SSAB launches steel tube family with extreme wear resistance

March 11, 2015
Source:

SSAB Steel, Sweden, has launched the new Hardox Tube 500 family, which provides the same hardness and toughness as Hardox wear plate, but in tubular form. It was developed for applications that require high wear resistance in combination with lower density. It is suitable for transporting all types of abrasive materials, such as wet concrete, soil, gravel, and ore slurry.

"The new Hardox Tube 500 range completes the existing Hardox family product range. We have  long experience in developing wear-resistant steel tubes. The final properties are set after tube rolling and welding, which guarantees consistency as well as high hardness and toughness qualities," says Fredrik Mikaelsson, Manager for Tubes & Sections at SSAB.

Its extreme wear resistance allows for a lighter product with a long service life. It can increase the competitiveness of certain products by extending their service life by two, five, ten times, or more.

Hardox Tube 500 is available from stock in 88.9-133 mm diameters and different material thicknesses. Custom tubes in thinner materials and other diameters are also available.

www.ssab.com 

 

SSAB Steel, Sweden, has launched the new Hardox Tube 500 family, which provides the same hardness and toughness as Hardox wear plate, but in tubular form. It was developed for applications that require high wear resistance in combination with lower density. It is suitable for transporting all types of abrasive materials, such as wet concrete, soil, gravel, and ore slurry.

“The new Hardox Tube 500 range completes the existing Hardox family product range. We have  long experience in developing wear-resistant steel tubes. The final properties are set after tube rolling and welding, which guarantees consistency as well as high hardness and toughness qualities,” says Fredrik Mikaelsson, Manager for Tubes & Sections at SSAB.

Its extreme wear resistance allows for a lighter product with a long service life. It can increase the competitiveness of certain products by extending their service life by two, five, ten times, or more.

Hardox Tube 500 is available from stock in 88.9-133 mm diameters and different material thicknesses. Custom tubes in thinner materials and other diameters are also available.

www.ssab.com 

 