Residual stress profiles of nitrided austenitic AISI 316 are shown in the graph.
Continue readingOne Minute Mentor: Residual Stress Profiles
August 3, 2017 Source: ASM International
One Minute Mentor: Residual Stress Profiles
August 3, 2017 Source: ASM International
Residual stress profiles of nitrided austenitic AISI 316 are shown in the graph.
Continue readingOne Minute Mentor: Tempering Corrosion-Resistant Tool Steels
May 6, 2016 Source:
The graph shows the tempering behavior of two corrosion-resistant tool steels: AISI 420 and the nitrogen-alloyed M333 (AISI 420 Mod). During tempering, the combination of properties such as hardness, toughness, and corrosion resistance, as well as residual stresses, can be adjusted within a wide range. Very low tempering temperatures (<300°F) are uncommon, as they result in very low impact toughness and high internal stresses.
With increased tempering temperatures, toughness properties can be improved significantly with only limited loss in hardness, as shown in the graph.
The precise behavior strongly depends on the uniformity of the microstructure and on chemical composition, with advantages shown by nitrogen-alloyed lower-carbon grades. Typical tempering temperatures for small and simple-shaped tools vary between 390 and 750°F. In the case of large and complex dies, such tempering temperatures can still lead to very high internal stresses, resulting in early tool failure despite good impact toughness.
Volume 4D, Heat Treating of Irons and Steels ⇒ Tool Steels ⇒ Heat Treating of Mold Steels and Corrosion-Resistant Tool Steels ⇒ Recommended Heat Treating Practices
During tempering, the combination of properties such as hardness, toughness, and corrosion resistance, as well as residual stresses, can be adjusted within a wide range