SAE International MedAccred Heat-Treating Standard recognized by U.S. FDA

January 31, 2018
Source: ASM International

SAE International, Warrendale, Pa., announces that technical standard AMS2750 – Pyrometry, has received complete recognition by the U.S. Federal Drug Administration Center for Devices and Radiological Health, and it has been added to its list of recognized consensus standards database, List #47.

AMS2750 covers pyrometric requirements for thermal processing equipment used for heat treatment, including sensors, instrumentation, thermal processing equipment, system accuracy tests, and temperature uniformity surveys.

The standard also serves as the cornerstone standard for the Performance Review Institute’s MedAccred heat treating Accreditation. MedAccred is an industry-managed supply chain oversight program that reduces risk to patient safety, and assures quality products and compliance with requirements as they apply to critical processes n the production of medical devices. All MedAccred heat treating accredited suppliers meet the requirements of the standard.

www.sae.org 

www.pri.org

 

Recommended Posts