One Minute Mentor: Annealing of Austenitic and Duplex Stainless Steels

August 4, 2016
Source:

The lower carbon content in an austenitic stainless steel slows the kinetics of carbide precipitation. This allows longer time at temperature before the onset of sensitization. The graph shows the Time-Temperature-Sensitization diagram (TTS) for 304 austenitic stainless steel with various amounts of carbon. Decreasing carbon content significantly delays the formation of chromium carbides and the onset of intergranular corrosion. In low-carbon grades, defined as those with carbon content below 0.030%, an exposure of about 8 hours is necessary before sensitization occurs

Carbon content of 0.03% and lower allows short excursions of several hours into the sensitizing temperature range without loss of corrosion resistance. Carbon in austenite can be retained in supersaturation for extended periods of time. This is why austenitic L grades do not sensitize even though they are slightly supersaturated. Sensitization occurs at higher levels of carbon by prolonged heating at 600 to 850°C.

Volume 4D, Heat Treating of Irons and Steels â‡’ Heat Treated High-Alloy Steels â‡’ Heat Treating of Austenitic and Duplex Stainless Steels â‡’ Annealing

One Minute Mentor: Annealing of Austenitic and Duplex Stainless Steels

The lower carbon content in an austenitic stainless steel slows the kinetics of carbide precipitation.

Continue reading

AMG Titanium Alloys to supply titanium aluminides for PW1100G-JM engine

August 3, 2016
Source:

AMG Advanced Metallurgical Group N.V., Amsterdam, announces that AMG Titanium Alloys and Coatings (AMG TAC) has been selected by MTU Aero Engines to provide titanium aluminides for the production of the Pratt & Whitney PurePower PW1100G-JM engine. The value of the long-term supply contract exceeds$40 million.

The TiAl intermetallic combines the heat resistance of nickel alloys with the lightweight characteristics of titanium. AMG's TiAl materials will be used to produce low-pressure turbine blades for the PurePower PW1100G-JM engine for single-aisle aircraft, including the Airbus A320neo.

According to Pratt & Whitney, the ultra-efficient PurePower PW1100G-JM engine delivers double-digit improvements in fuel efficiency, reduces noise by 20 dB, and slashes CO2 and NOX emissions.

To support this next stage of expansion, AMG TAC will invest in new vacuum furnaces supplied by AMG Engineering. The combined value of current and future supply contracts for AMG's TiAl business, across all customers, exceeds $130 million.

www.amg-nv.com

 

AMG Titanium Alloys to supply titanium aluminides for PW1100G-JM engine

AMG Advanced Metallurgical Group N.V, Amsterdam, announces that AMG Titanium Alloys and Coatings (AMG TAC) has been selected by MTU Aero Engines to provide titanium aluminides for the production of the Pratt & Whitney PurePower PW1100G-JM engine.

Continue reading

Laser profile scanner evaluates high-strength steel welds during welding process


Source:

SSAB Steel, Stockholm, announces that its engineers together with researchers from the Royal Institute of Technology have developed a quality assurance method for welds in high-strength steel in which a laser profile scanner assesses the welded surface and measures the quality of the weld. The most revolutionary aspect of this method is that the assessment takes place in real time – online – during the actual welding process.

"This system will provide instant feedback to the welding operator on whether the welded joint fulfills all its requirements," explains Dr. Thomas Stenberg. "If not, the welding robot will be able to adjust the process parameters to ensure that the weld quality complies with the desired result, without needing to disrupt the process or repeat the work."

As Anders Ohlsson, Manager of Joining & Thermal Cutting Technologies at SSAB's Knowledge Service Center explains, the new QA method has the potential to revolutionize the ways in which many of SSAB's customers utilize high-strength steel, opening up opportunities for more applications to benefit from its superior qualities, which include lower component weight and reduced fuel consumption.

"Minimizing the occurrence of failures caused by fatigue will enable us to use HSS in many applications in which they cannot be used today – such as in machines and components that are known to be subject to high stress concentrations. Examples of these applications may include chassis for manufacturing and forestry equipment, trailer chassis and components used in energy production," says Mr. Ohlsson.

According to Dr. Stenberg, who won the 2015 Swedish Steel Prize "University Challenge" award from SSAB for his groundbreaking work on the new QA method, the method will deliver significant benefits to the customers who implement it. 

