Femtosecond lasers make metals superhydrophobic


Source:

Scientists at the University of Rochester, N.Y., have reportedly transformed platinum, titanium, and brass into superhydrophobic materials with femtosecond laser pulses. Superhydrophobicity makes a surface rust-resistant, anti-icing, and anti-biofouling, all of which could help make such devices more robust and easier to maintain. The superhydrophobic surfaces can also clean themselves, since water droplets repelled from the surface carry away dust particles very efficiently. 

This work builds on earlier research by the team in which they used a similar laser-patterning technique that turned metals black. Dr. Guo states that using this technique they can create multifunctional surfaces that are not only super-hydrophobic, but also highly absorbent optically.

"This is the first time that a multifunctional metal surface is created by lasers that is superhydrophobic, self-cleaning, and highly light absorptive," said Chunlei Guo, a physicist at the Institute of Optics at the University of Rochester. He made the new surfaces with his colleague and fellow University of Rochester researcher Anatoliy Vorobyev. The researchers describe the laser-patterned surfaces in an article, "Multifunctional surfaces produced by femtosecond laser pulses." It was published in the Journal of Applied Physics on January 20, 2015 (DOI: 10.1063/1.4905616). It can be accessed at: http://scitation.aip.org/content/aip/journal/jap/117/3/10.1063/1.4905616.

Dr. Guo says that one of the big advantages of his team's process is that "the structures created by our laser on the metals are intrinsically part of the material surface." That means they won't rub off. And it is these patterns that make the metals repel water.

The team is now planning on focusing on increasing the speed of patterning the surfaces with the laser, as well as studying how to expand this technique to other materials such as semiconductors or dielectrics, opening up the possibility of water repellent electronics.

www.rochester.edu

 

Femtosecond lasers make metals superhydrophobic

Scientists at the University of Rochester, N.Y., have reportedly transformed platinum, titanium, and brass into superhydrophobic materials with femtosecond laser pulses.

Continue reading

Solar Atmospheres installs 1500-sq.-ft. climate-controlled room


Source:

Solar Atmospheres, Souderton, Pa., has installed a new 1500 ft2 room in its shop that incorporates temperature and humidity controls, as well as a slight positive pressure environment.  Adjacent to the room is a new state-of-the-art, all-metal hot-zone vacuum furnace, in which only the door protrudes through the wall. The furnace has the ability to isolate the quench system during the heat cycle, and features an all stainless-steel chamber and an oversize pumping system.

The furnace is capable of maintaining a vacuum level of 5x10-6 torr or lower, and has successfully processed sensitive materials unshielded without any surface contamination. 

Early in 2015, an existing furnace will be modified and updated with state-of-the-art controls and added to this new area as well. Currently two laboratory furnaces also reside within the room, bringing the total number of furnaces in the area to four.

This new climate-controlled room will lower the risk of discoloration and foreign object debris,  and will save time by eliminating  the need to shield parts during heat treating. 

 www.solaratm.com

 

Solar Atmospheres installs 1500-sq.-ft. climate-controlled room

Solar Atmospheres, Souderton, Pa., has installed a new 1500 ft2 room in its shop that incorporates temperature and humidity controls, as well as a slight positive pressure environment.

Continue reading

Constellium supplies high-strength aluminum structural parts to Ford F-150

January 20, 2015
Source:

Constellium N.V., Amsterdam, provides  Ford Motor Co. with aluminum structural parts for the Ford F-150 pickup truck in which high-strength, military-grade aluminum alloys are the primary build materials. Constellium is one of Ford's largest suppliers of these components for the F-150. To keep pace with increased demand, Constellium has doubled manufacturing capacity at its facility in Van Buren, Michigan.

The 2015 Ford F-150 delivers the industry's best towing and payload capability among full-size light-duty pickups, enabled by reducing up to 700 pounds of weight through the use of high-strength steel in the frame and aluminum alloys in the body.

