ASM Handbooks Online now includes Volume 5B: Protective Organic Coatings

October 29, 2015
Source:

ASM International, Materials Park, Ohio, recently released ASM Handbooks Online, which features the addition of ASM Handbook, Volume 5B: Protective Organic Coatings. This all new volume addresses a need for comprehensive information on organic coatings, including coating materials, surface preparation, application processes, industrial uses, and coating evaluation and analysis methods. It is an essential reference for industrial coating users, specifiers, and contractors. Industry respected authors and reviewers make this latest entry to ASM's handbook series the authoritative source for industrial coating information worldwide. See below for content included.  

COATING MATERIALS:

  • Alkyd resins
  • Acrylic coatings
  • Epoxy resins and curatives
  • Polyvinylidene fluoride-based coatings technology
  • Fluoroethylene vinyl ether resins for high-performance coatings
  • Phenolic coatings
  • Polyester and vinyl ester coatings
  • Polyurethane coatings
  • Polyurea-based coatings
  • Polyaspartic coatings
  • Polymeric floor coatings
  • Powder coatings: Pipelines
  • Powder coatings: Other industries
  • Silicon-based technologies in coatings
  • Polysiloxane hybrid coatings
  • Smart coatings and nanotechnology applications in coatings
  • Bitumens – coal tar and asphalt coatings
  • Wax-based coating systems
  • Zinc-rich coatings
     

SURFACE PREPARATION AND COATING APPLICATION:

  • Surface preparation
  • Soluble salts beneath coatings
  • Coating application methods
  • Shop and field quality control and quality assurance
  • Worker health and environmental hazards associated with coating application and removal
  • Green coatings
  • Coating various substrates
     

INDUSTRIAL USES:

  • Pipeline industry coatings
  • Marine coatings
  • Coatings used in the nuclear industry
  • Bridge coatings
  • Transportation-railcar  coatings
  • Guidance for the use of protective coatings in municipal potable water systems
  • Protective coatings for corrosion control in municipal wastewater  systems
  • Guidelines for maintenance coating of steel structures in pulp and paper mills
  • Coatings for commercial structures and building deficiencies that affect performance

COATING ANALYSIS AND EVALUATION:

  • Estimating the cost of industrial painting projects
  • Coating deterioration
  • Coating failure analysis
  • Laboratory testing
  • Coating failures and defects
  • Overview of other protection methods

ASM Handbooks Online is the industry's best known and most comprehensive source of information on ferrous and nonferrous metals and materials technology. Features the complete content of 34 ASM Handbook volumes, ASM Handbook supplements, and ASM Desk Editions—more than 25,000 pages of articles, illustrations, tables, graphs, specifications, and practical examples, providing peer-reviewed, trusted information in every area of materials specialization.

Quick and advanced search features enable users to search across the complete ASM Handbook collection in seconds. Additionally, a Contents Tree provides users with an intuitive way to browse and drill down to specific handbook volumes, articles, and sections of interest. The database provides aspiring and practicing engineers with instant, anytime access to the most trusted and comprehensive materials information resource available.

"ASM Handbooks are unique and valuable resources for the engineering community," says Scott D. Henry, ASM Director of Content and Knowledge Based Solutions. "They are written and edited by volunteers, assisted by ASM staff, to provide practical, in-depth technical information that is not readily available from other sources. This latest update to ASM Handbooks Online adds a wealth of information on organic coatings to the series."

For more information, or to schedule a customized demonstration via WebEx for your organization, please contact Denise Sirochman at 440.338.5409.

ASM Handbooks Online now includes Volume 5B: Protective Organic Coatings

ASM International, Materials Park, Ohio, recently released ASM Handbooks Online, which features the addition of ASM Handbook, Volume 5B: Protective Organic Coatings.

Continue reading

Unraveling structural ambiguities in lithium-rich transition metal oxides


Source:

Using complementary microscopy and spectroscopy techniques, researchers at Lawrence Berkeley National Laboratory (Berkeley Lab), Calif., say they have solved the structure of lithium- and manganese-rich transition metal oxides, a potentially game-changing battery material and the subject of intense debate in the decade since it was discovered.

Researchers have been divided into three schools of thought on the material's structure, but a team led by Alpesh Khushalchand Shukla and Colin Ophus spent nearly four years analyzing the material and concluded that the least popular theory is in fact the correct one. This material is important because the battery capacity can potentially be doubled compared to the most commonly used Li-ion batteries today due to the extra lithium in the structure. "However, it doesn't come without problems, such as voltage fade, capacity fade, and DC resistance rise," says Shukla. "It is immensely important that we clearly understand the bulk and surface structure of the pristine material. We can't solve the problem unless we know the problem."