"Firstly, we expect productivity to increase by about 50% due to increased robot travel speed, coupled with a reduction of up to 30% in the consumption of weld filler material," he says. "It will also allow manufacturers to cut lead times, thanks to the reduced number of inspections, while the need to scrap or rework products will be minimized."

www.ssab.com

 

Laser profile scanner evaluates high-strength steel welds during welding process

The Royal Institute of Technology in Stockholm announces that its researchers have developed a quality assurance method for welds in high-strength steel in which a laser profile scanner assesses the welded surface and measures the quality of the weld.

Continue reading

New graphite board insulation enables more thermally efficient furnace hot zone

August 1, 2016
Source:

Solar Manufacturing, Souderton, Pa., announces that it has been cooperating for the past year with Graphite Machining Inc., Topton, Pa., on the development and testing of a new graphite board material and its application in vacuum furnace hot zones. This new graphite board material has undergone extensive thermal and vacuum testing to prove its improved thermal efficiency and excellent vacuum performance compared to prior and present graphite board designs.

GMI intends to market this new graphite board under the name of Heatguard insulation, while Solar will incorporate this new material into its vacuum furnace hot zones under the trade name of Hefvac (High Efficiency Vacuum).

According to Frank C. Schoch, president of GMI, "After extensive testing against our existing and competitive insulating materials, Solar Manufacturing and Graphite Machining combined our respective experience and created this new thermally efficient graphite board insulation material."

By incorporating Hefvac board insulation, Solar Manufacturing has now developed a proven, more thermally efficient vacuum furnace hot zone design that is capable of achieving faster and better vacuum levels because of the Hefvac sealed and low-moisture-absorption structure.

William R. Jones, CEO of the Solar Atmospheres family of companies notes, "I will be giving a presentation at the 2016 FNA (Furnaces North America) show in Nashville, Tenn., to highlight the testing and comparisons of prior designs to this new board material and to illustrate not only the more thermally efficient aspect of the new material, but also the ease and advantages of its use. Hefvac will be on display at Solar Manufacturing's booth 301-303 with a full size hot zone."

www.solarmfg.com

 

New graphite board insulation enables more thermally efficient furnace hot zone

Solar Manufacturing, Souderton, Pa., announces that it has been cooperating for the past year with Graphite Machining Inc., Topton, Pa., on the development and testing of a new graphite board material and its application in vacuum furnace hot zones.

Continue reading

Buehler upgrades Wilson DiaMet hardness testing software


Source:

Buehler, Lake Bluff, Ill., announces that it has extensively upgraded its Wilson DiaMet hardness testing software with features designed to facilitate and accelerate specific applications, such as the documentation of the hardness distribution in welds, or the depth of hardening in induction-hardened workpieces or in objects hardened with conventional processes. The upgraded  DiaMet software is even more user friendly, and is internationally consistent.

DiaMet is designed for operation under Windows 10, and can interface with Office spreadsheet applications. It fulfills the requirements for industrial hardness measurement in a production-related environment – an application requiring high precision along with a maximum degree of automation in handling extensive test programs.

Designed for operation by mouse or touchscreen, the system offers expert users the required flexibility and broad feature set for planning, running, analyzing, documenting and archiving of individual measurements and measurement series, while at the same time enabling less extensively trained operators to work quickly and efficiently.

DiaMet is optimized for evaluating Macro-Vickers, Micro-Vickers, Knoop, and Brinell indents according to ISO 6507, ISO 4545, ASTM E384, ISO 6506 and ASTM E10. It is designed to work with all models of the current Wilson VH and UH hardness tester series, as well as some legacy systems.

As an international software package offered in multiple languages, the current Wilson DiaMet software addresses all relevant national and international hardness testing standards requirements.

"DiaMet users in global organizations can now share and compare results worldwide – regardless of where the measurements were made," says Marcel van Banning, Product Manager Hardness, Buehler ITW Test & Measurement GmbH. "With this new release, we are providing test engineers with a tool enabling them to supply detailed and reliable results, even when work assignments are time sensitive. In addition, the high degree of automation enables even less trained staff to conduct comprehensive test series and produce highly accurate results." 

