Solar Atmospheres of California is awarded Nadcap 24-month Merit status

August 9, 2016
Source:

Solar Atmospheres of California, Fontana, announces that it has been awarded Nadcap 24-month Merit status for Heat Treating, which means that instead of having its next Nadcap audit in eighteen months, it has been granted an accreditation that lasts until July 31, 2018.

"We are extremely pleased PRI has recognized our corporate commitment to quality," says a company news release. "Achieving 24-month Merit status has been a goal set by Solar's employees since the company opened its doors in 2011. The adherence to strict specification requirements, flawless process execution, and a daily commitment to quality processing is evident among all employees."

The company has held Nadcap accreditation since 2011. Having demonstrated its ongoing commitment to quality by satisfying customer requirements and industry specifications, the Nadcap Task Group has determined that Solar Atmospheres of California has earned this special recognition.

According to PRI's VP and COO Joe Pinto, "Benefitting from a less frequent audit schedule reduces audit costs and associated pressures, and demonstrates the trust that the aerospace industry has in Solar Atmospheres of California based on past performance in Nadcap audits. PRI is proud to support continuous improvement in the aerospace industry by helping such companies be successful, and we look forward to continuing to assist the industry moving forward."

www.solaratm-ca.com

 

Solar Atmospheres of California, Fontana, announces that it has been awarded Nadcap 24-month Merit status for Heat Treating, which means that instead of having its next Nadcap audit in eighteen months, it has been granted an accreditation that lasts until July 31, 2018.

“We are extremely pleased PRI has recognized our corporate commitment to quality,” says a company news release. “Achieving 24-month Merit status has been a goal set by Solar’s employees since the company opened its doors in 2011. The adherence to strict specification requirements, flawless process execution, and a daily commitment to quality processing is evident among all employees.”

The company has held Nadcap accreditation since 2011. Having demonstrated its ongoing commitment to quality by satisfying customer requirements and industry specifications, the Nadcap Task Group has determined that Solar Atmospheres of California has earned this special recognition.

According to PRI’s VP and COO Joe Pinto, “Benefitting from a less frequent audit schedule reduces audit costs and associated pressures, and demonstrates the trust that the aerospace industry has in Solar Atmospheres of California based on past performance in Nadcap audits. PRI is proud to support continuous improvement in the aerospace industry by helping such companies be successful, and we look forward to continuing to assist the industry moving forward.”

www.solaratm-ca.com

 