Lucifer Red Devil box furnace heat treats small loads

June 15, 2016
Source:

Lucifer Furnaces, Warrington, Pa., recently delivered a bench style RD7 Red Devil box furnace for batch heat treating small loads of low carbon steel. An all-purpose general bench unit, Lucifer's RD7 series can be purposed to various heat-treating operations such as hardening, drawing, tempering, or annealing of steel. Model RD7-KHE24, with 7 KW power, heats to 2200°F with easy-to-replace wire-wound heating elements in removable holders. 

A horizontal swing door seals the 12x14x24-inch chamber.  A ceramic hearth plate supports the work load and protects the floor brick. The Honeywell digital temperature controller with safety microswitch and on/off main control switch are housed in a NEMA 1 side mounted panel, and a rear-mounted Type K thermocouple senses chamber heat. 

This Red Devil Series furnace is insulated with a combined 4.5 inches of lightweight hotface firebrick insulation and coldface mineral wool.  Refractory is dry fit and easily replaced. Red Devil Series box furnaces can be fitted with optional accessories, including an over-temperature safety system, gas spring vertical lift door, and a base stand.  Red Devil Furnaces are completely wired, assembled, test fired, and shipped ready for connection to a main power supply. 

www.luciferfurnaces.com

 

Lucifer Furnaces, Warrington, Pa., recently delivered a bench style RD7 Red Devil box furnace for batch heat treating small loads of low carbon steel. An all-purpose general bench unit, Lucifer’s RD7 series can be purposed to various heat-treating operations such as hardening, drawing, tempering, or annealing of steel. Model RD7-KHE24, with 7 KW power, heats to 2200°F with easy-to-replace wire-wound heating elements in removable holders. 

A horizontal swing door seals the 12x14x24-inch chamber.  A ceramic hearth plate supports the work load and protects the floor brick. The Honeywell digital temperature controller with safety microswitch and on/off main control switch are housed in a NEMA 1 side mounted panel, and a rear-mounted Type K thermocouple senses chamber heat. 

This Red Devil Series furnace is insulated with a combined 4.5 inches of lightweight hotface firebrick insulation and coldface mineral wool.  Refractory is dry fit and easily replaced. Red Devil Series box furnaces can be fitted with optional accessories, including an over-temperature safety system, gas spring vertical lift door, and a base stand.  Red Devil Furnaces are completely wired, assembled, test fired, and shipped ready for connection to a main power supply. 