Boston Metal raises $20M to scale up molten oxide electrolysis production of ferroalloys
January 17, 2019
Source:
Boston Metal announces that it has raised $20 million in a Series A funding round to accelerate the first industrial-scale deployments of its molten oxide electrolysis (MOE) technology for the production of ferroalloys. The new funding also supports the continued scale-up of MOE for the production of emissions-free steel.
Molten oxide electrolysis is a process in which electricity transforms metal from its raw oxide form into molten metal products. The MOE process was invented on the lab-scale at MIT, and Boston Metal has since scaled up the technology by a factor of over 1000.
At the heart of the MOE cell is a soup of molten oxides tailored for each specific feedstock and product. Electrons act to melt this soup and selectively reduce the targeted oxide. The resulting metal gathers in pools at the bottom of the cell and is tapped by drilling into the cell in a process adapted from the blast furnace. The tap hole is then plugged and the process continues. The inherent modularity of these MOE cells provides the metal industry with a capital-efficient means of adding production capacity.
“Molten oxide electrolysis is a platform technology that can produce a wide array of metals and alloys,†says Tadeu Carneiro, CEO of Boston Metal, “but our first industrial deployments will target the ferroalloys on the path to our ultimate goal of steel. Boston Metal’s MOE technology will offer the steel industry a modular, low-cost, and zero-emissions solution for the production of high-tonnage steel.â€
Boston Metal operates a fleet of semi-industrial MOE systems at its headquarters outside of Boston, and will be commissioning its first industrial systems at this same facility. Boston Metal works closely with customers and partners to tailor the MOE platform for pecific feedstocks and products.
www.bostonmetal.com
Boston Metal announces that it has raised $20 million in a Series A funding round to accelerate the first industrial-scale deployments of its molten oxide electrolysis (MOE) technology for the production of ferroalloys.
Continue reading
Optomec partners with Phillips Federal to bring 3D printing to US government agencies
Source: ASM International
Optomec, Albuquerque, N.M., has signed a partnership agreement with Phillips Federal that will enable Phillips to resell the Optomec Laser Engineered Net Shaping (LENS) systems to U.S. government facilities.
Continue reading
Nucor to invest $1.35 billion to build state-of-the-art steel plate mill in the Midwest
Source:
Nucor Corp., Charlotte, N.C., announces plans to invest $1.35 billion to build a state-of-the-art plate mill in the United States Midwest that will be capable of producing 1.2 million tons per year of steel plate products. The mill is expected to be fully operational in 2022, and is expected to create approximately 400 full-time jobs.
The new plate mill will produce cut-to-length, coiled, heat-treated, and discrete plate ranging from 60 to 160 inches wide, and in gauges from 3/16 of an inch to 14 inches in thickness, enabling Nucor to supply plate products that the company does not currently offer. Nucor currently operates plate mills in North Carolina, Alabama, and Texas.
"This investment is consistent with our drive to continue delivering sustainable, profitable growth and superior returns for shareholders," said John Ferriola, Chairman, CEO & President of Nucor. "Together with the significant share repurchases completed in 2018, the Board's decision to fund this high-return opportunity demonstrates our commitment to balanced capital allocation. We have a strong foundation to build upon as we advance our goal of leading in every market in which we compete."
According to Leon Topalian, Executive Vice President of Beam and Plate products, "By building this state-of-the-art plate mill in the Midwest – the largest plate-consuming area in the United States – we will enhance our ability to serve our customers in the region while also furthering our goal of meeting all the steel needs of our customers around the country. We expect to select a site for the new mill early this year. Our team is poised and ready to take the next step in advancing our position in steel plate products."
"This administration is taking the decisive and meaningful actions that American manufacturers need to compete on a level playing field," Mr. Ferriola said. "Tax reform, continued improvements to our regulatory approach, and strong trade enforcement are giving businesses like ours the confidence to make long-term capital investments here in the United States that create jobs and ensure our success for decades to come."
www.nucor.com
Nucor Corp., Charlotte, N.C., announces plans to invest $1.35 billion to build a state-of-the-art plate mill in the United States Midwest that will be capable of producing 1.2 million tons per year of steel plate products.
Continue reading
One-Minute Mentor: Processing sequence for austempered ductile iron
January 10, 2019
Source:
The figure shows an isothermal transformation (IT) diagram for a ductile cast iron, together with a processing sequence depicting the production of ADI. In this process, austenitizing is followed by rapid quenching (usually in molten salt) to an intermediate temperature range for a time that allows the unique metastable carbon-rich (~2% C) austenitic matrix (γH) to evolve simultaneously with nucleation and growth of a platelike ferrite (α) or of ferrite plus carbide, depending on the austempering temperature and time at temperature.
This austempering reaction progresses to a point at which the entire matrix has been transformed to the metastable product (stage I in the figure). Then that product is “frozen in†by cooling to room temperature before the true bainitic ferrite plus carbide phases can appear (stage II).