"We are delighted to become one of Ford's largest supplier of high-strength aluminum structural parts for the groundbreaking F-150,  and we see this as an important milestone in the expansion of our global automotive structures business," said Paul Warton, President of Constellium's Automotive Structures and Industry business unit.

"We believe that the automotive industry demand for aluminum will continue to grow as automakers seek to reduce vehicle weight and improve fuel efficiency. With our innovative and value-added solutions and the expansion of our component manufacturing capabilities in the United States, Europe, and China, Constellium is strongly positioned to help meet that demand worldwide." 

www.constellium.com

 

Constellium supplies high-strength aluminum structural parts to Ford F-150

Constellium N.V., Amsterdam, provides Ford Motor Co. with aluminum structural parts for the Ford F-150 pickup truck in which high-strength, military-grade aluminum alloys are the primary build materials.

Continue reading

Bruker TriboLab’s modular platform enables a variety of tribology tests


Source:

Bruker, Tucson, Ariz., has release the UMT TriboLab, the latest generation of the Universal Mechanical Tester (UMT) platform. TriboLab incorporates into a single, modular platform the full range of performance previously offered in several UMT models. It provides increased load capacity and higher torques, all with greater ease of use and less training required.

As with previous UMT models, the UMT TriboLab has a universal base that can be equipped with a range of drive modules to allow multiple, different tribology tests to be performed on one platform. The design of the new TriboLab emphasizes ease-of-use due to a tool-less drive exchange, and easier software and scripting capabilities. It offers higher performance in areas such as speed, torque, and data accuracy. The redesign of the product also offers enhanced modularity while simplifying configuration requirements.

Its TriboID feature automatically recognizes the attached modules, and reconfigures user menus based on the hardware installed. The system's new TriboScript software is controlled entirely through a user-friendly graphical interface, enabling even complex scripts to be created simply by dragging and dropping icons. The launch of the UMT TriboLab system also introduces a new line of dual-axis, Gold-Series force sensors with an ultralow noise floor and optional increased frequency response.

Michael Khonsari, the Dow Chemical Endowed Chair and Professor and Director of the Center for Rotating Machinery (CeRoM) at the Department of Mechanical Engineering at Louisiana State University in Baton Rouge, Louisiana, added: "It is exciting to see a new generation of Bruker UMT coming to the market as we have several of its predecessors in our Center, and rely on them heavily. We are actively involved in collaborative projects with industry partners. Having the Bruker UMT in our Center enables us to perform various tribological tests precisely and efficiently, giving us confidence in reporting our results in archival journals."

www.bruker-nano.com

 

Bruker TriboLab’s modular platform enables a variety of tribology tests

Bruker, Tucson, Ariz., has release the UMT TriboLab, the latest generation of the Universal Mechanical Tester (UMT) platform.

Continue reading

Wall Colmonoy announces Modern Furnace Brazing School sessions


Source:

Wall Colmonoy, Madison Heights, Mich., offers a spring session of Modern Furnace Brazing School May 5 to 7 at the Aerobraze Engineered Technologies Brazing Engineering Center in Cincinnati. Engineers, technicians, quality managers, production managers, and others will participate in "hands-on" practical applications while learning about brazing technology from the industry's leading brazing engineers.

For over 60 years, Wall Colmonoy engineers have been gaining practical experience on actual problems in brazing plants around the world. This three-day seminar offers knowledge and practical applications on:

Brazing Design

Metallurgical Aspects / Brazing Operation

Brazing Atmosphere and Furnace Equipment

Brazing Material Selection and Applications

Quality Control

The school preserves the tradition originated by the late Robert Peaslee, a brazing pioneer who invented the first nickel-based brazing filler metal. Unlike other classroom-only seminars, Brazing School attendees will tour the facility and see the actual brazing application on the shop floor. They will also have the opportunity to apply different forms of filler metal to supplied samples, have them vacuum brazed and discuss the outcomes. Wall Colmonoy's Leading Brazing Engineers have the technical know-how and practical experience to guide attendees through the brazing process from beginning to end production.