A viable battery with a marked increase in storage capacity would not only shake up the cell phone and laptop markets, it would also transform the market for electric vehicles (EVs). "The problem with the current lithium-ion batteries found in laptops and EVs now is that they have been pushed almost as far as they can go," says Ophus. "If we're going to ever double capacity, we need new chemistries."

Using state-of-the-art electron microscopy techniques at the National Center for Electron Microscopy (NCEM) at Berkeley Lab's Molecular Foundry and at SuperSTEM in the UK, researchers imaged the material at atomic resolution. Because previous studies have been ambiguous about the structure, the researchers minimized ambiguity by looking at the material from different directions, or zone axes. "Misinterpretations from electron microscopy data are possible because individual two-dimensional projections do not give you the three-dimensional information needed to solve a structure," Shukla says. "So you need to look at the sample in as many directions as you can."

Scientists have been divided on whether the material structure is single trigonal phase, double phase, or defected single monoclinic phase. The "phase" of a material refers to the arrangement of the atoms with respect to each other; Ophus, a Project Scientist at the Molecular Foundry, explains how easy it is for researchers to reach different conclusions: "The two-phase and one-phase model are very closely related. It's not like comparing an apple to an orange—it's more like comparing an orange and a grapefruit from very far away. It's hard to tell the difference between the two."

In addition to viewing the material at atomic resolution along multiple zone axes, the researchers made another important decision, that is, to view entire particles rather than just a subsection. "Imaging with very high fields of view was also critical in solving the structure," Shukla said. "If you just look at one small part you can't say that the whole particle has that structure."

Putting the evidence together, Shukla and Ophus are fairly convinced that the material is indeed defected single phase. "Our research gives strong support for the defected single-phase monoclinic model and rules out the two-phase model, at least in the range of compositions used in our study," says Ophus, whose expertise is in understanding structure using a combination of computational methods and experimental results.

"We need to know what goes on at the atomic scale in order to understand the macroscopic behavior of new emerging materials, and the advanced electron microscopes available at national facilities such as SuperSTEM or NCEM are essential in making sure their potential is fully realized," he adds.

In addition to solving the structure of the bulk material, which has been studied by other research groups, they also solved the surface structure, which is different from the bulk and consists of just a few layers of atoms on select crystallographic facets. "The intercalation of lithium starts at the surface, so understanding the surface of the pristine material is very important," Shukla says.

On top of the STEM (scanning transmission electron microscopy) imaging that they used for the bulk, they had to use additional techniques to solve the surface, including EELS (electron energy loss spectroscopy) and XEDS (x-ray energy dispersive spectroscopy). "We show for the first time which surface structure occurs, how thick it is, how it's oriented in relation to the bulk, and in particular on what facets the surface phase does and doesn't exist," Ophus says.

An important part of the study was the quantity and quality of the samples studied. They started with lab-made samples. They used a molten-salt method that produces high-quality discrete primary particles that are impurity-free, making them ideal candidates for performing fundamental characterization. Taking a conservative approach, the researchers also decided to procure and analyze two commercial samples from two different companies.

"We could have finished the paper a year earlier, but because there was so much controversy we wanted to make sure we didn't leave any stone unturned," says Shukla. In the end, it took nearly four years to complete the research. Ophus calls it a "tour de force of microscopy" because of its thoroughness.

The work was funded by the Vehicle Technologies Office under the U.S. Department of Energy. The Molecular Foundry is a DOE Office of Science User Facility.

Image caption — The cube on the right represents the structure of lithium- and manganese- rich transition metal oxides. The models on the left show the structure from three different directions, which correspond to the STEM images of the cube.

Unraveling structural ambiguities in lithium-rich transition metal oxides

Using complementary microscopy and spectroscopy techniques, researchers at say they have solved the structure of lithium- and manganese-rich transition metal oxides.

Continue reading

New welding technique welds “unweldable” metals


Source:

Engineers at The Ohio State University, Columbus, developed a new welding technique that consumes 80% less energy than a common welding technique, yet creates bonds that are 50% stronger. The new technique could have a huge impact on the auto industry, which is poised to offer new cars which combine traditional heavy steel parts with lighter, alternative metals to reduce vehicle weight.

