One Minute Mentor: Hardness Gradients in Nitrided High-Speed Tool Steel
March 4, 2016
Source:
The graph shows the effect of bath conditions and immersion time on hardness gradients in Type T1 high-speed tool steel.
It compares the hardness gradients obtained on specimens of T1 high-speed steel nitrided at 565°C (1050°C) for 90 minutes in a new bath and for various lengths of time in an aged bath. Nitriding of decarburized high-speed steel tools should be avoided because it results in a brittle surface condition. For those surfaces that have been softened from grinding, nitriding is frequently employed as an offsetting corrective measure.
Volume 4D, Heat Treating of Irons and Steels ⇒ Tool Steels ⇒ Heat Treating of High-Speed Tool Steels ⇒ Recommended Heat-Treating Procedures
The graph shows the effect of bath conditions and immersion time on hardness gradients in Type T1 high-speed tool steel.
Continue reading
NIST ultrasound method detects cracks in capacitors
March 3, 2016
Source:
The National Institute of Standards and Technology, Gaithersburg, Md., and collaborators have demonstrated a nondestructive acoustic method for detecting cracks in ceramic capacitors before they go bad. The method relies on acoustic measurements at frequencies much higher than humans can hear. Researchers briefly apply an electric field across the electrodes of a capacitor, causing a vibration at a specific frequency. They then measure the decay over time (called ringdown) of the signal. These data are analyzed to determine slight shifts in frequency versus the magnitude of the vibration. These shifts are greater when cracks are present. This nonlinear approach — focusing on frequency shifts relative to signal strength, rather than the frequency shifts alone — is especially useful because it is not affected by slight variations in size of the capacitors.
NIST researchers invented the technique, and the study of crack detection levels was carried out with collaborators from the University of Maryland, NASA Goddard Space Flight Center, and Colorado State University. In the study, the prototype method led to the rejection of more than 90% of sample capacitors with visible cracks. Once further studies quantify and confirm detection levels, the new technique may help prevent failures in medical devices such as cardiac pacemakers and defibrillators, and also avert electronics failures in satellites and other spacecraft. The new method may also detect structural flaws in other types of materials.
The ceramics in the NIST study are highly nonlinear, meaning the capacitors get less stiff and their resonant frequency drops when they vibrate more strongly. The new NIST method measures patterns in how this tone changes over time in relation to the strength of the vibrations.
Researchers measured 41 multilayer barium-titanate ceramic capacitors, each roughly 2 by 3 millimeters in size, before and after heating to high temperatures (189°C) and quenching in ice water. This thermal treatment generated surface-breaking cracks in 27 samples. The nonlinear acoustic results were strongly correlated with the presence of visible cracks: Measurements on 25 of the 27 visibly cracked capacitors yielded results that were outside the range of those for capacitors without cracks.
The study concluded that nonlinear acoustic measurements offer a promising approach for nondestructive detection of cracks in capacitors before electrical failure occurs, and that further work should be pursued to quantify the level of detection. NIST staff are continuing this research in collaboration with a capacitor manufacturer.
www.nist.gov
The National Institute of Standards and Technology, Gaithersburg, Md., and collaborators have demonstrated a nondestructive acoustic method for detecting cracks in ceramic capacitors before they go bad.
Continue reading
3D-printed titanium hip implant features fully porous acetabular cup
Source:
Smith & Nephew, Andover, Mass., introduces its first 3D-printed titanium hip implant, the new Redapt revision acetabular fully porous cup with Conceloc technology. To support bone growth, the 3D manufacturing process will be used to produce an entirely porous implant, one that mimics the structure of cancellous bone.
The company noted that the Conceloc advanced porous titanium technology is an alternative to external porous coatings, such as sintered beads or fiber mesh, used in other uncemented implants. The new Redapt cup has been developed for use in revision cases where compromised bone makes implant fixation and stability more difficult.
"Bringing to market a 3D-printed titanium acetabular cup for difficult revision procedures is just one example of the potential of this remarkable technology," says Smith & Nephew global reconstruction vice-president Mike Donoghue.
Redapt variable-angle locking screws, as well as traditional non-locking screws, work within the implant's geometry to provide both compression and a rigid construct to the acetabular shell. The 3D-printed titanium hip implants are available at selected sites in the United States.
www.smith-nephew.com
Smith & Nephew, Andover, Mass., introduces its first 3D-printed titanium hip implant, the new Redapt revision acetabular fully porous cup with Conceloc technology.
Continue reading
Bonnell Aluminum to invest $18 million in extrusion line for auto structures
March 2, 2016
Source:
Bonnell Aluminum, Newnan, Ga., announces it will invest approximately $18 million over the next year to fund an expansion project that will include the purchase of a new state-of-the-art aluminum extrusion line at its Aacoa facility in Niles, Mich. The new line will include a state-of-the-art 3600-ton extrusion press, housing a nine-inch container, handling systems, and ancillary equipment. Capacity is estimated at approximately 16 million pounds. The project also includes additional floor space to accommodate future value-added fabrication capacity. Planned startup is the second quarter 2017.
