Solar Atmospheres Southeast can heat treat up to 50,000 pounds in vacuum

July 20, 2016
Source:

Solar Atmospheres, Souderton, Pa., announces that its newest facility in Greenville, South Carolina, has a wide range of vacuum processing capacity, from furnaces suited for small lots and development cycles, to a 24-foot vacuum chamber capable of processing up to 50,000 pounds at 2650°F. All are backed by AS9100 and Nadcap quality systems to provide the assurance that products are processed as they should be.

A wide range of options is available, including vacuum carburizing and cryogenic processing. A metallurgical testing laboratory provides product and process validation from surface hardness testing to microstructure evaluation

"The Southeast continues to grow and attract manufacturers supporting a broad range of market sectors," says President Steve Prout. "We are proud to be a supplier that is positioned to support this growth, and we are excited to find ways to help our customers achieve their goals and contribute toward their success."

www.solaratm.com

 

Solar Atmospheres, Souderton, Pa., announces that its newest facility in Greenville, South Carolina, has a wide range of vacuum processing capacity, from furnaces suited for small lots and development cycles, to a 24-foot vacuum chamber capable of processing up to 50,000 pounds at 2650°F. All are backed by AS9100 and Nadcap quality systems to provide the assurance that products are processed as they should be.

A wide range of options is available, including vacuum carburizing and cryogenic processing. A metallurgical testing laboratory provides product and process validation from surface hardness testing to microstructure evaluation

“The Southeast continues to grow and attract manufacturers supporting a broad range of market sectors,” says President Steve Prout. “We are proud to be a supplier that is positioned to support this growth, and we are excited to find ways to help our customers achieve their goals and contribute toward their success.”

www.solaratm.com

 