In ductile cast irons the presence of 2 to 3 wt% Si prevents the rapid formation of iron carbide (Fe3C). Hence the carbon rejected during ferrite formation in the first stage of the reaction (stage I) enters the matrix austenite, enriching it and stabilizing it thermally to prevent martensite formation upon subsequent cooling.
Thus the processing sequence shows that the austempering reaction is terminated before stage II begins, and illustrates the decrease in the martensite start (Ms) and martensite finish (Mf) temperatures as γH forms in stage I. The kinetics of stages I and II have been described in detail in the literature.
Typical austempering times range from 1 to 4 hours. If the part is austempered too long, undesirable bainite will form. Unlike steel, bainite in cast iron microstructures exhibits lower toughness and ductility.
Volume 4D, Heat Treating of Irons and Steels -> Heat Treatiment of Cast Irons -> -> Heat Treating and Properties of Ductile Iron -> General Characteristics
The figure shows an isothermal transformation (IT) diagram for a ductile cast iron, together with a processing sequence depicting the production of ADI.
Continue reading
ASM member Julien Noel named Vice President/General Manager of Buehler
January 8, 2019
Source:
ITW Test and Measurement Group President Yahya Gharagozlou has named ASM member Julien Noel Vice President/General Manager of its Buehler worldwide division. Buehler, Lake Bluff, Ill., is an ITW company and a premier manufacturer of scientific equipment and consumables for materials analysis.
Julien Noel has been at Buehler since 2015, where he most recently served as the Americas Commercial Director in addition to Global Director of Strategy and Innovation. Noel came to ITW during the acquisition of North Star Imaging in 2010. There he held several leadership roles including General Manager of Europe, Product Management and Business Development. Prior to that, he was Business Manager for Digisens and Professor at the Grenoble School of Management in France. He replaces Meredith Platt, who has been transferred to ITW's Automotive segment and is taking up the role of Vice President/General Manager for a global automotive division -- Seats, Safety, and Motion.
“I am excited to take on this crucial leadership role for Buehler,†says Mr. Noel. "During the last few years we developed successful new products, streamlined online shopping, and improved our customer care/service offerings. I look forward to leading the charge and continuing on the path to create superior products.â€
www.buehler.com
ITW Test and Measurement Group President Yahya Gharagozlou has named ASM member Julien Noel Vice President/General Manager of its Buehler worldwide division.
Continue reading
Solar installs 100-ton vacuum hot press heat treating system with gas fan quench cooling
Source:
Solar Manufacturing Inc., Souderton, Pa., announces that it has completed the installation and startup of a large 100-ton-force vacuum hot press that is capable of treating a 4000-pound part for Refrac Systems’ commercial and aerospace diffusion-bonding operation in Chandler, Arizona. The system includes a two-bar gas fan quench.
Working with Solar’s engineering team, Refrac Systems selected a derivative of the Solar Manufacturing standard HLF-5748-2IQ internally quenched two-bar vacuum furnace as the base design. The furnace hot zone was modified to contain a 100-ton load hydraulic ram centered over the zone, which is configured to diffusion bond parts up to 36 inches wide x 48 inches long x 30 inches tall. The system was specifically designed to diffusion bond large plastic injection molding dies, while concurrently quench hardening them. In addition, the system is finding applications in bonding advanced superalloy heat exchangers, for which the quench cooling offers significant improvement in performance.
According to Norm Hubele, President of Refrac Systems, “We really drew on the extensive engineering experience base that Solar Manufacturing has for building large gas fan quench-cooled vacuum furnaces coupled with our own vacuum hot-pressing experience to build this very unique hot-press system.â€
During the course of system design and development, a number of new and complex engineering solutions were needed to reduce the operational and ownership risks for the new type of furnace system.
William Jones, CEO of the Solar Atmospheres family of companies, notes that “Norm put together a team of engineers to design and build this state-of-the-art GFQVHP, and it contains many innovations. Throughout the entire process, Norm personally reviewed all aspects of the design and added considerable insight to the development of this unique vacuum furnace system.â€
Solar Manufacturing designs and manufactures a wide variety of vacuum heat treating, sintering and brazing furnaces, and offers replacement hot zones, spare parts, and professional service.
www.solarmfg.com
www.refrac.com
Solar Manufacturing Inc., Souderton, Pa., announces that it has completed the installation and startup of a large 100-ton-force vacuum hot press that is capable of treating a 4000-pound part for Refrac Systems’ commercial and aerospace diffusion-bonding operation in Chandler, Arizona.
Continue reading
Wisconsin Oven ships mix of custom and standard ovens in 2018 to many industries
Source:
Wisconsin Oven, East Troy, reports that 2018 was another year of strong growth, as the company shipped 224 pieces of equipment to customers in industries such as composites, aerospace, technology, and automotive.
This equipment included a mix of custom and standard batch and conveyor ovens that were used for curing composites, treating aluminum castings, post curing refractory material, and stress relieving automotive springs. This year the Wisconsin Oven team installed the world’s largest composite cure oven, a significant accomplishment in the drive to be the leading supplier of composite curing ovens in the world.
