Lindberg MPH box furnace can provide six different heat treating atmospheres

August 1, 2017
Source:

Lindberg MPH, Riverside, Mich., has shipped an electrically heated, rod over-bend atmosphere box furnace capable of providing six different atmospheres to a company in the steel and mining industry. This is the second heat treating furnace of this kind that the customer has purchased, and the design is tailored for the customer's specific process.

The atmosphere system includes flow meters for nitrogen, hydrogen, argon, carbon monoxide, and carbon dioxide. An atmosphere saturator allows variation of the moisture dew point of the nitrogen that flows to the furnace chamber. The saturator tank is fabricated of 304 stainless steel. The dew point is controlled from a dew-point transmitter located in the nitrogen atmosphere line before entering the furnace chamber. Dew point is also monitored through a sample port located in the side of the furnace chamber. Maximum load capacity is 465 pounds at 2000°F.

The atmosphere box furnace has work chamber dimensions of 15x30x12 inches, and has a maximum temperature rating of 2000°F. The furnace is constructed with a gas-tight steel shell made from continuous-welded steel plate reinforced with structural steel members. The furnace door lifts up to provide access to the work chamber, and is sealed by metal to metal contact to eliminate gasket wear and maintenance.

The door is raised and lowered by an air cylinder with roller chain. A natural-gas flame curtain is provided for the door area, and is activated when the front door is opened to ignite exiting combustible atmosphere and minimize air infiltration back into the purge chamber. The furnace chamber is heated with a radiant heating system.

Six different atmospheres are available, including nitrogen, hydrogen, endothermic, argon, carbon monoxide, and carbon dioxide.

"At Lindberg MPH, we pride ourselves on having the experience to design our equipment to meet the most stringent requirements," says Kelley Shreve, Sales Representative. "This customer's process required the furnace to provide six different gas atmospheres. This is the second system we have shipped to them with this advanced atmosphere system."

www.lindbergmph.com

 

Lindberg MPH box furnace can provide six different heat treating atmospheres

Lindberg MPH, Riverside, Mich., has shipped an electrically heated rod over-bend atmosphere box furnace capable of providing six different atmospheres, to a company in the steel and mining industry.

Continue reading

Wisconsin Oven enhanced-duty walk-in ovens will dry sand cores for casting in two hours


Source:

Wisconsin Oven Corp., East Troy, Wis., has shipped two natural-gas-fired enhanced-duty walk-in batch ovens that are designed to dry the sand cores used in the casting of a variety of parts. The sand-core dryers have the capability to raise the temperature from 70 to 450°F, driving water and resin from 6000 pounds of sand cores and a 600-pound steel load car within two hours.

Work chamber dimensions are 10x8x20 inches, with a maximum temperature rating of 500°F. Guaranteed temperature uniformity of ±10°F at 500°F was documented with a nine-point temperature survey. The oven bodies are constructed of tongue-and-groove panel assemblies featuring Wisconsin Oven's patented high-efficiency panel seams that provide 25% better insulating efficiency.

"These sand core dryers were designed to maximize efficiency and decrease drying time of the cores," says David Burke, Sales Representative, Torrid Enterprises. "The customer is able to pour and dry more cores in less time than before, resulting in increased production."

The dryers were fully factory tested and adjusted prior to shipment. All safety interlocks were checked for proper operation and the equipment was operated at the normal and maximum operating temperatures. An extensive quality assurance check list was completed to ensure the equipment met all Wisconsin Oven quality standards.

www.wisoven.com

 

Wisconsin Oven enhanced-duty walk-in ovens will dry sand cores for casting in two hours

Wisconsin Oven Corp., East Troy, Wis., has shipped two natural-gas-fired enhanced-duty walk-in batch ovens that are designed to dry the sand cores used in the casting of a variety of parts.

Continue reading

Heat Treating Society member Steve Ferdon earns CHTE Distinguished Service Award


Source:

The Center for Heat Treating Excellence at the Worcester Polytechnic Institute, Mass., announces that it has presented its Distinguished Service Award to Steve Ferdon. The award is granted to an individual who has made significant, commendable, and long-standing contributions to the promotion of CHTE. A member of the ASM Heat Treating Society, Mr. Ferdon is the Director of Global Engineering Technology in the Fuel Systems Business Unit at global power leader Cummins Inc.

A member of CHTE since 2010, he has served as chair of its board of directors since 2012. His leadership at CHTE has contributed to mentoring the next generation of engineers, formalizing industrial membership governance of the board of directors, and sharing technical knowledge of heat treating applications with members.

Mr. Ferdon received the award at a formal ceremony recently during CHTE's biennial meeting on the WPI campus. "I am surprised and humbled by this recognition from the CHTE membership," he said. "Every year, I look forward to the spring and fall CHTE meetings, and the energizing collaboration with this unique group of talented, experienced, and highly practical technical leaders."

