings to meet special situations. Coating processes are Nadcap certified with complete documentation and traceability.

www.wallworkht.co.uk

 

Nitride coatings based on titanium and other metals protect jet engine components

Wallwork Heat Treating, England, reports that its Nitron Flight PVD-applied nitride coatings based on titanium, chromium, chromium-aluminum, and carbon/metal carbides improve the performance of key jet engine components.

Continue reading

How manganese prevents oxidation in high-strength steel


Source:

A team from the University of Warwick, UK, discovered that the amount of oxide that forms at the surface of automotive high-strength steels depends on the ratio between manganese and additional alloying elements. High-strength steels are obviously an important backbone for applications in the automotive industry, but cost-efficient manufacture requires the suppression of oxides within the steel during sheet production.

When steel sheet is produced in rolling mills at high temperatures, the surface oxidizes quickly, but the grain boundary oxides underneath define the depth of the corroded zone and also the forming limit. Hence, oxidation plays an essential role during the manufacture of high strength steels for automotive applications, because they often contain a higher amount of manganese. Due to their unique mechanical properties, this allows for a significant reduction of sheet thickness, allowing vehicles to be lighter in weight with lower carbon emissions.

The research was led by the Warwick Manufacturing Group (WMG) at the University of Warwick. The research, led by Dr. Michael Auinger of WMG, together with the Vienna University of Technology (Austria) and Voestalpine Stahl GmbH (Austria) developed a better understanding for the oxidation behavior inside steels during hot rolling, which could potentially help manufacturers to reduce the amount of steel lost during production. Therefore, adapted process parameters and knowledge about the admissible limits of alloy content would help to prevent negative effects of grain boundary oxidation during further steel processing and in-service properties of HSS car body parts.

Dr. Auinger and his co-researchers analyzed the oxidation behavior of different iron-based alloys. They found that particularly the combinations of iron-manganese and a second alloy addition - representing a simplified version of many high strength steels  - undergo severe oxide formation along grain boundaries if not processed appropriately.

"Isotope exchange experiments verified that grain boundaries in manganese-containing steels are extremely susceptible to oxide formation. On the other hand, oxide particles inside the grains strongly bind their oxygen atoms. It means that new oxygen has to penetrate the entire oxide zone before forming a new oxide particle at the front," Dr. Auinger says. "The reduced depth of internal oxidation is suggested to be caused by lowering the oxygen diffusion due to trapping reactions at crystal imperfections."

Dr. Auinger argues that from a scientific point of view, this work is particularly important, since it indicates not that the oxidation along grain boundaries is enhanced, but that the oxidation of the alloy additions inside the metallic grains is significantly slower than predicted by theoretical simulations. This helps the understanding of the mechanisms of oxide formation. It also may enable inventing novel strategies that could help to prevent unwanted oxidation, which is currently determined by the cooling efficiency after hot rolling.
 

How manganese prevents oxidation in high-strength steel

The University of Warwick, England, announces that a team of researchers has discovered that the amount of oxide that forms at the surface of automotive high-strength steels depends on the ratio between manganese and additional alloying elements.

Continue reading

AK Steel launches advanced high-strength steel for automotive applications


Source:

AK Steel, Westchester, Ohio, launches Nexmet 440EX high-strength steel, which provides improved ductility, strength, and formability for automotive applications. The steel is designed for automotive light-weighting in all types of structural and exterior parts. The products are especially designed to help original equipment manufacturers meet their U.S. Corporate Average Fuel Economy targets for the year 2025.

This new exposed-surface-quality product combines high yield and tensile strength at thinner gauges to facilitate lightweight designs. This results in enhanced performance where surface appearance and dent resistance are critical.  Nexmet 440EX is currently available and is being qualified by automotive OEMs as a steel solution for exposed body panel lightweighting needs.

AK Steel will launch its other next-generation Advanced High Strength Steel (AHSS) products, Nexmet 1000 and 1200, in early 2017, following completion of upgrades at AK Steel's Dearborn Works hot-dip galvanized line.  These AHSS steels will offer significantly improved ductility at tensile strengths of 1000 and 1200 MPa, and will serve to help lightweight automotive body structures. 

www.aksteel.com

 

AK Steel launches advanced high-strength steel for automotive applications

AK Steel, Westchester, Ohio, launches its Nexmet 440EX high-strength steel that provides greater ductility, strength, and formability for automotive applications.

Continue reading

Aleris Aluminum to be acquired by Chinese aluminum extrusion company


Source:

Aleris Corp., Cleveland, Oho, a global aluminum rolled products producer, announces that it has entered into a definitive agreement to be acquired by Zhongwang USA LLC, a Chinese company. The aggregate value of Aleris amounts to $2.33 billion, comprising $1.11 billion in cash for the equity to be paid by Zhongwang USA, plus $1.22 billion in net debt.