Aacoa reportedly has a solid market reputation as a manufacturer, fabricator, and anodizer of aluminum extrusions with operations in Niles, Mich., and Elkhart, Ind. It is said to be highly regarded as a leader in the markets it serves, primarily consumer durables and machinery and equipment. The Niles facility also serves the automotive market due to its regional location.
"With continued growing demand from our customers, it is exciting to invest in this additional capacity, knowing that we will satisfy these opportunities with the high quality products and services that Aacoa is known for in the industry," commented Brook Hamilton, President and General Manager for Bonnell Aluminum.
Bonnell Aluminum is a subsidiary of Tredegar Corp., Richmond, Virginia. The company produces soft and medium-strength alloy aluminum extrusions for building and construction, automotive, machinery and equipment, consumer durables, transportation, electrical and distribution markets. On October 1, 2012, Bonnell Aluminum acquired Aacoa, a world-
www.bonlalum.com
www.aacoa.com
Bonnell Aluminum, Newnan, Ga., announces it will invest approximately $18 million over the next year to fund an expansion project that will include the purchase of a new state-of-the-art aluminum extrusion line at its Aacoa facility in Niles, Michigan.
Continue reading
Solar Atmospheres partners with Pressure Technology for aircraft parts
Source:
Solar Atmospheres, Hermitage, Pa., announces that it now partners with Pressure Technology Inc. (PTI), Concord, Ohio, to provide heat treating of aircraft parts after they have been hot isostatically pressed to high density at the PTI facility. With the escalation of additively manufactured components being printed, and the increased production of engine blade manufacturing to support newer more efficient aircraft, hot isostatic pressing (HIPing) is in more demand for the densification of many materials.
Over the years, Solar Atmospheres and PTI have understood the complementary synergies between the two companies. As an added value service, parts that require heat treat processing after HIP will be picked up by Solar from the PTI facility at no charge.
According to Michael Johnson, Sales Manager for Solar's Hermitage facility, "As both vacuum heat treating and HIPing are gaining popularity, by providing the customer with both state-of-the-art services as one, we can offer quicker turnaround time and savings on shipping costs."
www.solaratm.com
www.pressuretechnology.com
Solar Atmospheres, Hermitage, Pa., announces that it now partners with Pressure Technology Inc. (PTI), Concord, Ohio, to provide heat treating of aircraft parts after they have been hot isostatically pressed to high density at the PTI facility.
Continue reading
Single-flow precision case hardening enables low-distortion gears
Source:
Seco Warwick, Meadville, Pa., introduces the UniCase Master, which is said to provide a single flow, precision case hardening system for low-pressure vacuum carburizing; and 4D high-pressure gas quenching with low distortion for high-volume gear manufacturing.
The UniCase Master system is very flexible, as it can be resized depending on part shape and size, and is not limited to case hardening. It can be adapted for through hardening, brazing, annealing, and other heat treatment processes for in-line production. The system is dedicated to high-volume manufacturing for continuous, automated, single-piece flow, and can be operated with no human intervention. With a part exiting the system at a rate as short as 30 seconds each, customers can experience throughput as high as one million parts per year. This process is ideal for the automotive, transmission, and bearing industry and related industries.
The company also introduces ZeroFlow, a new method of controlled gas nitriding and nitrocarburizing based on nitriding with a single-component atmosphere – raw ammonia (NH3). The nitriding potential Kn is controlled by temporary stop and reactivation of the NH3 feeding into the furnace. Industrial applications to date have shown that the ZeroFlow gas nitriding technology is characterized by much lower consumption and emission of post process gases. The system requires a simpler control system and allows for forming the layer phase structure, while at the same time it delivers even better precision as processes with double-component atmospheres.
www.secowarwick.com
Seco Warwick, Meadville, Pa., introduces the UniCase Master, which is said to provide a single flow, precision case hardening system for low-pressure vacuum carburizing; and 4D high-pressure gas quenching with low distortion for high-volume gear manufacturing.
Continue reading
UTC Aerospace Systems opens $8 million advanced materials laboratory in Connecticut
Source:
UTC Aerospace Systems, Windsor Locks, Conn., has opened an $8 million, 20,000 ft2 state-of-the-art Materials and Process Engineering laboratory to support research, engineering, and production of advanced materials for aerospace applications. Lab capabilities include additive manufacturing to build metal and plastic parts. The lab will develop high-temperature materials such as carbon-carbon and silicon carbide-based composites for applications such as aircraft brakes. The lab will also focus on nanomaterials to develop light-weight metal-matrix and polymer-matrix composites for a variety of applications across UTC Aerospace Systems.