The new design of the DiaMet testing software substantially facilitates the process of meeting ISO 9015 and ISO 15614 hardness testing of welds.  The software guides the operator through the setup process by adapting a fixed test pattern to the sample in hand with only a few clicks – strictly in accordance with the standards. The software produces a graphical image of the complete weld, including indent positions and associated measurement values, which can be used in a test report.

ISO 9015 and ISO 15614 describe the test loads, number of indents in the parent material, heat affected zone (HAZ) , distances between each indent and the depth below the surface of the welded joint. Fulfilling these test requirements traditionally requires a time-consuming setup and an experienced operator, not least due to the fact that no two weld samples are completely identical. DiaMet saves time and improves accuracy.

www.buehler.com

 

Buehler upgrades Wilson DiaMet hardness testing software

Buehler, Lake Bluff, Ill., announces that it has extensively upgraded its Wilson DiaMet hardness testing software with features designed to facilitate and accelerate specific applications, such as the documentation of the hardness distribution in welds, or the depth of hardening in induction-hardened workpieces or in objects hardened with conventional processes.

Continue reading

Hardness testers feature high accuracy and deadweight loads from 10 g to 2 kg


Source:

Buehler, Lake Bluff, Ill., introduces two universal hardness testers: the Wilson VH1102 and VH1202, both equipped with the extensively upgraded version of DiaMet software. They offer cost-efficient and reliable solutions for Knoop and Vickers micro-hardness testing in accordance with ISO 6507, 9385, and 4546, or ASTM E384 and E92.

The instruments meet the highest standards in terms of accuracy, and can be used both in quality control and research and development. They feature deadweight loads from 10 g up to 2 kg, and nine different, automatically selectable loading stages. Both models feature an ergonomic, adjustable 7-inch color touchscreen for rapid test method selection and data collection.

The system is highly intuitive and can be operated by less extensively trained staff after a brief period of training. The wide load range with test scales from HV/HK0.01 to HV/HK2 is the same for both models. The usual knob for manual selection of test weights has been replaced by a durable, software-controlled electric motor to automatically change test weights, thereby providing a level of operator convenience that is normally found only on higher-end instruments.

The two models differ with regard to the electrically driven, high-speed, low-noise turret. The VH1102 model is equipped with a turret providing four positions, including an indenter for Knoop or Vickers, and two standard objectives for 10x and 50x magnification at normal working distance.  

The VH1202 model is equipped with a six-position turret, including two indenters for both Knoop and Vickers, and an additional objective with 5x magnification at long working distance. For both models, the turret can be set to the magnification selected on the touch screen by simply pushing the Start button. They can be configured to meet a wide range of requirements, from a stand-alone version for laboratories with a relatively low sample volume, up to a fully equipped system for high sample volumes in an industrial environment.

The system includes the extensively upgraded version of its DiaMet software. Designed for operation by mouse or touchscreen, the system offers expert users the required flexibility and broad feature set for planning, running, analyzing, documenting, and archiving of individual measurements and measurement series. At the same time, the new software enables less extensively trained operators to work quickly and efficiently. The new version contains features designed to facilitate and accelerate specific applications, such as the documentation of the hardness distribution in welds, or the depth of hardening in induction-hardened workpieces, or parts treated with conventional hardening processes.

www.buehler.com

 

Hardness testers feature high accuracy and deadweight loads from 10 g to 2 kg

Buehler, Lake Bluff, Ill., introduces two universal hardness testers: the Wilson VH1102 and VH1202, both equipped with the extensively upgraded version of its DiaMet software.

Continue reading

One Minute Mentor: Metallurgy of Austenitic Stainless Steels

July 29, 2016
Source:

The metallurgy of austenitic stainless steels is based on alloying that enlarges the austenite loop, as shown in the graphs. Additions of carbon expand the austenite loop, as shown in (a). Other elements that expand the loop include nickel, manganese, and nitrogen; while silicon, molybdenum, and titanium have an opposite effect. The actions of these elements shown in (b) form the basis for the microstructure of stainless steels.

Volume 4D, Heat Treating of Irons and Steels â‡’ Heat Treated High-Alloy Steels â‡’ Heat Treating of Austenitic and Duplex Stainless Steels â‡’ Metallurgy

One Minute Mentor: Metallurgy of Austenitic Stainless Steels

The metallurgy of austenitic stainless steels is based on alloying that enlarges the austenite loop, as shown in the graphs.