For seminar details and registration information, contact Jim Nicoll, Marketing Associate, at [email protected] or 248.585.6400, ext. 233.

www.wallcolmonoy.com

 

Wall Colmonoy announces Modern Furnace Brazing School sessions

Wall Colmonoy, Madison Heights, Mich., offers a spring session of Modern Furnace Brazing School on May 5-7 at the Aerobraze Engineered Technologies Brazing Engineering Center in Cincinnati, Ohio.

Continue reading

EFD Induction offers four-cylinder crankshaft hardening machine

January 14, 2015
Source:

EFD Induction India will be displaying a crankshaft hardening machine model at the IMTEX show to be held January 22-28 in Bangalore. The show, officially known as the Indian Metalcutting Machine Tool Exhibition, is the largest event of its kind to be held in South and Southeast Asia. EFD Induction will be positioned in Hall 1A, Stand B106.

Each crankshaft hardening system is packed with features to help ensure optimum hardening results at minimal cost. The equipment on display is a miniature model of a recently delivered four-cylinder crankshaft machine. The system was equipped with five power sources, a hardening and tempering station, and an advanced PLC solution with real-time monitoring features.

As one of the world's largest induction heating companies, EFD Induction has a long-established presence in India and Asia. It has a major manufacturing facility in Bangalore. The Bangalore center plays a key manufacturing role for EFD Induction, supplying other factories with parts for further assembly. The center also designs and builds complete industrial induction heating systems for customers worldwide.

www.efd-induction.com

 

EFD Induction offers four-cylinder crankshaft hardening machine

EFD Induction India will be displaying a crankshaft hardening machine model at the IMTEX show to be held January 22-28 in Bangalore.

Continue reading

J.L. Becker installs car bottom furnace with duplicate combustion and control systems


Source:

J.L. Becker, a Gasbarre Furnace Group Company, Plymouth, Mich., has installed two similar furnace systems for a domestic alloy manufacturer. One is a retrofit of an existing 6 x 32 x 3 ft. car bottom furnace with a complete insulation reline, upgraded pulse-fired combustion system with self-recuperative burners, and upgraded furnace controls with data logging.  The other is a new 55,000 lb., 6 x 32 x 3 ft. car bottom furnace with duplicate combustion and control systems.  Operating temperatures of both furnaces range from 900 to 2000°F, and comply with AMS-2750E specifications.

J.L. Becker designs, manufactures and services industrial atmosphere heat treating equipment, specializing in Tip Up, Car Bottom, and Large Batch Furnace Systems. It has been delivering custom solutions to the heat treating industry for over 40 years.

www.jlbecker.com

www.gasbarrefurnacegroup.com

 

 

J.L. Becker installs car bottom furnace with duplicate combustion and control systems

J.L. Becker, a Gasbarre Furnace Group Company, Plymouth, Mich., has installed two similar furnace systems for a domestic alloy manufacturer.

Continue reading

Nanovea automated indentation technology eliminates user error


Source:

Nanovea, Irvine, Calif., announces the M3 hardness tester with automated indentation technology. It combines automated controlled load and depth, nano- through micro-range (ASTM E2546), and a competitive price to compete in the $20K market. The indentation method has been fully automated, with no need to visually observe the indent. This eliminates user error or problems with image recognition software that may have issues with material color and texture.

The M3 introduces an entirely new user capability within this price range, providing affordable access to quick and easy nanoindentation results under the  ASTM standard. It offers next- generation technology to replace the traditional Visual Micro Vickers Hardness Testers that have not changed in more than 15 years. Also, this new technology can achieve lower load and will work on thin coatings and all ranges of materials including ceramics, polymers, metals and others.

The fully automated system has a touch screen start that gives automatic average of multiple measurements in minutes. The unit is compact and fully contained with only one standard electrical cable to connect. Input function includes load, creep time, and material type. Output function includes hardness, Young's modulus, and creep depth.

www.nanovea.com

 

Nanovea automated indentation technology eliminates user error

Nanovea, Irvine, Calif., announces the M3 hardness tester with automated indentation technology.

Continue reading