One Minute Mentor: Maps of Wear Resistance

November 27, 2017
Source: ASM International

One Minute Mentor: Maps of Wear Resistance

The images show wear maps for (a) treated and (b) nontreated 316 stainless steel. The T316 stainless steel was treated by low-temperature carburization.

Continue reading

Novelis Advanz automotive aluminum is heat-treatable, formable, and strong

November 20, 2017
Source: ASM International

Novelis Advanz automotive aluminum is heat-treatable, formable, and strong

Novelis, Atlanta, announces that its Advanz 6HF – e/s200 heat-treatable aluminum alloy provides automakers greater design flexibility due to its superior formability, strength, and weight savings for automotive outer and inner applications.

Continue reading

Improving the Nitriding Process Using ZeroFlow® Gas Nitriding Technology

November 14, 2017
Source: ASM International

Improving the Nitriding Process Using ZeroFlow® Gas Nitriding Technology

Gas nitriding has been performed for almost a century with many variations over the years. The benefits of nitriding are well documented and nitriding has gained amazing industrial acceptance. However, the equipment and control of the nitrided layer has continued to be challenging, and as such, nitriding is still slowly being adopted by industry, but the rate of change is improving.

Continue reading

One Minute Mentor: Fatigue Testing of 316 Stainless Steel Round Bar

November 13, 2017
Source: ASM International

One Minute Mentor: Fatigue Testing of 316 Stainless Steel Round Bar

The graph shows the results of fatigue testing of standard round bar 316 stainless steel specimens, in tension-compression cycling (R = –1) The symbols represent different sets of specimens, with nontreated specimens identified by triangles, treated specimens by squares.

Continue reading