Despite recent advances in materials design, alternative metals still pose a challenge to manufacturers in practice. Many are considered unweldable by traditional means, in part because high heat and re-solidification weaken them, said Glenn Daehn, professor of materials science and engineering at Ohio State, who helped develop the new technique.

"Materials have gotten stronger, but welds haven't. We can design metals with intricate microstructures, but we destroy the microstructure when we weld," he says. "With our method, materials are shaped and bonded together at the same time, and they actually get stronger." Daehn explained the new process in a keynote address at the Materials Science & Technology 2015 meeting recently in Columbus.

In a common technique called resistance spot welding, manufacturers pass a high electrical current through pieces of metal, so that the metals' natural electrical resistance generates heat that partially melts them together and forms a weld. The drawbacks: generating high currents consumes a lot of energy, and the melted portions of metal are never as strong afterward as they were before.

Over the last decade, Daehn and his team have been trying to find ways around those problems. They've amassed more than half a dozen patents on a system called vaporized foil actuator (VFA) welding. In VFA, a high-voltage capacitor bank creates a very short electrical pulse inside a thin piece of aluminum foil. Within microseconds (millionths of a second), the foil vaporizes, and a burst of hot gas pushes two pieces of metal together at speeds approaching thousands of miles per hour.

The pieces do not melt, so there is no seam of weakened metal between them. Instead, the impact directly bonds the atoms of one metal to atoms of the other. Seen under a high-powered microscope, the bond is actually quite beautiful, and often features delicate curlicues in spots where veins of both materials extend outward and wrap around each other. The technique uses less energy because the electrical pulse is so short, and because the energy required to vaporize the foil is less than what would be required to melt the metal parts.

So far, the engineers have successfully bonded different combinations of copper, aluminum, magnesium, iron, nickel and titanium. They have created strong bonds between commercial steel and aluminum alloys—a feat which is impossible normally. Also, high-strength steel and aluminum join together with weld regions that are stronger than the base metals.

The technique is powerful enough to shape metal parts at the same time it welds them together, saving manufacturers a step. Daehn and his team now want to join with manufacturers to further develop the technology, which will be licensed through Ohio State's Technology Commercialization Office.

This project is funded by the Department of Energy and the National Science Foundation (NSF), and was one of the first to participate in I-Corps@Ohio, a new collaboration modeled after and approved by NSF's successful I-Corps commercialization program. Ohio is the first to have a statewide collaboration that is based on the NSF model, yet fully funded by the state. The program is funded and supported by the Ohio Department of Higher Education.

The Materials Science & Engineering annual meeting is organized by the American Ceramic Society, the Association for Iron & Steel Technology, ASM International, and the Minerals, Metals & Materials Society.

Image caption — Microscope view of steel (top) welded to aluminum alloy (bottom) using a new technique developed at The Ohio State University. Courtesy of Glenn Daehn/OSU.

New welding technique welds “unweldable” metals

Engineers at The Ohio State University developed a new welding technique that consumes 80% less energy than a common welding technique, yet creates bonds that are 50% stronger—creating a huge impact on the auto industry.

Continue reading

SSAB launches high-strength steels designed for auto chassis

October 28, 2015
Source:

SSAB, Sweden, announces that during the next 12 months it will release two hot-rolled advanced high-strength steel grades that exceed 800 and 1000 MPa in tensile strength for automobile chassis applications.

"The steels offer a unique combination of properties for maximized hole expansion and edge ductility," says José Puente Cabrero, Portfolio manager, automotive products.  

SSAB is a producer of advanced high-strength steels for the transport and automotive industries. These steels help designers and manufacturers meet new, exacting demands from industry and customers to reduce weight and COâ‚‚ emissions, increase cost efficiency, and improve crashworthiness. Through close collaboration with customers, research institutes, and universities, the R&D department at SSAB has created a series of new alloys.
SSAB will also introduce new cold-rolled martensitic steels with improved flatness. The latest Docol martensitic steels for cold-formed applications, with a tensile strength above 1700 MPa, are being designed into upcoming car models.

Up to now, higher tensile strength has affected the ductility of advanced high-strength steel products. "Now we are going to introduce new press-hardening steels. These are optimized to reach tensile strengths above 2000 MPa, but with retained good ductility," says Mr. Cabrero.

www.ssab.com

 

SSAB launches high-strength steels designed for auto chassis

SSAB, Sweden, announces that during the next 12 months it will release two hot-rolled advanced high-strength steel grades that exceed 800 and 1000 MPa in tensile strength for automobile chassis applications.