Dave Strand, President, and CEO, had been noticing for years the need for more skilled trades workers in the job market, and in 2018 made his dream of Wisconsin Oven Universal Training Center (WOC-U) a reality. At the new WOC-U center, experienced Wisconsin Oven production personnel and engineers provide specialized training to help prepare the workforce of the future. The students are paid during their training and many are hired to full time upon graduation.
www.wisoven.com
Wisconsin Oven, East Troy, reports that 2018 was another strong year of growth, as the company shipped 224 pieces of equipment to customers in industries such as composites, aerospace, technology, and automotive.
Continue reading
Lindberg ships 130 heat treating systems to automotive, aerospace, and other industries
Source:
Lindberg MPH, Riverside, Mich., reports that in 2018 the company shipped a total of 130 units to companies in industries such as automotive, aerospace, foundry, electronics, R&D, oil & gas, and technology. Some examples of applications include soldering parts for computers, casting parts for recreational vehicles, and stress relieving drill heads for the oil & gas industry.
"Our strategic growth plan has been paying off, as we realized significant growth in equipment orders,†says Steve Kempowski, President, Lindberg/MPH. “We have added many jobs to our work force to support our growth. As we continue to execute our growth initiatives, we expect 2019 to be another very good year.â€-
www.lindbergmph.com
Lindberg MPH, Riverside, Mich., reports that in 2018 the company shipped a total of 130 units to companies in industries such as automotive, aerospace, foundry, electronics, R&D, oil & gas, and technology.
Continue reading
Contour Hardening acquires gas nitride induction system to heat treat complex parts
Source:
Contour Hardening, Indianapolis, announces the purchase of a gas nitride unit that will help Contour expand its offerings in the automotive sector and expand more deeply into the aerospace market. Contour will install the first unit at its global headquarters in Indianapolis, in late spring 2019.
Since its founding in 1986, Contour has both manufactured induction heat treat systems and offered commercial induction processing services for industry partners around the globe. The new gas nitride unit allows Contour to expand services focusing on distortion-critical, complex parts for clients. With the addition of nitriding, it allows increased offerings to solve complex parts demanding dimensional control through engineered processes.
“Our customers rely on our controlled heat-treatment processes, 100% hardness verification, and dimensional inspections,†says Neil Merrell, Director-Heat Treat.. “Our goal is to drive out part variation and provide a repeatable dimensionally accurate part.â€
“For several years we have planned to have a more significant presence in the aerospace, agricultural, heavy truck and light automotive industries,†says Ben Crawford, Contour CEO and President. “The purchase of this gas nitride unit will allow us to do just that, and complement our induction and dimensional services. We are committed to offering innovative thermal heat treat solutions to our clients globally, and this investment is proof of our commitment.â€
www.contourhardening.com)
Contour Hardening, Indianapolis, announces the purchase of a gas nitride unit that will help Contour expand its offerings in the automotive sector and expand more deeply into the aerospace market.
Continue reading
AK Steel uses neutron spallation source at Oak Ridge to improve manufacture of AHSS
January 3, 2019
Source:
AK Steel Corp., West Chester, Ohio, accepted an award of up to $1.2 million last October from the U.S. Department of Energy under the Office of Energy Efficiency and Renewable Energy’s Advanced Manufacturing Office program to investigate novel low-density steels that could ultimately be used in automotive structural applications.
Specifically, scientists from AK Steel are using neutrons at Oak Ridge National Laboratory's Spallation Neutron Source (SNS) to discover how different manufacturing processes affect the performance of the company's new advanced high-strength steel (AHSS), called Nexmet 1000. Neutrons, unlike electrons or X-rays, are highly penetrating, nondestructive, and sensitive to lighter elements, making them an ideal probe for this novel category of steel materials.
"The Vulcan instrument at the SNS provides information about the crystal structure of AHSS during different stages of the stamping process that we cannot get anywhere else in the United States," said Wei Wu of AK Steel. "This data will be vital to improving our manufacturing methods and will make it easier to quickly identify the best new materials to blend with Nexmet 1000 to produce lighter, safer, and more durable automotive components."
The three-year project is being conducted in collaboration with Oak Ridge National Laboratory Materials Science and Technology Division, and the Advanced Steel Processing and Products Research Center in the Department of Metallurgical & Materials Engineering at the Colorado School of Mines.
The objective of the project is to conduct alloy design, laboratory validation, and testing of low density steels that are alternatives to currently available advanced high strength steels and other lightweight metals. These low density steels are expected to generate energy savings by bringing efficiencies in manufacturing and lifetime savings in automotive structural applications.
www.aksteel.com
AK Steel Corp., West Chester, Ohio, accepted an award of up to $1.2 million last October from the U.S. Department of Energy under the Office of Energy Efficiency and Renewable Energy’s Advanced Manufacturing Office program to investigate novel low-density steels that could ultimately be used in automotive structural applications.
Continue reading