Continue reading

ASM member Thomas V. Bovalina named new president and CEO of Tenova Core

July 27, 2016
Source:

Tenova Core Inc., Coraopolis, Pa., announces that Thomas V. Bovalina, previously its Chief Operating Officer, has been named Tenova Core's President and CEO. Robert J. Schurko, President and CEO of Tenova Core since April 2010, retired on July 1. The company is a fully owned subsidiary of Tenova S.p.A., Milan, Italy.

Mr. Bovalina has 37 years of steel industry and industrial equipment engineering experience. He has held various positions at the company, beginning in 1988 as a process engineer at LOI Industrial Furnaces Inc., which was subsequently acquired by Tenova in 2006. In his varous roles, he has been responsible for managing several functions, including corporate operations, project management, and sales.

Mr. Bovalina's career began in 1979 at Wheeling Pittsburgh Steel as a Metallurgical Engineer. He holds a B.S. degree in chemistry and a B.A. degree in economics from Washington & Jefferson College. He earned an M.B.A. from Wheeling Jesuit University in 1983. He lives in McMurray, Pa., with his wife Sharon.

www.tenovacore.com

 

ASM member Thomas V. Bovalina named new president and CEO of Tenova Core

Tenova Core Inc., Coraopolis, Pa., announces that Thomas V. Bovalina, previously its Chief Operating Officer, has assumed the position of Tenova Core’s President and CEO.

Continue reading

Asian electronic company selects Harper for elevator furnaces


Source:

Harper International, Buffalo, N.Y., has been selected by a leading Asian electronic components firm for the design of two high-temperature elevator furnaces for its production plant. The furnaces will sinter specialty ferrite materials processed at 3090°F in an oxygen atmosphere.

Harper's Elevator kiln systems were chosen for the high-quality design, engineering, and construction that Harper is known for. The design incorporates superior thermal uniformity and extremely high system up-time, supporting the yield of high quality, finished products.

"Harper's teams of talented engineers continuously strive to meet and exceed customers' goals and expectations. This unique furnace system is another great example of our commitment to providing advanced technologies and tailored solutions," commented Brian Fuller, Sales Manager at Harper International.

www.harperintl.com/technologies

 

Asian electronic company selects Harper for elevator furnaces

Harper International, Buffalo, N.Y., has been selected by a leading Asian electronic components firm for the design of two high-temperature elevator furnaces for its production plant.

Continue reading

Nucor to acquire steel plate mill in Texas


Source:

Nucor Corp., Charlotte, N.C., has agreed to acquire the Joy Global steel plate mill in Longview, Texas, for approximately $29 million. The mill produces carbon and alloy steel plate products with heat-treating capabilities, and has an annual capacity of 180,000 tons. The mill produces specialty plate products with the capability of producing plate that can range from 1 to 12 inches thick and up to 138 inches wide.  

"This acquisition builds on our strategy to capture a growing share of higher value-added plate products, and complements the capabilities of our two existing plate mills," said John Ferriola, Chairman, CEO, and President of Nucor. "The Longview mill will serve as a valuable addition to Nucor's plate products, which we believe can be further leveraged by our Nucor commercial team."

Nucor's existing plate mills are in North Carolina and Alabama, and have a combined capacity of 2.9 million tons per year. Nucor's existing mills produce plate for manufacturers of barges, bridges, heavy equipment, rail cars, refinery tanks, ships, wind towers, armor, and other markets. Nucor plate products are also used in the pipe and tube, pressure vessel, transportation and construction industries.

Nucor and its affiliates are manufacturers of steel products, with operating facilities primarily in the United States and Canada.  Products include carbon and alloy steel  as bars, beams, sheet, and plate; steel pilings; steel joists and joist girders; steel decks; fabricated concrete reinforcing steel; cold-finished steel; steel fasteners; metal building systems; steel grating; and wire and wire mesh.  Nucor, through the David J. Joseph Company, also brokers ferrous and nonferrous metals, pig iron and HBI/DRI; supplies ferro-alloys; and processes ferrous and nonferrous scrap. Nucor is North America's largest recycler.

www.nucor.com

 

Nucor to acquire steel plate mill in Texas

Nucor Corp., Charlotte, N.C., has agreed to acquire the Joy Global steel plate mill in Longview, Texas, for approximately $29 million.

Continue reading