Continue reading

Seco-Warwick case-hardening system reduces distortion in gears


Source:

Seco Warwick, Meadville, Pa., introduces UniCase Master, a single flow, precision case-hardening system said to reduce distortion in gears; and the ZeroFlow gas nitriding process.  ZeroFlow is an ammonia-only nitriding process characterized by extremely low gas consumption and low emission of post-process gases. It features a simpler control system and reportedly delivers even better precision than processes with double-component atmospheres.

UniCase Master is said to offer not only a step forward in minimizing production cost and maximizing reliability, but also a real breakthrough in quality and repeatability in case hardening of gears by high-pressure gas quenching. It was created in collaboration with Professor Leszek Małdziński from the Institute of Work Machines and Vehicles of the Technical University in Poznan as a new method of controlled gas nitriding and nitrocarburizing.

The ZeroFlow method is based on performing the nitriding process in a single-component atmosphere: raw ammonia (NH3). The adjustment of nitriding atmosphere chemical composition and therefore control of nitriding potential Kn is performed only by a temporary stop and reactivation of NH3 feeding into the furnace.

www.secowarwick.com

 

Seco-Warwick case-hardening system reduces distortion in gears

Seco Warwick, Meadville, Pa., introduces UniCase Master, a single flow, precision case-hardening system said to reduce distortion in gears; and the ZeroFlow gas nitriding process.

Continue reading

MTS provides test equipment to engineering lab at Penn State


Source: ASM International

MTS provides test equipment to engineering lab at Penn State

MTS Systems Corp., Eden Prairie, Minn., has provided Penn State University, State College, with a suite of advanced materials testing equipment and software for its Department of Engineering Science and Mechanics laboratory.

Continue reading

Constellium launches Aeral aluminum for aerosol cans


Source:

Constellium N.V., Amsterdam, has launched Aeral, an aluminum solution designed for making aerosol containers by the "drawn and ironed" technology currently used to produce beverage cans. Aeral enables a minimum of 30% weight savings versus traditional impact-extruded containers, all while maintaining the same level of performance in terms of ductility and resistance to pressure.

According to the company, Aeral is based on an alloy that can be used efficiently throughout the D&I canmaking process, including the necking operation, while meeting the pressure resistance and aesthetic requirements of cosmetics companies.

Aeral is said to demonstrate Constellium's commitment to sustainability and the development of innovative, lighter, and infinitely recyclable solutions.  It was developed through a combination of cutting-edge research at C-TEC, Constellium's world-class technology center in Voreppe, France, and strong industrial capabilities at the company's rolling mill in Neuf-Brisach, France, which has long experience in manufacturing light-weighting products, including beverage cans. Constellium is already in advanced discussions with some key players in the market. 

www.constellium.com

 

 

Constellium launches Aeral aluminum for aerosol cans

Constellium N.V., Amsterdam, has launched Aeral, an aluminum solution designed for making aerosol containers by the “drawn and ironed” technology currently used to produce beverage cans.

Continue reading

Praxair, Atmosphere Engineering sign joint marketing agreement


Source:

Praxair Inc., Danbury, Conn., has signed an agreement with Atmosphere Engineering that will allow customers to access Praxair's industrial gases, application technologies, and supply systems, as well as Atmosphere Engineering's furnace control systems and sensors.

The combined capabilities of the two companies cover a broad spectrum of batch and continuous heat-treating processes such as carburizing, carbonitriding, neutral hardening, annealing, gas quenching, and heat treatment under vacuum.

"The automotive and aerospace industries are expanding technology and material requirements in the heat-treat market," said Steve Mueller, business development manager for Metals and Materials Processing in Praxair's U.S. industrial gases business. "Our team approach will better enable heat-treaters to meet high-quality product needs and reproducible standards in their furnace operations."

"This collaboration with Praxair will help us to build on our global presence while providing our customers with the best solutions to meet their heat-treating requirements," said Eric Jossart, vice president of sales for Atmosphere Engineering.

www.praxair.com

 

 

Praxair, Atmosphere Engineering sign joint marketing agreement

Praxair Inc., Danbury, Conn., has signed an agreement with Atmosphere Engineering that will allow customers to access Praxair’s industrial gases, application technologies, and supply systems, as well as Atmosphere Engineering’s furnace control systems and sensors.

