Solar Manufacturing receives U.S. patent for vacuum furnace hot zone improvement

August 30, 2017
Source:

Solar Manufacturing, Souderton, Pa., announces that it has been awarded a patent for an innovation in vacuum furnace hot zone design.  This hot zone improvement centers on the configuration of heating element supports, providing for simpler, streamlined manufacture of the support assembly.  The new design further provides for easy assembly and disassembly of heating elements, a significant improvement over prior designs.

Inventors are Robert Wilson, Solar Manufacturing's VP of Engineering; and Mark Hughes, Senior Design Engineer. Copies of U.S. Patent No. 9,702,627 B2 may be obtained by visiting www.uspto.gov.

www.solarmfg.com

 

Solar Manufacturing, Souderton, Pa., announces that it has been awarded a patent for an innovation in vacuum furnace hot zone design.  This hot zone improvement centers on the configuration of heating element supports, providing for simpler, streamlined manufacture of the support assembly.  The new design further provides for easy assembly and disassembly of heating elements, a significant improvement over prior designs.

Inventors are Robert Wilson, Solar Manufacturing’s VP of Engineering; and Mark Hughes, Senior Design Engineer. Copies of U.S. Patent No. 9,702,627 B2 may be obtained by visiting www.uspto.gov.

www.solarmfg.com

 