One Minute Mentor: Metallurgy of Ferritic Stainless Steels

May 12, 2016
Source:

One Minute Mentor: Metallurgy of Ferritic Stainless Steels

Chromium stabilizes the ferritic structure at high temperatures, but some austenite can form at high temperature in steels with 12% chromium and a low or medium percentage of carbon, as shown in the graph. The graph shows the effect of chromium additions on the extent of the austenite phase field in the iron-carbon system.

Carbon and nitrogen added together also produce about the same effect as carbon alone, which means that a fully ferritic stainless steel at elevated temperatures is not possible below 20% chromium without refining to remove carbon and nitrogen.

In addition, because chromium is a strong carbide former, the presence of carbon causes the formation of chromium carbides. This depletes the amount of dissolved (in solution) chromium that is needed to create the corrosion-resistant oxide layer of a stainless steel. 

Volume 4D, Heat Treating of Irons and Steels â‡’ Heat Treated High-Alloy Steels â‡’ Heat Treating of Ferritic Stainless Steels â‡’ Metallurgy of Ferritic Stainless Steels 

 

One Minute Mentor: Metallurgy of Ferritic Stainless Steels

Chromium stabilizes the ferritic structure at high temperatures, but some austenite can form at high temperature in steels with 12% chromium and a low or medium percentage of carbon, as shown in the graph. The graph shows the effect of chromium additions on the extent of the austenite phase field in the iron-carbon system.

Carbon and nitrogen added together also produce about the same effect as carbon alone, which means that a fully ferritic stainless steel at elevated temperatures is not possible below 20% chromium without refining to remove carbon and nitrogen.

In addition, because chromium is a strong carbide former, the presence of carbon causes the formation of chromium carbides. This depletes the amount of dissolved (in solution) chromium that is needed to create the corrosion-resistant oxide layer of a stainless steel. 

Volume 4D, Heat Treating of Irons and Steels ? Heat Treated High-Alloy Steels ? Heat Treating of Ferritic Stainless Steels ? Metallurgy of Ferritic Stainless Steels 

 