NSF award will help UAB researchers develop and understand high-temperature-resistant materials

July 20, 2022
Source: ASM International

NSF award will help UAB researchers develop and understand high-temperature-resistant materials

Shane Aaron Catledge, Ph.D., associate professor in the University of Alabama at Birmingham Department of Physics, was awarded a three-year Division of Materials grant from the National Science Foundation for his project “New frontiers in synthesis of high-entropy transition metal borides enabled by microwave-induced plasma.”

Continue reading

One Minute Mentor: Austenitizing

July 12, 2022
Source: ASM International

One Minute Mentor: Austenitizing

Austenitizing is the most critical of all heating operations performed on tool steels. Along with quenching it will usually be referred to as the hardening step in tool steel heat treatment and, associated with tempering, will be responsible for the final properties.

Continue reading

Seco/Warwick to produce specialized dies for motorcycle parts


Source: ASM International

Seco/Warwick to produce specialized dies for motorcycle parts

Seco/Warwick, Poland, will supply a Vector vacuum furnace to Atlas Autos Ltd, the largest manufacturer of motorcycle parts in Pakistan. The solution is intended for hardening and tempering processes, and its design will allow for gas cooling elements and dies for parts used in automotive production.

Continue reading

Students from Lehigh University tour Solar Atmospheres


Source: ASM International

Students from Lehigh University tour Solar Atmospheres

Solar Atmospheres, Souderton, Pa., hosted over 40 high school students enrolled in the Summer Engineering Institute (SEI) at Lehigh University. The SEI program, under the guidance of Laura Moyer, is a two-week residential program, running two sessions back to back.

Continue reading

Constellium and Morf3D enter a joint additive manufacturing development program

May 31, 2022
Source: ASM International

Constellium and Morf3D enter a joint additive manufacturing development program

Constellium, Paris, is entering into an agreement to provide Aheadd CP1, one of its proprietary additive manufacturing (AM) powder solutions, to Morf3D Inc., a subsidiary of Nikon Corp., specializing in AM optimization and engineering for the aviation, space, and defense industries.

Continue reading

Ipsen USA provides Turbo2Treater for Italian commercial heat treater


Source: ASM International

Ipsen USA provides Turbo2Treater for Italian commercial heat treater

Ipsen, Cherry Valley, Ill., installed a second Turbo2Treater vacuum furnace at Temprasud, a commercial heat treater in Fresagrandinaria, Italy. The new furnace will help them continue to grow business in the automotive market, with anticipated expansion into aerospace.

Continue reading

Heat treating niobium for better particle accelerators


Source: ASM International

Heat treating niobium for better particle accelerators

Virgina Tech, Va., scientists have developed a new theoretical model for preparing particle accelerator structures made of niobium metal. The model predicts the rate of oxygen diffusion into niobium on heat treatment.

Continue reading

One Minute Mentor: Induction Hardening

May 5, 2022
Source: ASM International

One Minute Mentor: Induction Hardening

Spur gears, bevel gears, splined hubs, and cams are ideal components for production using powder metallurgy. Induction hardening is a method to make these parts locally hard and wear-resistant with a tougher ductile matrix.

Continue reading