The acquisition of Aleris reflects commitment to disciplined operating investments over the long-term by Mr. Liu Zhongwang, the majority owner of Zhongwang USA, in an industry to which he has been committed for two decades.  In addition to his role at Zhongwang USA, Mr. Liu is also the chairman and founder of China Zhongwang, the second largest aluminum extrusions product developer and manufacturer in the world, and the largest in Asia.  With the acquisition of Aleris, Mr. Liu will now oversee companies that have complementary geographic footprints and capabilities.

Aleris will continue to be headquartered in Cleveland, and will be operated as an independent entity. The Aleris management team will remain in place, providing continuity for Aleris employees and customers, and supporting the continued implementation of the Aleris strategy. 

Aleris will retain its name and continue to serve its customers with no changes to current operations, contracts, or commitments.  It will continue with the implementation of all strategic growth projects, including its major expansion project in Lewisport, Kentucky, which will enable Aleris to meet the North American automotive industry's growing demand for aluminum auto body sheet.

The transaction is expected to close in the first quarter of 2017, following the customary regulatory approvals and closing conditions.

Aleris is a privately held, global leader in aluminum rolled products serving diverse industries including aerospace, automotive, building and construction, commercial transportation, and industrial manufacturing.  Headquartered in Cleveland, Ohio, Aleris operates production facilities in North America, Europe and Asia.

www.aleris.com

 

Aleris Aluminum to be acquired by Chinese aluminum extrusion company

Aleris Corp., Cleveland, Oho, a global aluminum rolled products producer, announces that it has entered into a definitive agreement to be acquired by Zhongwang USA LLC, a Chinese company.

Continue reading

CERN heat treating furnace to process niobium-tin superconducting magnets

August 24, 2016
Source:

The European Organization for Nuclear Research (CERN), Geneva, announces that it has received a 105-foot-long furnace for the heat treatment of niobium-tin (Nb3Sn) superconducting coils that will be installed in the Future Circular Collider. The furnace completes the equipment required for the production of superconducting coils, which are needed for the High-Luminosity LHC (HL-LHC) upgrade and future circular colliders.

Superconducting accelerator magnets are key for reaching higher energies and luminosities in particle accelerators.

The HL-LHC upgrade aims for magnetic fields up to 11 Tesla for the dipole magnets, while the Future Circular Collider study explores using magnets with a field of 16 Tesla, almost double the 8.3 Tesla of the superconducting magnets used in the LHC.

To reach these goals new superconducting materials are needed.

"Nb3Sn has been chosen for the next generation of superconducting magnets," says Friedrich Lackner, a project engineer who supervises the coil production for HL-LHC. "The field achieved with this material can reach up to 16 Tesla. The production of such coils is complex, as we must first wind the coils and then carry out the heat treatment that allows the tin and niobium to react and convert to the superconducting Nb3Sn compound."

After the material has undergone this heat treatment, it becomes very brittle, which is why this process is implemented after the winding process—the opposite to magnets in the LHC.

Called GL010000, the furnace will allow the heat treatment of coils up to 36 feet long, and can reach temperatures up to 1650°F, providing a sufficient margin for future challenges.

This treatment involves a two-week process during which the coils are raised to different temperature plateaus up to 1230°F. A special feature is that it is able to raise the coils to such high temperatures completely uniformly throughout the entire furnace, making sure one part does not heat more or less than another.

http://cds.cern.ch/record/2203181

 

CERN heat treating furnace to process niobium-tin superconducting magnets

The European Organization for Nuclear Research (CERN), Geneva, announces that it has received a 105-foot-long furnace for the heat treatment of niobium-tin (Nb3Sn) superconducting coils that will be installed in the Future Circular Collider.

Continue reading

Sinterite custom pusher furnace designed for continuous sintering


Source:

Sinterite, a Gasbarre Furnace Group Company, St. Marys, Pa., has installed a manually operated custom pusher furnace designed for continuous sintering of a range of materials and grades at a facility in Pennsylvania. It consists of two heat control zones and one cooling zone, with a maximum operating temperature of 1800°F.

This particular pusher furnace is unique because of its low operating temperature. Typically, these types of furnaces are designed to operate up to 3000°F. Because of the customer's specialized sintering process and lower temperature requirements, this furnace was customized to meet those unique processing needs.

Sinterite designs, manufactures, and services custom continuous belt and batch furnaces for sintering, brazing, annealing, steam treating, drying and heat treating applications. The installed base of equipment is in excess of 1300 units in more than 47 countries. Sinterite's quality design includes alloy and ceramic muffle systems, powder-handling equipment, custom fabrications, and the exclusively-manufactured HyperCooler sinter-hardening and rapid cooling system.

www.sinterite.com   

 

Sinterite custom pusher furnace designed for continuous sintering

Sinterite, a Gasbarre Furnace Group Company, St. Marys, Pa., has installed a manually operated custom pusher furnace designed for continuous sintering of a range of materials and grades at a facility in Pennsylvania.

