The nitriding potential controls the amount of nitrogen in the metal. The graph shows the atomic concentration of nitrogen as a function of nitriding potential (Kn) and depth.
One Minute Mentor: Nitriding Potential
February 17, 2017 Source:
The nitriding potential controls the amount of nitrogen in the metal. The graph shows the atomic concentration of nitrogen as a function of nitriding potential (Kn) and depth.