"Steve has impacted the advancement of CHTE," said Richard Sisson, George F. Fuller professor of Mechanical Engineering at WPI and technical director of CHTE. "From a technical standpoint, he brings a broad perspective to the industry. Cummins works with an extensive network of heat treating service providers from all over the world, applying multiple processes for ferrous alloys, and he shares a great deal of what Cummins has learned with our industrial members."

Prof. Sisson also noted Mr. Ferdon's efforts to bring the next generation of engineers to the meetings, where they can learn practical experience from industry leaders.

Steve received the Outstanding Materials Science Engineer Award from Purdue University's School of Materials Engineering in 1998, and is on the school's advisory committee. He holds six patents, is a Licensed Professional Engineer, and is a member of the AISI Bar Steel Fatigue Property Consortium Steering Committee. He began his career at Indiana-based Cummins in 1992 as a technical specialist in materials engineering.

http://wp.wpi.edu/chte/

 

 

Heat Treating Society member Steve Ferdon earns CHTE Distinguished Service Award

The Center for Heat Treating Excellence at the Worcester Polytechnic Institute, Mass., announces that it has presented its Distinguished Service Award to Steve Ferdon.

Continue reading

Can-Eng Furnaces awarded contract for austenitizing and molten salt quenching system


Source:

Can-Eng Furnaces International Ltd., Niagara Falls, Ontario, has been awarded a contract to design and build a 1500 lb/hr mesh belt furnace system for the austenitizing and molten salt quenching of unique components for drivetrain systems.  This contract was awarded by a repeat Mexico-based client who has purchased several Can-Eng multi-facility heat treatment lines.

The system incorporates several technological advancements for continuous atmosphere processing of products requiring carbon diffusion and quenching by a molten salt system. The new austempering system includes automated bin-dumping loading, mesh belt atmosphere hardening furnace, salt quench, post quench wash and rinse system, mesh belt temper oven, and endothermic gas generator.

This new project is a result of Can-Eng's commitment to its customer's success, years of teamwork, and mutual cooperation, yielding a custom engineering project integrating the customer's focused needs with Can-Eng's robust Continuous Mesh Belt Heat Treatment System technology.

The project is scheduled to be commissioned early 2018 in Mexico's centralized automotive manufacturing corridor.  Can-Eng's mesh belt heat treatment design team continues to focus globally on the design and development of mesh belt heat treatment technology, servicing the increasingly stringent and demanding global automotive industry. These systems continue to lead the industry in up-time reliability, energy efficiency, and soft handling features.

www.can-eng.com

 

Can-Eng Furnaces awarded contract for austenitizing and molten salt quenching system

Can-Eng Furnaces International Ltd., Niagara Falls, Ontario, has been awarded a contract to design and build a 1500 lb/hr mesh belt furnace system for the austenitizing and molten salt quenching of unique components for world-class drivetrain systems.

Continue reading

Women in Engineering Profile: Ursula Kattner

July 27, 2017
Source: ASM International

Women in Engineering Profile: Ursula Kattner

This profile series introduces leading materials scientists from around the world who happen to be females. Here we speak with Ursula Kattner, physical scientist at the National Institute of Standards and Technology and recipient of the 2016 J. Willard Gibbs Phase Equilibria Award.

Continue reading

Women in engineering profile: Margaret Flury


Source: ASM International

Women in engineering profile: Margaret Flury

This profile series introduces leading materials scientists from around the world who happen to be females. Here we speak with Margaret Flury, principal materials engineer at Medtronic.

Continue reading

High-strength magnesium sheet with high formability features low-cost alloying metals


Source:

Japan's National Institute for Materials Science and Nagaoka University of Technology announce development of a high-strength magnesium sheet alloy that has excellent formability comparable to that of the aluminum sheet currently used in body panels of some automobiles. The alloy is composed of only common metals, and is expected to be a low-cost lightweight sheet metal for automotive applications.

Magnesium alloys are roughly 75% lighter than steels and 33% lighter than aluminum alloys. However, virtually no magnesium alloys are used in automotive bodies because of their high processing cost originating from the poor formability and low strength of magnesium sheet alloys.

The research team recently developed a new age-hardenable magnesium alloy: Mg-1.1Al-0.3Ca-0.2Mn-0.3Zn, named AXMZ1000. The newly developed alloy has excellent room-temperature formability comparable to that of medium-strength aluminum alloys. In addition, the new alloy is 1.5 to 2.0 times stronger than the aluminum alloy.

The excellent formability was achieved by adding very small amounts of zinc and manganese, which led to the formation of fine grain structures. The high strength was achieved by adding aluminum and calcium, which induced the strengthening of the alloy by the formation of atomic clusters.

The newly developed alloy is composed of only common metals, so the material cost is not expensive. Also, it can be rolled into sheets by simple processes and heat treatments typical for aluminum alloys. The alloy overcomes the long-standing issues for magnesium namely, low strength and poor room temperature formability. As the processing cost of the new material is expected to be low, there is good potential for practical applications in automotive bodies or casing of notebook computers and cell phones.