Continue reading

Titanium 2016 conference to focus on world demand trends


Source:

The International Titanium Association, Northglenn, Colo., announces that the Titanium 2016 conference and exhibition will focus on the global titanium industry. The event will be held September 25th - 28th at the J.W. Marriott Desert Ridge Golf Resort in Scottsdale, Arizona, providing nearly 1000 attendees with valuable insights, timely information and networking opportunities in the global titanium industry.

The conference will host numerous speaker sessions to address titanium business trends and manufacturing technology innovations, along with presentations by a number of accomplished individuals.  Special guest speakers include Richard Aboulafia, vice president of analysis at the Teal Group; Allan McArtor, the chairman and chief executive officer of Airbus Group Inc.; award-winning author, journalist and international correspondent Robin Wright; American inventor and electrical vehicle pioneer William Morrison (Chip) Yates, who serves as vice president of marketing for Norsk Titanium; and pilot, author and photographer Brian Shul, one of only 93 men in history to fly the legendary, titanium-intensive SR-71 spy plane, the fastest jet ever built.

Henry Seiner will deliver a presentation on "Trends in the Defense Market: A Titanium Perspective," as a member of the World Titanium Industry Demand Trends segment.  Henry will address aerospace, marine and land-based titanium applications and their market drivers. Seiner will frame his remarks in the larger scope of defense budgets and increasing global tensions. China and United States continue to have the world's two largest defense budgets. However, the gap is closing as the U.S. defense budget declined for the fifth consecutive year in a row and its ratio of outspending China has dropped from 10:1 to 3:1 in the last decade. The decline in value of the euro, the ruble and the price of oil has caused a shake-up of ranking for the remaining top 15 military spenders. 

www.titanium.org

 

 

Titanium 2016 conference to focus on world demand trends

The International Titanium Association, Northglenn, Colo., announces that the Titanium 2016 conference and exhibition will focus on the global titanium industry.

Continue reading

Bodycote Ipswich heat treating facility earns MedAccred status


Source:

Bodycote, England, announces that its facility in Ipswich, Mass., has earned MedAccred accreditation, underlining its high standards of quality.

MedAccred, administered by the Performance Review Institute (PRI), is an industry-managed approach to ensuring critical manufacturing process quality throughout the medical device supply chain. It establishes stringent consensus audit criteria based on industry and specific OEM requirements that ensure compliance and quality. Adherence to these requirements leads to greater process discipline, operational efficiency and ongoing improvement which results in higher quality and performance.

Strategically located in New England, Bodycote's plant in Ipswich is fast becoming a center of excellence for the region's medical device and implants market, offering heat treatment services to process and strengthen medical implants, surgical and dental tools, and other medical devices. The plant's close proximity to Bodycote's hot isostatic pressing (HIP) plant in Andover makes it an ideal source for a complete thermal processing solution.

Bodycote continues to invest in new capacity and technology to support opportunities within the growing medical industry for classic heat treatment and HIP,  along with its Specialty Stainless Steel Processes (S3P) in North America. For Bodycote, the benefits of MedAccred to the supplier are evident. The process provides for consistent and standardized critical process audits, which result in fewer redundant onsite audits by multiple OEMs and first tier customers. The MedAccred certification reinforces customer confidence in Bodycote as a premier quality provider of heat treating.

www.bodycote.com

 

Bodycote Ipswich heat treating facility earns MedAccred status

Bodycote, England, announces that its facility in Ipswich, Mass., has earned MedAccred accreditation, underlining its high standards of quality.

Continue reading

One Minute Mentor: Stress Relieving Type 347 Stainless Steel

August 18, 2016
Source:

Although stabilized alloys do not require high-temperature annealing to avoid intergranular corrosion, the stress-relieving temperature exerts an influence on the general corrosion resistance of these alloys.

The graphs show how the percentage of stress relief increases with an increase in stress-relieving temperature for type 347 stainless steel. These data also demonstrate the relative unimportance of holding time.

Volume 4D, Heat Treating of Irons and Steels â‡’ Heat Treated High-Alloy Steels â‡’ Heat Treating of Austenitic and Duplex Stainless Steels â‡’ Stress Relieving 

One Minute Mentor: Stress Relieving Type 347 Stainless Steel

Although stabilized alloys do not require high-temperature annealing to avoid intergranular corrosion, the stress-relieving temperature exerts an influence on the general corrosion resistance of these alloys.