SSAB launches Laser Plus steel with guaranteed flatness after laser cutting

October 29, 2014
Source:

SSAB Stockholm, Sweden, has introduced Laser Plus, a new generation of steels for laser cutting that comes with unique guarantees: maximum flatness deviation of 3 mm/m after laser cutting, and bending radius of 0 -1.5 x the material thickness. These features make it possible to meet the most challenging requirements in automated production environments.

The production process of Laser Plus steels results in a surface that is covered with a thin micro scale. This enables extremely efficient laser- water- and plasma cutting. The quality of the cut edge remains excellent, even up to a thickness of 30 mm. The cold forming properties of Laser Plus steels are excellent and SSAB guarantees inner bending radius of 0-1.5 x the material thickness, depending on strength level in combination with thickness.

Laser Plus steels are now available both as heavy plates and hot-rolled strip products. It is the new standard for demanding applications in mechanical engineering and construction, as well as in the automotive and electronics industries.

www.ssab.com

 

SSAB Stockholm, Sweden, has introduced Laser Plus, a new generation of steels for laser cutting that comes with unique guarantees: maximum flatness deviation of 3 mm/m after laser cutting, and bending radius of 0 -1.5 x the material thickness. These features make it possible to meet the most challenging requirements in automated production environments.

The production process of Laser Plus steels results in a surface that is covered with a thin micro scale. This enables extremely efficient laser- water- and plasma cutting. The quality of the cut edge remains excellent, even up to a thickness of 30 mm. The cold forming properties of Laser Plus steels are excellent and SSAB guarantees inner bending radius of 0-1.5 x the material thickness, depending on strength level in combination with thickness.

Laser Plus steels are now available both as heavy plates and hot-rolled strip products. It is the new standard for demanding applications in mechanical engineering and construction, as well as in the automotive and electronics industries.

www.ssab.com

 