UTC Aerospace Systems also announces establishment of the Materials Engineering Center of Excellence at the University of Connecticut (UCONN). The agreement includes a five-year, million-dollar commitment to work with UCONN in the areas of additive manufacturing, high-temperature composites, thermoplastics, and other advanced materials. UTC Aerospace Systems will provide opportunities to rising UCONN sophomores and juniors to work in the new MPE lab and learn alongside UTC Aerospace Systems engineers and scientists in the areas of materials and manufacturing technologies for future aircraft.
"We are very excited about the new MPE lab, which will transform the way engineers and scientists collaborate to produce innovative solutions using a spectrum of material and manufacturing combinatorial techniques," said Mun Choi, Provost at the University of Connecticut. "The Center of Excellence we've established will provide our students with a unique learning experience by working in the lab with talented engineers."
UTC Aerospace Systems designs, manufactures and services integrated systems and components for the aerospace and defense industries. UTC Aerospace Systems supports a global customer base, with significant worldwide manufacturing and customer service facilities.
www.utc.com
www.utcaerospacesystems.com
UTC Aerospace Systems, Windsor Locks, Conn., has opened an $8 million, 20,000 ft2 state-of-the-art Materials and Process Engineering laboratory to support research, engineering, and production of advanced materials for aerospace applications.
Continue reading
Wilson hardness test system measures very high or very low test loads
February 29, 2016
Source:
Buehler, Lake Bluff., Ill., introduces the Wilson VH3300 Vickers/Knoop hardness test system, which expands the range of automatic these hardness testers with a solution tailored to measurements with very high and/or very low test loads. It provides an extensive variety of scales and magnifications, and provides maximum flexibility for automated hardness testing to ASTM and ISO standards.
It is useful in the test laboratory, in materials and product development, in clean production environments, and in routine quality control. It is ideal for the more advanced heat treatment processes that require hardness testing systems to be durable while maintaining precise control during critical test data generation.
The instrument is equipped with the patent-pending collision protection technology, a high-speed sample stage, and the DiaMet universal testing software. It features a six-position test head with up to three indenters and three zoom objectives, an automated X/Y sample stage available in two sizes (180 mm x 180 mm as standard) and a powerful image analysis system. A wide range of test loads from 5 g to 60 kg (depending on configuration) renders the sturdy system suitable for a wide variety of applications.
A purpose-designed collision protection system helps to avoid accidental damage to the indenters and objectives due to operator errors. The VH3300 hardness testing system provides the ultimate high-capacity testing platform capable of performing 150 make-and-measure indents an hour.
A high-resolution digital camera and long working distance objectives, in combination with innovative, calibrated digital zooming capability, provide up to 2000x magnification. The entire system is controlled through the DiaMet hardness automation software, including setting of test parameters, automated indentation and measuring, acquisition of test data, statistical analysis, data export, and a range of other functions speeding up the test procedure and ensuring high-accuracy acquisition and analysis of test data.
www.buehler.com
Buehler, Lake Bluff., Ill., introduces the Wilson VH3300 Vickers/Knoop hardness test system, which expands the range of automatic Vickers/Knoop hardness testers with a solution tailored to measurements with very high and/or very low test loads.
Continue reading
Keough to Present AFS Honorary Lecture
Source:
John R. (Chip) Keough, FASM, of Applied Process Inc., Ann Arbor, Mich., was selected by the American Foundry Society (AFS) to present the Cast Iron Division Honorary Lecture at its upcoming Metalcasting Congress in April. The lecture was established in 1993 to honor distinguished members of AFS who have contributed to the knowledge base of cast iron. Keough was selected by the leadership of the Cast Iron Division Programs and Papers Committee to present the invited lecture. Past talks have been delivered by both metal casting professors and industry leaders. Keough's lecture, entitled "The Stuff Matters," will take place on April 17 at the AFS Metalcasting Congress in Minneapolis. Keough is director of the technologies division at Applied Process Inc. and also serves as ASM board liaison on the ASM Heat Treating Society Board.
For more information, visit afsinc.org.
John R. (Chip) Keough, FASM, of Applied Process Inc., Ann Arbor, Mich., was selected by the American Foundry Society (AFS) to present the Cast Iron Division Honorary Lecture at its upcoming Metalcasting Congress in April.
Continue reading
One Minute Mentor: Tempering Tool Steels
February 26, 2016
Source:
As shown in the graph for an M2 steel austenitized at 2225°F, the hardness of high-speed steel is directly affected by tempering temperature and time. From the slopes of the curves, it can be seen that M2 undergoes secondary hardening at temperatures above approximately 700°F, and that secondary hardening proceeds at higher temperatures up to about 1100°F, depending on time at temperature.
These temperatures approximate the practical limits for most tempering operations; lower temperatures do not evoke the secondary hardening response, and higher temperatures produce hardness considerably lower than usually desired.
Volume 4D, Heat Treating of Irons and Steels -> Tool Steels -> Heat Treating of High-Speed Tool Steels -> Recommended Heat-Treating Procedures
As shown in the graph for an M2 steel austenitized at 2225°F, the hardness of high-speed steel is directly affected by tempering temperature and time.
Continue reading