Continue reading

Fireworks at Heat Treat Social Event Causes an International Stir

October 27, 2015
Source:

MATERIALS PARK, OH – October 27, 2015 – Last week at Heat Treat 2015, the ASM Heat Treating Society rolled out their new social event, "The Heat Is On", which included a fireworks display that delighted guests and locals alike.

The "Heat Is On" networking event took place on Wednesday evening at the Port of Detroit facility right on the Detroit River.  The 350+ attendees were greeted with flame twirlers as they arrived at the venue, and throughout the evening they enjoyed delicious Detroit-style food, hand rolled cigars, an open bar that included some great local craft beers, and a local band. The evening was capped off by an amazing surprise fireworks display on the water, which was sponsored by Surface Combustion to celebrate their 100th anniversary. The Detroit River is considered international waters as well as a major shipping lane, so guests and locals from Detroit and Windsor were surprised by the seemingly impromptu show.

The "mystery" fireworks caused quite a stir on social media and in local news outlets on Wednesday night. Detroit and Windsor residents took to social media to ask who was behind this unexpected display on international waters, while several news outlets in Windsor and Detroit picked up the story. ASM solved the mystery by claiming responsibility on Thursday afternoon.

Kelly Thomas, Senior Manager, Events at ASM International, was pleased at the outcome of the first Heat Treat social event. "We set the bar high in 2015 and HTS will continue to grow the programming, exposition and networking events to remain the leaders in the industry. To find out what we have planned next, you will have to join us at Heat Treat 2017!"

The next Heat Treat event will take place on October 24-26, 2017 in Columbus, Ohio.

 

CBC Canada – "ASM International company behind mysterious fireworks show over Detroit River"

Detroit Free Press – "Source of Detroit's mystery fireworks revealed"

Windor Independent – "Surprise fireworks baffles residents – we've got the answer"

WXYZ Detroit – "Mystery solved: Last night's massive fireworks display over Detroit River was part of private event"

M Live – "Mysterious fireworks show on river leaves Detroiters and Canadians wondering"

 

About ASM International

As the world's largest association of materials-centric engineers and scientists, ASM International is dedicated to informing, educating, and connecting the materials community. A member and volunteer based organization, ASM serves as a central resource that gathers the latest applied information from the field and disseminates it back to industry, academia, and government through published content, classes, conferences, expositions, and local chapter engagement.

To learn more about ASM International, visit www.asminternational.org.


About The ASM Heat Treating Society

HTS, an Affiliate Society of ASM International formed in 1994, is the world's largest network of heat treaters. HTS members work to provide events and services to serve their worldwide membership of captive and commercial heat treaters, equipment manufacturers, researchers, governments and technicians. HTS members have their own unique leadership and agenda to serve the global heat treating community, and are dedicated to: Bringing heat treaters together to discuss heat treating challenges; providing the technical information, knowledge and education needed by all heat treaters; serving as a central clearinghouse for information of value to heat treaters; and interfacing with all organizations that serve heat treaters.

To learn more about HTS, visit www.asminternational.org/hts3-new

Fireworks at Heat Treat Social Event Causes an International Stir

MATERIALS PARK, OH – October 26, 2015 – Last week at Heat Treat 2015, the ASM Heat Treating Society rolled out their new social event, “The Heat Is On”, which included a fireworks display that delighted guests and locals alike.

Continue reading

Isothermal Transformation Diagram for Tool Steels

October 23, 2015
Source:

Isothermal Transformation Diagram for Tool Steels

The graph shows the isothermal transformation diagram for the steel AISI 1075/DIN EN C75. Cooling curves  show three process cycles for molten metal quenching in the time-temperature-transformation plots:

  • Ms: martempering to produce circular or band saws, flapper valves, or springs
  • Bai: austempering to produce cutting dies, leather and paper cutting tools, and on parts for cars
  • P: patenting to produce a ready-to-roll strip for seat belt springs or cable springs

Volume 4D, Heat Treating of Irons and Steels -> Tool Steels ->  Processes and Furnace Equipment for Heat Treating of Tool Steels -> Equipment for Austenitizing, Quenching, and Tempering of Tool Steels

Isothermal Transformation Diagram for Tool Steels

The graph shows the isothermal transformation diagram for the steel AISI 1075/DIN EN C75. Cooling curves show three process cycles for molten metal quenching in the time-temperature-transformation plots.

Continue reading