One Minute Mentor: Effects of Different Cooling Rates on Corrosion-Resistant Tool Steels

March 18, 2016
Source:

The graph shows the effects of different cooling rates on the toughness properties (un-notched samples) of AISI 420 and nitrogen-alloyed M333 tool steels.

The cooling parameter λ8/5, which is the cooling time from 1470° to 930°F in seconds, divided by 100, is used. Besides the general trend of falling toughness with rising cooling time, it is clearly evident that the nitrogen-alloyed steel grade M333 (420Mod), which has a lower carbon content, shows significantly higher toughness values. These can be further improved by lowering the austenitizing temperature. This behavior correlates well with the reduced tendency to form proeutectoid carbides at grain boundaries. A similar correlation can be found for the steel grades AISI 440B and the nitrogen-alloyed M340 (440Mod).

Volume 4D, Heat Treating of Irons and Steels â‡’ Tool Steels ⇒ Heat Treating of Mold Steels and Corrosion-Resistant Tool Steels â‡’ Recommended Heat Treating Practices

The graph shows the effects of different cooling rates on the toughness properties (un-notched samples) of AISI 420 and nitrogen-alloyed M333 tool steels.

The cooling parameter ?8/5, which is the cooling time from 1470° to 930°F in seconds, divided by 100, is used. Besides the general trend of falling toughness with rising cooling time, it is clearly evident that the nitrogen-alloyed steel grade M333 (420Mod), which has a lower carbon content, shows significantly higher toughness values. These can be further improved by lowering the austenitizing temperature. This behavior correlates well with the reduced tendency to form proeutectoid carbides at grain boundaries. A similar correlation can be found for the steel grades AISI 440B and the nitrogen-alloyed M340 (440Mod).

Volume 4D, Heat Treating of Irons and Steels ? Tool Steels ? Heat Treating of Mold Steels and Corrosion-Resistant Tool Steels ? Recommended Heat Treating Practices