This study was published in Scripta Materialia on June 16, 2017.  M.Z. Bian et al. A heat-treatable Mg–Al–Ca–Mn–Zn sheet alloy with good room temperature formability, Scripta Materialia (2017). DOI: 10.1016/j.scriptamat.2017.05.034

[email protected]

 

High-strength magnesium sheet with high formability features low-cost alloying metals

Japan’s National Institute for Materials Science and Nagaoka University of Technology announce development of a high-strength magnesium sheet alloy that has excellent formability comparable to that of the aluminum sheet currently used in body panels of some automobiles.

Continue reading

Ipsen invests $1 million in heat-treat industry by offering $50,000 credits for Titan furnaces


Source:

Ipsen, Cherry Valley, Ill., announces that it will offer a $50,000 credit toward the purchase of a new Titan vacuum furnace (applies to the 2017 list price of any Titan model) to any company that trades in its old furnace. Ipsen will accept a trade in of any brand heat-treating furnace (vacuum or atmosphere) in any condition. To receive this credit, transactions must take place by October 31, and the new Titan furnace must ship from Ipsen's facility by December 31, 2017. Ipsen offers this credit up to a total of $1,000,000.

The Titan vacuum furnace comes complete with PdMetrics, an advanced predictive maintenance software platform, and it incorporates years of customer feedback to deliver user-friendly features, all while maintaining a global platform, small footprint, and short delivery times.

Available in several sizes and horizontal or vertical configurations, the Titan provides powerful performance for both experienced and first-time heat treaters. It is Ipsen's hope that this investment results in future growth and innovations – for you, your customers, and the industry as a whole.

www.IpsenUSA.com/Invest.  

 

Ipsen invests $1 million in heat-treat industry by offering $50,000 credits for Titan furnaces

Ipsen, Cherry Valley, Ill., announces that it will offer a $50,000 credit toward the purchase of a new Titan vacuum furnace (applies to the 2017 list price of any Titan model) to any company that trades in its old furnace.

Continue reading

One MInute Mentor: X-Ray Diffraction Patterns in AISI 316

July 20, 2017
Source:

The graph shows X-ray diffraction patterns of nitrided (and carburized) stainless steel AISI 316. Carburizing was carried out in 20% CO-80% H2 gas atmosphere at 515°C (788 K) for five hours. X-ray diffraction analysis corroborates that the nitrogen content is significantly higher in the sample nitrided at the highest nitriding potential. The 111 Bragg reflections (peaks) are shifted to lower scattering angles, where the largest shift is observed for the highest nitriding potential.

The peak shift is caused primarily by dissolution of nitrogen, leading to a dilation of the fcc lattice; residual stress and stacking faults also contribute. Peaks originating from the unexpanded austenite are visible in the sample nitrided at KN = 0.293, indicating that the γN zone is not as thick as for the samples nitrided at high potentials.

Volume 4D, Heat Treating of Irons and Steels â‡’ Heat Treated High-Alloy Steels ⇒ Low-Temperature Surface Hardening of Stainless Steel ⇒ Gaseous Low-Temperature Surface Hardening of Austenitic Stainless Steel 

One MInute Mentor: X-Ray Diffraction Patterns in AISI 316

The graph shows X-ray diffraction patterns of nitrided (and carburized) stainless steel AISI 316.

Continue reading

Bodycote combines AM with powder metallurgy processes to produce complex parts


Source:

Bodycote, England, introduces Bodycote Powdermet technologies, a group of additive manufacturing processes for the production of complex components via powder metallurgy.

Powdermet technologies incorporate new, patent-pending techniques that combine 3D printing with well-established net-shape and near-net-shape processes. They greatly reduce manufacturing time and production cost compared to 3D printing alone.

Powdermet technologies ensure complete powder consolidation, achieve structural homogeneity, and eliminate internal porosity and unconsolidated powder flaws. The process can produce components with varying surface features and thicknesses, with higher structural integrity than alternative production techniques. The need for brazing or welding parts to form larger structures is eliminated. Instead, the finished article can be produced as one seamless component and largely avoid the size limitations imposed by the constraints of 3D printing.

Different parts of a component can be formed from different alloys, presenting the ideal and most cost-efficient solution. Component design can be tailored to the actual requirements for performance, and not limited by subsequent machining operations.

According to Stephen Harris, Group Chief Executive, "The recent breakthroughs are truly game changing technologies for component design and manufacturing. Industry applications are wide ranging, with early adoption expected in aerospace, oil and gas, power generation, and mining."

Bodycote continues to invest in resources and capital for developments in additive manufacturing technology to create significant value for customers and meet future growth demands. In addition to its Powdermet technologies, Bodycote provides a full range of heat treatment, hot isostatic pressing, and electrical discharge machining services across North America and Europe, tailored specifically to support the needs of companies manufacturing metal components by 3D printing.

www.bodycote.com

 

Bodycote combines AM with powder metallurgy processes to produce complex parts

Bodycote, England, introduces Bodycote Powdermet technologies, a group of additive manufacturing processes for the production of complex components via powder metallurgy.